# US 2025/0214838 A1 · Method for producing high-purity alkali metal sulfide

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0214838 A1
- Document ID: US20250214838A1
- Status: Published application
- Kind: A1
- Application number: 18/851,868
- Filed: 2023-03-27
- Published: 2025-07-03
- Earliest claimed: 2022-03-31
- Assignees: Solivis Inc.
- Applicants: Solivis Inc.
- Inventors: Dong Wook SHIN; Young Min LEE; Sang Ho PARK; Sung Jae KIM
- Web page: https://patentgrep.com/patent/US20250214838A1

## CPC

- C01B 17/28: with reducing gases
- C01B 17/36: Purification
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2002/82: by IR- or Raman-data
- C01P 2006/80: Compositional purity
- Y02E 60/10: Energy storage using batteries
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

One embodiment of the present disclosure includes a method of producing high-purity alkali metal sulfide including mixing an alkali metal sulfide salt precursor and a reducing agent to form a mixture, reducing the mixture to obtain alkali metal sulfide; and purifying the obtained alkali metal sulfide.

## Claims

### Claim 1

A method of producing high-purity alkali metal sulfide, comprising:
mixing an alkali metal sulfide salt precursor and a reducing agent to form a mixture;
reducing the mixture to obtain alkali metal sulfide; and
purifying the alkali metal sulfide which is obtained.

### Claim 2 (depends on 1)

The method of producing high-purity alkali metal sulfide claim 1, wherein
in the mixing, the mixture is formed in a non-polar solvent.

### Claim 3 (depends on 1)

The method of producing high-purity alkali metal sulfide of claim 1, wherein
in the reducing, the mixture is reduced by a reducing gas.

### Claim 4 (depends on 3)

The method of producing high-purity alkali metal sulfide of claim 3, wherein
the reducing gas comprises hydrogen and at least one selected from the group consisting of carbon monoxide, nitrogen, argon, helium, neon, methane, ethane, propane, and butane.

### Claim 5 (depends on 1)

The method of producing high-purity alkali metal sulfide of claim 1, wherein
the reducing comprises heat-treating.

### Claim 6 (depends on 5)

The method of producing high-purity alkali metal sulfide of claim 5, wherein
the heat-treatment is performed at 800° C. to 1500° C.

### Claim 7 (depends on 1)

The method of producing high-purity alkali metal sulfide of claim 1, wherein
in the purifying, the alkali metal sulfide which is obtained is purified using a polar solvent.

### Claim 8 (depends on 7)

The method of producing high-purity alkali metal sulfide of claim 7, wherein
a polarity index of the polar solvent is 4.3 to 6.2.

### Claim 9 (depends on 7)

The method of producing high-purity alkali metal sulfide of claim 7, wherein
in the purifying, the alkali metal sulfide which is obtained is dissolved in the polar solvent.

### Claim 10 (depends on 1)

The method of producing high-purity alkali metal sulfide of claim 1, further comprising
crystallizing the alkali metal sulfide after the purifying.

### Claim 11 (depends on 10)

The method of producing high-purity alkali metal sulfide of claim 10, wherein
the crystallizing is performed by heat-treating at 300° C. to 1000° C.