# US 2025/0218773 A1 · Amorphous carbon film and deposition method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0218773 A1
- Document ID: US20250218773A1
- Status: Published application
- Kind: A1
- Application number: 19/002,154
- Filed: 2024-12-26
- Published: 2025-07-03
- Earliest claimed: 2023-12-27
- Assignees: Tes Co., Ltd
- Applicants: TES Co., Ltd
- Inventors: Seung Hwan JEON; Hye Ok KIM; Sungho KIM
- Web page: https://patentgrep.com/patent/US20250218773A1

## CPC

- H10P 76/405: {characterised by their composition, e.g. multilayer masks}
- C23C 16/26: Deposition of carbon only
- C23C 16/45523: {Pulsed gas flow or change of composition over time}
- C23C 16/46: characterised by the method used for heating the substrate (C23C16/48, C23C16/50 take precedence)
- C23C 16/50: using electric discharges {(generation and control of plasma in discharge tubes for surface treatment H01J37/32, H01J37/34)}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

Disclosed are an amorphous carbon film having excellent film quality such as hardness, modulus, density, and the like, and a deposition method thereof. The method for depositing the amorphous carbon film includes (a) loading a substrate into a chamber; (b) supplying a carbon precursor and a nitrogen gas into the chamber; (c) raising a temperature of the substrate to 350 to 450° C.; and (d) discharging the carbon precursor and the nitrogen gas in the chamber to deposit a nitrogen-doped amorphous carbon film on the substrate, wherein a flow rate of the nitrogen gas is in a range of about 1500 to 4000 sccm during the step (d).

## Claims

### Claim 1

A method for depositing an amorphous carbon film, the method comprising:
(a) loading a substrate into a chamber;
(b) supplying a carbon precursor and a nitrogen gas into the chamber;
(c) raising a temperature of the substrate to 350 to 450° C.; and
(d) discharging the carbon precursor and the nitrogen gas in the chamber to deposit a nitrogen-doped amorphous carbon film on the substrate,
wherein a flow rate of the nitrogen gas is in a range of about 1500 to 4000 sccm during the step (d).

### Claim 2 (depends on 1)

The method for depositing the amorphous carbon film of claim 1, wherein the carbon precursor together with a carrier gas is supplied into the chamber, wherein the carrier gas includes argon gas.

### Claim 3 (depends on 2)

The method for depositing the amorphous carbon film of claim 2, wherein the carrier gas is free of helium gas.

### Claim 4 (depends on 2)

The method for depositing the amorphous carbon film of claim 2, wherein the argon gas is supplied at a flow rate of about 3000 sccm or smaller.

### Claim 5 (depends on 1)

The method for depositing the amorphous carbon film of claim 1, wherein the carbon precursor is a carbon precursor in a gaseous state at room temperature.

### Claim 6 (depends on 5)

The method for depositing the amorphous carbon film of claim 5, wherein the carbon precursor is selected from C2H2, C2H4, C2H6, C3H6 and C3H8.

### Claim 7 (depends on 1)

The method for depositing the amorphous carbon film of claim 1, wherein in the step (d), a high frequency power of about 1500 W or greater is applied.

### Claim 8 (depends on 1)

The method for depositing the amorphous carbon film of claim 1, wherein in the step (d), both a high frequency power of about 1500 W or greater and a low frequency power of about 1000 W or lower are applied.

### Claim 9 (depends on 1)

The method for depositing the amorphous carbon film of claim 1, wherein the step (d) is performed at a pressure of about 5 to 9 Torr.