# US 2025/0210697 A1 · Composite solid-state electrolyte, method of preparing the same, and lithium battery comprising the solid-state electrolyte

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0210697 A1
- Document ID: US20250210697A1
- Status: Published application
- Kind: A1
- Application number: 18/985,549
- Filed: 2024-12-18
- Published: 2025-06-26
- Earliest claimed: 2023-12-20
- Assignees: Samsung Electronics Co., Ltd.
- Applicants: Samsung Electronics Co., Ltd.
- Inventors: Taeyoung Kim; Giyun Kwon; Youngjoon Bae; Jeongkuk Shon; Heungchan Lee
- Web page: https://patentgrep.com/patent/US20250210697A1

## CPC

- H01M 10/0562: Solid materials
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2300/0071: Oxides
- H01M 2300/0077: based on zirconium oxide
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A composite solid-state electrolyte, a method of preparing the same, and a lithium battery including the same. The composite solid-state electrolyte includes a first solid-state electrolyte including a cubic garnet phase and a pyrochlore phase, and a second solid-state electrolyte including a glass phase, and a volume of the first solid-state electrolyte is greater than that of the second solid-state electrolyte, based on a total volume of the composite solid-state electrolyte.

## Claims

### Claim 1

A composite solid-state electrolyte comprising:
a first solid-state electrolyte comprising a cubic garnet phase and a pyrochlore phase; and
a second solid-state electrolyte comprising a glass phase,
wherein a volume of the first solid-state electrolyte is greater than a volume of the second solid-state electrolyte, based on a total volume of the composite solid-state electrolyte.

### Claim 2 (depends on 1)

The composite solid-state electrolyte of claim 1, wherein a crystallization temperature T1 of the first solid-state electrolyte is less than a crystallization temperature T2 of the second solid-state electrolyte.

### Claim 3 (depends on 1)

The composite solid-state electrolyte of claim 1, wherein a crystallization temperature of the first solid-state electrolyte is about 300° C. to about 450° C., and
a crystallization temperature of the second solid-state electrolyte is about 450° C. to about 600° C.

### Claim 4 (depends on 1)

The composite solid-state electrolyte of claim 1, wherein the composite solid-state electrolyte includes a heat treatment product of a composite solid-state electrolyte-forming composition comprising a first solid-state electrolyte precursor and a second solid-state electrolyte precursor, and a heat treatment temperature T of the composite solid-state electrolyte-forming composition is 550° C. or less, and
the crystallization temperature T1 of the first solid-state electrolyte, the heat treatment temperature T of the composite solid-state electrolyte-forming composition, and the crystallization temperature T2 of the second solid-state electrolyte satisfy Expression 1:
T
⁢
1
<
T
<
T
2.
Expression
⁢
1

### Claim 5 (depends on 1)

The composite solid-state electrolyte of claim 1, wherein a crystal phase of the first solid-state electrolyte has a size of about 50 nanometers to about 50 micrometers.

### Claim 6 (depends on 1)

The composite solid-state electrolyte of claim 1, wherein the composite solid-state electrolyte has an ionic conductivity of about 1×10−6 siemens per centimeter to about 1×10−3 siemens per centimeter and a relative density of about 80% to about 95%, based on a theoretical density of the composite solid-state electrolyte.

### Claim 7 (depends on 1)

The composite solid-state electrolyte of claim 1, wherein an amount of the first solid-state electrolyte is greater than 50 volume percent and 99 volume percent or less, based on a total volume of the composite solid-state electrolyte.

### Claim 8 (depends on 1)

The composite solid-state electrolyte of claim 1, wherein the first solid-state electrolyte comprises a compound represented by Formula 1:
(LixAa)(LayB′b)(ZrzC′c)O12 Formula 1
wherein in Formula 1, A is a monovalent cation, a divalent cation, a trivalent cation, or a combination thereof,
B′ is a monovalent cation, a divalent cation, a trivalent cation, or a combination thereof,
C′ is a monovalent cation, a divalent cation, a trivalent cation, a tetravalent cation, a pentavalent cation, a hexavalent cation, or a combination thereof,
6≤x≤8, 0≤a≤2, 2≤y≤3, 0≤b≤1, 0<z≤2, and 0≤c≤2.

### Claim 9 (depends on 8)

The composite solid-state electrolyte of claim 8, wherein the first solid-state electrolyte comprises a compound represented by Formula 2, a compound represented by Formula 3, or a combination thereof:
Lix(LayB′b)(ZrzC′c)O12 Formula 2
wherein in Formula 2, B′ comprises at least one of calcium, strontium, cesium, or barium,
C′ comprises at least one of aluminum, tungsten, niobium or tantalum,
6≤x≤8, 2≤y≤3, 0<z≤2, 0<b≤1, and 0.01≤c≤2, or
(LixAa)(Lay)(Zrz)O12 Formula 3
wherein in Formula 3, A comprises at least one of gallium or aluminum, 6≤x≤8, 0≤a≤2, 2≤y≤3, and 0<z≤2.

### Claim 10 (depends on 8)

The composite solid-state electrolyte of claim 8, wherein the solid-state electrolyte represented by Formula 1 is a compound represented by Formula 4:
Li3+xLa3Zr2aC′aO12 Formula 4
wherein, in Formula 4, C′ may include at least one of aluminum, tungsten, niobium or tantalum, 3≤x≤5 and 0≤a≤0.7.

### Claim 11 (depends on 1)

The composite solid-state electrolyte of claim 1, wherein the second solid-state electrolyte is an oxide glass comprising lithium, oxygen, and at least one of germanium, silicon, boron, or phosphorus.

### Claim 12 (depends on 1)

The composite solid-state electrolyte of claim 1, wherein the second solid-state electrolyte comprises a glass comprising SiO2, B2O3, and Li2O,
wherein an amount of the Li2O is 20 mole percent to 75 mole percent, an amount of the SiO2 is greater than 0 mole percent to 70 mole percent, and an amount of the B2O3 is greater than 0 mole percent to 60 mole percent.

### Claim 13 (depends on 1)

The composite solid-state electrolyte of claim 1, wherein, when analyzed by X-ray diffraction using CuKa radiation, peaks of the pyrochlore phase are observed at diffraction angles of about 27.5°2θ to about 29°2θ, about 32°2θ to about 33.5°2θ, about 46.5°2θ to about 48°2θ, and about 55°2θ to about 56.5°2θ.

### Claim 14 (depends on 1)

A lithium battery comprising:
a positive electrode;
a negative electrode; and
an electrolyte layer disposed between the positive electrode and the negative electrode,
wherein at least one of the positive electrode, the negative electrode, or the electrolyte layer comprises the composite solid-state electrolyte of claim 1.

### Claim 15 (depends on 14)

The lithium battery of claim 14, wherein the positive electrode comprises:
a first solid-state electrolyte including a cubic garnet phase and a pyrochlore phase; and
a second solid-state electrolyte including a glass phase,
wherein a volume of the first solid-state electrolyte is greater than a volume of the second solid-state electrolyte, based on a total volume of the composite solid-state electrolyte.

### Claim 16

A method of preparing a composite solid-state electrolyte comprising a first solid-state electrolyte and a second solid-state electrolyte,
wherein the first solid-state electrolyte comprises a cubic garnet phase and a pyrochlore phase, and the second solid-state electrolyte comprises a glass phase, and
wherein a volume of the first solid-state electrolyte is greater than a volume of the second solid-state electrolyte, based on a total volume of the composite solid-state electrolyte, the method comprising:
mixing a first solid-state electrolyte precursor comprising an amorphous phase and a second solid-state electrolyte precursor comprising a glass phase to prepare a composite solid-state electrolyte-forming composition; and
heat-treating the composite solid-state electrolyte-forming composition to prepare the composite solid-state electrolyte.

### Claim 17 (depends on 16)

The method of claim 16, wherein the second solid-state electrolyte comprising a glass phase is an oxide glass comprising lithium, oxygen, and at least one of germanium, silicon, boron, or phosphorus.

### Claim 18 (depends on 16)

The method of claim 16, wherein the second solid-state electrolyte is a glass comprising SiO2, B2O3, and Li2O,
wherein an amount of the Li2O is about 20 mole percent to about 75 mole percent, an amount of the SiO2 is greater than 0 mole percent to about 70 mole percent, and an amount of the B2O3 is greater than 0 mole percent to about 60 mole percent.

### Claim 19 (depends on 16)

The method of claim 16, wherein the heat-treating of the composite solid-state electrolyte-forming composition is performed at a temperature greater than a crystallization temperature of a first solid-state electrolyte precursor and less than a crystallization temperature of a second solid-state electrolyte precursor, and
the heat-treating of the composite solid-state electrolyte-forming composition is performed at 550° C. or less.

### Claim 20 (depends on 1)

The composite solid-state electrolyte of claim 1, wherein the ratio of the cubic garnet phase to the pyrochlore phase is about 99.5:0.5 to about 3:2.