# US 2025/0215329 A1 · Method and system for treating polymer waste comprising heteroatomic polymers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0215329 A1
- Document ID: US20250215329A1
- Status: Published application
- Kind: A1
- Application number: 18/851,833
- Filed: 2023-03-23
- Published: 2025-07-03
- Earliest claimed: 2022-03-28
- Applicants: Pointbreak AS
- Inventors: Tina KRISTIANSEN; Siw Bodil FREDRIKSEN
- Web page: https://patentgrep.com/patent/US20250215329A1

## CPC

- C10B 53/07: {of solid raw materials consisting} of synthetic polymeric materials, e.g. tyres (recovery or working-up of waste materials of organic macromolecular compounds or compositions based thereon by dry-heat treatment for obtaining partially depolymerised materials C08J11/10; production of liquid hydrocarbon mixtures from rubber or rubber waste C10G1/10)
- C10G 1/10: from rubber or rubber waste
- C10G 47/22: Non-catalytic cracking in the presence of hydrogen
- C10G 2300/1088: Olefins
- C10G 2300/202: Heteroatoms content, i.e. S, N, O, P
- C10B: DESTRUCTIVE DISTILLATION OF CARBONACEOUS MATERIALS FOR PRODUCTION OF GAS, COKE, TAR, OR SIMILAR MATERIALS (cracking oils C10G; underground gasification of minerals E21B43/295)
- C10G: CRACKING HYDROCARBON OILS; PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVE HYDROGENATION, OLIGOMERISATION, POLYMERISATION (cracking to hydrogen or synthesis gas C01B; cracking or pyrolysis of hydrocarbon gases to individual hydrocarbons or mixtures thereof of definite or specified constitution C07C; cracking to cokes C10B); RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, OR GASES; REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS; REFORMING OF NAPHTHA; MINERAL WAXES

## Abstract

The present invention relates to a method for producing a hydrocarbon product from mixed polymer waste, preferably plastic waste and/or post consumer plastic waste, wherein said mixed polymer waste comprises 50-99.5 wt % polyolefins and 0.5-50 wt % polymer comprising heteroatoms, based on the total weight of the mixed polymer waste, comprising: (i) feeding said mixed polymer waste into an extruder, preferably a single screw extruder; (ii) adding chemicals, preferably alkali metal salt and/or alkali earth metal salt, to said mixed polymer waste to degrade said polymer comprising heteroatoms; (iii) removing degradation products derived from said polymer comprising heteroatoms from said hydrocarbon product; and (iv) collecting the hydrocarbon product. The method and system of the present invention may be used as a pre-treatment in recycling mixed polymer waste to produce a hydrocarbon product ideally suited for pyrolysis.

## Claims

### Claim 1

A method for producing a hydrocarbon product from mixed polymer waste, wherein said mixed polymer waste comprises 50-99.5 wt % polyolefins and 0.5-50 wt % polymer comprising heteroatoms, based on the total weight of the mixed polymer waste, comprising:
(i) feeding said mixed polymer waste into an extruder;
(ii) adding chemicals, to said mixed polymer waste to degrade said polymer comprising heteroatoms;
(iii) removing degradation products derived from said polymer comprising heteroatoms from said hydrocarbon product; and
(iv) collecting the hydrocarbon product.

### Claim 2 (depends on 1)

A method as claimed in claim 1, wherein said mixed polymer waste comprises 50-99 wt % polyolefins, based on the total weight of the mixed polymer waste composition.

### Claim 3 (depends on 1)

A method as claimed in claim 1, wherein said polyolefins are selected from polyethylene, polypropylene, polystyrene and mixtures thereof.

### Claim 4 (depends on 1)

A method as claimed in claim 1, wherein said mixed polymer waste comprises 1-50 wt % polymer comprising heteroatoms, based on the total weight of the mixed polymer waste composition.

### Claim 5 (depends on 1)

A method as claimed in any claim 1, wherein said polymer comprising heteroatoms is selected from polyethylene terephthalate (PET), polyamide (PA), polyurethane (PU), biopolymers (e.g. polylactic acid, polyhydroxyalkanoates), cellulose, poly(ethylene-co-vinyl acetate) (EVA), poly(vinyl alcohol-co-ethylene) (EVOH), polycarbonate, poly(acrylonitrile-co-butadiene-co-styrene) (ABS), poly(styrene-co-acrylonitrile) (SAN), polymethylmethacrylate (PMMA) and mixtures thereof.

### Claim 6 (depends on 1)

A method as claimed in claim 1, wherein said mixed polymer waste further comprises non-polymeric compounds comprising heteroatoms.

### Claim 7 (depends on 1)

A method as claimed in claim 1, wherein said mixed polymer waste is mixed with alkali metal salt, and/oralkali earth metal salt prior to feeding said mixed polymer waste to the extruder.

### Claim 8 (depends on 7)

A method as claimed in claim 7, wherein the mixture of alkali metal salt and/or alkali earth metal salt and mixed polymer waste is all fed into the extruder

### Claim 9 (depends on 1)

A method as claimed in claim 1, wherein said extruder is at a temperature of at least 300° C.

### Claim 10 (depends on 1)

A method as claimed in claim 1, wherein the residence time of said mixed polymer waste in said extruder is 0.1-20 minutes.

### Claim 11 (depends on 1)

A method as claimed in claim 1, wherein said polymers comprising heteroatoms and optionally non-polymeric compounds comprising heteroatoms, are simultaneously degraded in said extruder.

### Claim 12 (depends on 1)

A method as claimed in claim 1, wherein the degradation products derived from the polymer comprising heteroatoms, and optionally from non-polymeric compounds comprising heteroatoms, are removed in the form of volatiles and via a devolatization outlet of the extruder, the extruder die or a devolatization unit connected to the extruder exit.

### Claim 13 (depends on 1)

A method as claimed in claim 1, wherein the degradation products derived from the polymer comprising heteroatoms, and optionally from non-polymeric compounds comprising heteroatoms, are removed in the form of solids and via a melt filter.

### Claim 14 (depends on 1)

A method as claimed in claim 1, wherein said hydrocarbon product comprises 0-5 wt % polyethylene terephthalate (PET), based on the total weight of the hydrocarbon product, and/or said hydrocarbon product comprises 0-5 wt % polyamide (PA), based on the total weight of the hydrocarbon product.

### Claim 15 (depends on 1)

A method as claimed in claim 1, wherein said polyolefins present in said mixed polymer waste undergo cracking in said extruder, and preferably wherein said hydrocarbon product has:
a lower weight average molecular weight than said mixed polymer waste;
a lower complex viscosity, Eta (0.5) than said mixed polymer waste;
a lower complex viscosity, Eta (200) than said mixed polymer waste; and/or
a higher MFR2 than said mixed polymer waste.

### Claim 16 (depends on 1)

A method as claimed in claim 1, further comprising pyrolysis of said hydrocarbon product.

### Claim 17

A system for producing a hydrocarbon product from mixed polymer waste, comprising:
an extruder for conversion of mixed polymer waste comprising 50-99.5 wt % polyolefins and 0.5-50 wt % polymer comprising heteroatoms into a mixture of hydrocarbon product and degradation products derived from the polymer comprising heteroatoms;
a melt filter for receiving the mixture of hydrocarbon product and degradation products from the extruder and removing solid degradation products from said hydrocarbon product; and
a degassing unit for receiving the hydrocarbon product from the melt filter and removing volatile degradation products from said hydrocarbon product.

### Claim 18 (depends on 1)

A method for recycling mixed polymer waste comprising a pre-treatment to remove polymer comprising heteroatoms, wherein said pre-treatment comprises a method as defined in claim 1.

### Claim 19

A system for recycling mixed polymer waste, comprising:
an extruder for conversion of mixed polymer waste comprising 50-99.5 wt % polyolefins and 0.5-50 wt % polymer comprising heteroatoms, and chemicals into a mixture of hydrocarbon product and degradation products derived from the polymer comprising heteroatoms;
a melt filter for receiving the mixture of hydrocarbon product and degradation products from the extruder and removing solid degradation products from said hydrocarbon product;
a degassing unit for receiving the hydrocarbon product from the melt filter and removing volatile degradation products from said hydrocarbon product; and
a pyrolysis unit for receiving the hydrocarbon product from the degassing unit and pyrolysing said the hydrocarbon product.