# US 2025/0215210 A1 · Diene rubber composition and method for producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0215210 A1
- Document ID: US20250215210A1
- Status: Published application
- Kind: A1
- Application number: 18/851,308
- Filed: 2023-03-30
- Published: 2025-07-03
- Earliest claimed: 2022-03-31
- Assignees: ETIC Inc.
- Applicants: ETIC Inc.
- Inventors: Iwakazu Hattori; Hisao Ono; Motokazu Mizutani
- Web page: https://patentgrep.com/patent/US20250215210A1

## CPC

- C08C 19/25: Incorporating silicon atoms into the molecule
- C08L 55/005: {Homopolymers or copolymers obtained by polymerisation of macromolecular compounds terminated by a carbon-to-carbon double bond}
- C08C 1/14: Coagulation
- C08C 19/22: Incorporating nitrogen atoms into the molecule
- C08C 19/44: of polymers containing metal atoms exclusively at one or both ends of the skeleton
- C08F 290/048: {Polymers of monomers having two or more carbon-to-carbon double bonds as defined in group C08F36/00}
- C08J 3/246: {Intercrosslinking of at least two polymers}
- C08K 3/04: Carbon
- C08K 3/36: Silica
- C08L 15/00: Compositions of rubber derivatives (C08L11/00, C08L13/00 take precedence)
- C08G 81/024: {Block or graft polymers containing sequences of polymers of C08C or C08F and of polymers of C08G}
- C08J 2353/02: of vinyl aromatic monomers and conjugated dienes
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2312/02: with dienes
- C08C: TREATMENT OR CHEMICAL MODIFICATION OF RUBBERS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

The present invention addresses the problem of providing: a conjugated diene rubber composition which has excellent rebound resilience and wear resistance, while exhibiting good workability during rubber kneading and excellent wet grip performance; and a method for producing this conjugated diene rubber composition. The present invention provides a diene rubber composition which is obtained by subjecting a mixture of a diene rubber component 1 that is obtained by terminally modifying a conjugated diene polymer 1 with at least one silicon compound that is represented by formula (1) and/or formula (2) and a diene rubber component 2 that is obtained by terminally modifying a conjugated diene polymer 2 with at least one silicon compound that is represented by formula (1) and/or formula (2) to a hydrolysis process, and subsequently drying the resulting product.

## Claims

### Claim 1

A diene rubber composition which is obtained by subjecting a diene rubber component 1, that is obtained by terminally modifying a conjugated diene polymer 1 with at least one silicon compound that is represented by formula (1) and/or formula (2), and a diene rubber component 2, that is obtained by terminally modifying a conjugated diene polymer 2 with at least one silicon compound that is represented by formula (1) and/or formula (2), to a hydrolysis process, and subsequently drying the resulting product,
wherein the conjugated diene polymer 1 is obtained by polymerizing a conjugated diene compound and an aromatic vinyl compound, and has a peak molecular weight in terms of polystyrene of 400 k to 2,000 kg/mol,
and wherein the conjugated diene polymer 2 is obtained by polymerizing a conjugated diene compound and an aromatic vinyl compound, and has a peak molecular weight in terms of polystyrene of 15 k to 60 kg/mol,
(X1)n(R1O)—Si—(R2)4-n-m Formula (1)
wherein R1 and R2 are each independently an alkyl group, an aromatic group, or an allyl group which has 1 to 12 carbon atoms, or an alkyl group, an aromatic group, or an allyl group which contains an oxygen atom and/or a nitrogen atom in the group, wherein X1 is iodine, bromine, or chlorine, and each of n and m are 0, 1, 2, 3, or 4,
wherein R3 to R8 are each independently an alkyl group, an aromatic group, or an allyl group which has 1 to 12 carbon atoms, or an alkyl group, an aromatic group, or an allyl group which contains an oxygen atom and/or a nitrogen atom in the group, and may also be a cyclic structure without R7 and R8, and p is a number between 1.5 and 1,000 in increments of 0.5.

### Claim 2 (depends on 1)

The diene rubber composition according to claim 1, wherein 1, 2-structure or 3, 4-structure of the diene part in the diene rubber component 1 is 20 to 70% and weight ratio of aromatic vinyl compound component in the diene rubber component 1 is 10 to 50%, and wherein 1, 2-structure or 3, 4-structure of the diene part in the diene rubber component 2 is 40 to 80% and weight ratio of aromatic vinyl compound component in the diene rubber component 2 is 5 to 35%.

### Claim 3 (depends on 1)

The diene rubber composition according to claim 1, wherein the ratio between the diene rubber component 1 and the diene rubber component 2 is 10 to 90 phr of the diene rubber component 2 for 100 phr of the diene rubber component 1.

### Claim 4 (depends on 2)

A rubber compounded composition comprising at least 20 to 150 phr of silica for 100 phr of the total rubber component, wherein said 100 phr of the total rubber component contains at least 20 phr of the diene rubber composition according to claim 2.

### Claim 5 (depends on 2)

A rubber compounded composition comprising at least 20 to 150 phr of silica and 5 to 30 phr of carbon black for 100 phr of an entire rubber component, wherein said 100 phr of the total rubber component contains at least 20 phr of the diene rubber composition according to claim 2.

### Claim 6

A method for producing a diene rubber composition, comprising steps of:
i) initiating polymerization of a conjugated diene compound and an aromatic vinyl compound in a hydrocarbon in the presence of an organolithium compound;
ii) producing diene rubber component 1 by terminally modifying a conjugated diene polymer 1, which was polymerized in the step i) and has a peak molecular weight in terms of polystyrene of 400 k to 2,000 kg/mol, right after the polymerization with at least one silicon compound that is represented by formula (1) and/or formula (2);
iii) producing diene rubber component 2 by terminally modifying a conjugated diene polymer 2, which was polymerized in the step i) and has a peak molecular weight in terms of polystyrene of 15 k to 60 kg/mol, right after the polymerization with at least one silicon compound that is represented by formula (1) and/or formula (2);
iv) subjecting the obtained diene rubber component 1 and diene rubber component 2 to a hydrolysis step, preferably steam coagulation, and subsequently drying the resulting product;
(X1)n(R1O)—Si—(R2)4-n-m Formula (1)
wherein R1 and R2 are each an alkyl group, an aromatic group, or an allyl group which has 1 to 12 carbon atoms, or an alkyl group, an aromatic group, or an allyl group which contains an oxygen atom and/or a nitrogen atom in the group, wherein X1 is a halogen atom of iodine, bromine, or chlorine, and each of n and m are 0, 1, 2, 3, or 4,
wherein R3 to R8 are each independently an alkyl group, an aromatic group, or an allyl group which has 1 to 12 carbon atoms, or an alkyl group, an aromatic group, or an allyl group which contains an oxygen atom and/or a nitrogen atom in the group, and may also be a cyclic structure without R7 and R8, and p is a number between 1.5 and 1,000 in increments of 0.5.

### Claim 7 (depends on 6)

The method according to claim 6, wherein polymerization of diene rubber component 1 alone or both diene rubber component 1 and diene rubber component 2 is initiated in the presence of an organolithium compound and a secondary amine compound.

### Claim 8 (depends on 6)

The method according to claim 6, wherein, during polymerization of diene rubber component 1, after preliminarily polymerizing isoprene with an organolithium compound, conjugated diene compound other than isoprene and an aromatic vinyl compound are polymerized.

### Claim 9 (depends on 6)

The method according to claim 6, wherein, after polymerization of the diene rubber component 1, conjugated diene compound, aromatic vinyl compound, and optionally 1,2- or 3,4-structure modifiers of the diene part are added, and then polymerization is resumed in the presence of organic lithium compounds.

### Claim 10 (depends on 6)

The method according to claim 6, wherein after the step iii) and before the step iv), the steam coagulation/drying of the step iv) are performed after addition of a halogenated silicon compound represented by formula (3) or an alkali metal compound represented by formula (4) in an amount satisfying the conditions of formula (5),
(R9)q-M1(X2) Formula (3)
wherein M1 is a silicon atom, R9 is an alkyl group, aromatic group, or allyl group which has 1 to 12 carbons, X2 is a halogen atom of iodine, bromine, or chlorine, and q is 0 or 1,
R10—OM2 Formula (4)
wherein M2 is an alkali metal atom, preferably a lithium, sodium, or potassium atom, and R10 is an alkyl group, aromatic group, allyl group, or acyl group which has 1 to 12 carbons,
1.5≥[nX1+(4-q)X2]/(L+M2)≥0.9 Formula (5)
wherein L is the number of moles of organolithium compound added at the initiation of polymerization, M2 is the number of moles of alkali metal compound represented by formula (4), X1 is the number of moles of silicon compound represented by formula (1), X2 is the number of moles of halogenated silicon compound represented by formula (3), n is the same as n in the silicon compound represented by formula (1) and q is the same as q in the halogenated silicon compound represented by formula (3).

### Claim 11 (depends on 6)

The method according to claim 6, wherein the ratio between the diene rubber component 1 and the diene rubber component 2 is 10 to 90 phr of the diene rubber component 2 for 100 phr of the diene rubber component 1.