# US 2025/0218975 A1 · Wafer-level chip scale package semiconductor devices with light blocking material and methods

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0218975 A1
- Document ID: US20250218975A1
- Status: Published application
- Kind: A1
- Application number: 18/399,630
- Filed: 2023-12-28
- Published: 2025-07-03
- Earliest claimed: 2023-12-28
- Assignees: Texas Instruments Incorporated
- Applicants: Texas Instruments Incorporated
- Inventors: Daiki Komatsu; Masamitsu Matsuura
- Web page: https://patentgrep.com/patent/US20250218975A1

## CPC

- H10W 42/20: protecting against electromagnetic or particle radiation, e.g. light, X-rays, gamma-rays or electrons
- H10W 74/129: {forming a chip-scale package [CSP]}
- H10P 54/00: Cutting or separating of wafers, substrates or parts of devices
- H10P 54/20: by laser cutting
- H10W 72/012: {of bump connectors, dummy bumps or thermal bumps}
- H10W 72/90: Bond pads, in general
- H10W 74/014: {using batch processing}
- H10P 54/30: by forming weakened zones for subsequent cutting or separating, e.g. by laser treatment or by ion implantation
- H10P 54/90: Auxiliary processes or arrangements
- H10P 54/92: for protecting or reinforcing the surface of wafers or substrates during cutting or separating, e.g. using adhesive tapes
- H10P 54/924: {using expanding wafer tapes}
- H10P 72/7402: {Wafer tapes, e.g. grinding or dicing support tapes}
- H10P 72/7416: {used during dicing or grinding}
- H10W 72/019: {of bond pads}
- H10W 72/0198: {batch processes}
- H10W 72/20: Bump connectors, e.g. solder bumps or copper pillars; Dummy bumps; Thermal bumps
- H10W 72/252: {comprising solid metals or solid metalloids, e.g. PbSn, Ag or Cu}
- H10W 72/29: Bond pads specially adapted therefor
- H10W 72/981: {Auxiliary members, e.g. spacers}
- H10W 74/134: {the encapsulations being in grooves in the semiconductor body}
- H10W 74/141: {the encapsulations being on at least the sidewalls of the semiconductor body}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A described example includes: a semiconductor die having bond pads on a device side surface, having a backside surface opposite the device side surface and having four sides extending between the device side surface and the backside surface; a layer of light blocking material deposited on the device side surface, the light blocking material also covering the four sides; semiconductor material on the exterior of the light blocking material covering the four sides, the semiconductor material spaced from the semiconductor device die by the light blocking material covering the four sides; a backside coating of light blocking tape covering the backside surface; openings in the layer of light blocking material on the device side surface, the openings exposing under-bump material formed on the bond pads; and terminals that are formed by solder bumps or conductive post connects formed on the under-bump material.

## Claims

### Claim 1

A method for making a packaged semiconductor device, comprising:
forming under-bump metallization material on bond pads of semiconductor dies arranged in rows and columns on a device side surface of a semiconductor wafer, the semiconductor dies spaced from one another by scribe lanes, the semiconductor wafer having a backside surface opposite the device side surface;
forming trenches extending from the device side surface into but not through the semiconductor wafer along sides of the semiconductor dies, the trenches adjacent the scribe lanes;
depositing light blocking material over the device side surface, the light blocking material filling the trenches to form filled trenches and forming a layer of the light blocking material covering the device side surface of the semiconductor wafer;
patterning the layer of light blocking material to expose the under-bump metallization material over the bond pads of the semiconductor dies and to expose the scribe lanes between the filled trenches;
forming solder bumps on the under-bump metallization material;
backgrinding the backside surface to thin the semiconductor wafer and to expose the light blocking material in the filled trenches;
depositing a light blocking backside coating tape on the backside surface;
dicing the semiconductor wafer along the scribe lanes using either laser dicing or plasma dicing, the dicing leaving semiconductor material edges on the sides of the semiconductor dies; and
expanding the semiconductor wafer along the scribe lanes to separate the semiconductor dies from one another to form packaged semiconductor dies.

### Claim 2 (depends on 1)

The method of claim 1, wherein after expanding the semiconductor wafer along the scribe lanes to separate the semiconductor dies from one another to form packaged semiconductor dies, the light blocking material covers the device side surface and four sides that extend perpendicularly from the device side surface to the backside surface of the packaged semiconductor dies, and the backside surface is covered with the light blocking backside coating tape, so that all external surfaces of the packaged semiconductor dies are covered with light blocking material.

### Claim 3 (depends on 1)

The method of claim 1, wherein dicing the semiconductor wafer along the scribe lanes using either laser dicing or plasma dicing further comprises:
using a stealth laser dicing process, focusing a laser beam into the semiconductor wafer beneath the device side surface, and traversing the semiconductor wafer along the scribe lanes with the laser beam to form stress dislocation regions within the semiconductor wafer.

### Claim 4 (depends on 1)

The method of claim 1, wherein dicing the semiconductor wafer along the scribe lanes using either laser dicing or plasma dicing further comprises performing a plasma dicing process in the scribe lanes of the semiconductor wafer to etch through the semiconductor wafer in the scribe lanes to expose the light blocking backside coating tape.

### Claim 5 (depends on 1)

The method of claim 1, wherein depositing a layer of light blocking material over the device side surface of the semiconductor dies on the semiconductor wafer further comprises:
dispensing a liquid pre-wet material onto the semiconductor wafer in a spin-coating process;
using a first spin speed, allowing the pre-wet material to fill the trenches;
dispensing liquid light blocking material onto the semiconductor wafer;
using a second spin speed, displacing the pre-wet material and filling the trenches with the light blocking material;
using a third spin speed greater than the first spin speed, making the thickness of the light blocking material on the device side surface uniform; and
thermally curing the liquid light blocking material to form the layer of light blocking material.

### Claim 6 (depends on 1)

The method of claim 1, wherein depositing a light blocking backside coating tape on the backside surface further comprises:
attaching a first side of the light blocking backside coating tape to the backside surface of the wafer; and
thermally curing the light blocking backside coating tape.

### Claim 7 (depends on 1)

The method of claim 1, wherein depositing a light blocking backside coating tape on the backside surface further comprises depositing a backside coating tape that blocks infrared light.

### Claim 8 (depends on 7)

The method of claim 7, wherein depositing a backside coating tape that blocks infrared light further comprises depositing ADWILL LC backside coating tape from LINTEC OF AMERICA, INC.

### Claim 9 (depends on 1)

The method of claim 1, wherein depositing light blocking material over the device side surface of the semiconductor wafer further comprises depositing a material that blocks infrared light.

### Claim 10 (depends on 9)

The method of claim 9 wherein depositing a material that blocks infrared light further comprises depositing a black matrix resist.

### Claim 11 (depends on 10)

The method of claim 10, wherein depositing a material that blocks infrared light further comprises depositing SK-7000 resist material from Fujifilm Electronic Materials U.S.A., Inc., or depositing CFPR BK-8310 resist material Tokyo Ohka Kogyo (TOK) America, Inc., Milpitas, California, U.S.A.

### Claim 12

An apparatus, comprising:
a semiconductor die having bond pads on a device side surface, having a backside surface opposite the device side surface and having four sides extending between the device side surface and the backside surface;
a layer of light blocking material deposited on the device side surface, the light blocking material also covering the four sides extending between the device side surface;
semiconductor material on the exterior of the light blocking material covering the four sides, the semiconductor material spaced from the semiconductor device die by the light blocking material covering the four sides;
a backside coating of light blocking tape covering the backside surface;
openings in the layer of light blocking material on the device side surface, the openings exposing under-bump material formed on the bond pads; and
terminals that are formed by solder bumps or conductive post connects formed on the under-bump material.

### Claim 13 (depends on 12)

The apparatus of claim 12, wherein the terminals that are formed by solder bumps or conductive post connects formed on the under-bump material further comprise:
copper pillars formed on the under-bump material and extending away from the device side surface of the semiconductor die to a distal end; and
solder bumps formed on the distal end of the copper pillars, the copper pillars and the solder bumps forming copper pillar bumps.

### Claim 14 (depends on 12)

The apparatus of claim 12, wherein terminals that are formed by solder bumps or conductive post connects formed on the under-bump material are solder bumps formed by a solder ball drop and reflow process.

### Claim 15 (depends on 12)

The apparatus of claim 12, wherein the layer of light blocking material and the backside coating of light blocking material block infrared light.

### Claim 16 (depends on 12)

The apparatus of claim 12, wherein the layer of light blocking material comprises a black matrix resist.

### Claim 17 (depends on 16)

The apparatus of claim 16, wherein the layer of light blocking material comprises an infrared blocking resist.

### Claim 18 (depends on 17)

The apparatus of claim 17, wherein the layer of light blocking material comprises SK-7000 resist material from Fujifilm Electronic Materials U.S.A., Inc., or CFPR BK-8310 resist material from Tokyo Ohka Kogyo (TOK) America, Inc.

### Claim 19 (depends on 12)

The apparatus of claim 12, wherein the backside coating of light blocking tape comprises Adwill LC backside coating tape from LINTEC OF AMERICA, INC.

### Claim 20

A method for forming wafer-level chip scale packaged semiconductor devices, comprising:
forming under-bump metallization material on bond pads of semiconductor dies arranged in rows and columns on a device side surface of a semiconductor wafer, the semiconductor dies spaced from one another by scribe lanes of less than 50 microns width from die edge to die edge;
forming trenches adjacent the scribe lanes extending from the device side surface into but not through the semiconductor wafer along edges of the semiconductor dies;
depositing light blocking material over the device side surface of the semiconductor wafer, the light blocking material filling the trenches to form filled trenches and forming a layer of the light blocking material covering the device side surface of the semiconductor dies, the layer of light blocking material having a thickness of about 10 microns or less;
patterning the layer of light blocking material to expose the under-bump metallization material over the bond pads of the semiconductor dies and to expose the scribe lanes between the filled trenches;
forming solder bumps on the under-bump metallization;
backgrinding a backside surface of the semiconductor wafer to thin the semiconductor wafer and to expose the light blocking material in the filled trenches at the backside surface;
depositing a light blocking backside coating tape on the backside surface;
dicing the semiconductor wafer along the scribe lanes using laser dicing or plasma dicing, the dicing leaving semiconductor material edges along the filled trenches on the sides of the semiconductor dies; and
expanding the semiconductor wafer to separate the semiconductor dies from one another to form packaged semiconductor devices.

### Claim 21 (depends on 20)

The method of claim 20, wherein expanding the semiconductor wafer to separate the semiconductor dies from one another to form packaged semiconductor devices further comprises: forming the packaged semiconductor devices having the layer of light blocking material over the device side surface, having the light blocking backside coating tape on the backside surface opposite the device side surface, and having the light blocking material on the four sides between the device side surface and the backside surface, whereby exterior surfaces of the packaged semiconductor devices are covered with light blocking material.

### Claim 22 (depends on 21)

The method of claim 21, and further comprising leaving semiconductor material edges on the exterior surfaces of the four sides of the packaged semiconductor devices, the semiconductor material edges spaced from the semiconductor dies by the light blocking material.