# US 2025/0210642 A1 · Cathode active materials, their manufacture and their use

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0210642 A1
- Document ID: US20250210642A1
- Status: Published application
- Kind: A1
- Application number: 18/847,385
- Filed: 2023-04-11
- Published: 2025-06-26
- Earliest claimed: 2022-04-19
- Assignees: BASF SE
- Applicants: BASF SE
- Inventors: Young Jin KIM; Jacob HAAG
- Web page: https://patentgrep.com/patent/US20250210642A1

## CPC

- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/364: {as mixtures}
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/625: {Carbon or graphite}
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Disclosed herein is a process for making an electrode active material for lithium-ion batteries. The process includes the steps of (a) providing a cathode active material (α) that has the general formula Li1+x1TM1−x1O2, (b) providing another cathode active material (β) that has the general formula Li1+x2TM1−x2O2, and (c) combining cathode active material (α) and cathode active material (β) in a mass ratio in the range of from 1:5 to 5:1.

## Claims

### Claim 1

A process for making an electrode active material for lithium-ion batteries, wherein said process comprises the steps of:
(a) providing a cathode active material (α) that has a general formula Li1+x1TM1−x1O2, wherein TM is a combination of metals according to a general formula (I), and x1 is in a range of from 0.05 to 0.3, and wherein the cathode active material (α) has a pressed density in a range of from 2.85 to 3.1 g/cm3, determined at 250 MPa;
(b) providing another cathode active material (β) that has a general formula Li1+x2TM1−x2O2, wherein TM is a combination of metals according to the general formula (I), wherein TM in the cathode active material (α) and the cathode active material (β) may be identical or different, and x2 is in a range of from 0.05 to 0.3, and wherein the cathode active material (β) has a pressed density in a range of from 2.50 to 2.80 g/cm3, determined at 250 MPa; and
(c) combining the cathode active material (α) and the cathode active material (β) in a mass ratio in a range of from 1:5 to 5:1,
(NiaCobMnc)1−dM1d (I),
wherein
a is in a range of from 0.30 to 0.38,
b is in a range of from zero to 0.05,
c is in a range of from 0.60 to 0.70, and
d is in a range of from zero to 0.05,
M1 is selected from Al, Ti, Zr, W, Mo, Mg, B, and combinations of at least two of the foregoing, and
a
+
b
+
c
=
1.

### Claim 2 (depends on 1)

A process according to claim 1, wherein TM in the cathode active materials (α) and (β) are substantially the same.

### Claim 3 (depends on 1)

A process according to claim 1, wherein the cathode active material (α) is treated with aqueous sulfuric acid before step (c).

### Claim 4 (depends on 1)

A process according to claim 1, wherein the cathode active material (β) is coated with a layer containing Al2O3 or a Li—Al oxide compound.

### Claim 5 (depends on 1)

A process according to claim 1, wherein a BET surface of the cathode active material (α) is lower than a BET surface of the cathode active material (β), and wherein each BET surface is determined by nitrogen adsorption after outgassing of a sample at 200° C. for 30 minutes or more and beyond this accordance with DIN ISO 9277:2010.

### Claim 6 (depends on 1)

A process according to claim 1, wherein at least one of the cathode active material (α) or the cathode active material (β) has an average particle diameter (D50) in a range of from 4 to 7 μm.

### Claim 7

A mixture comprising:
(a) a cathode active material (α) that has a general formula Li1+xTM1−z1O2, wherein TM is a combination of metals according to a general formula (I), and x1 is in a range of from 0.05 to 0.3, and wherein the cathode active material (α) has a pressed density in a range of from 2.85 to 3.1 g/cm3, determined at 250 MPa; and
(b) a cathode active material (β) that has a general formula Li1+x2TM1−x2O2, wherein TM is a combination of metals according to the general formula (I), wherein TM in the cathode active material (α) and the cathode active material (β) may be identical or different, and x2 is in a range of from 0.05 to 0.3, and wherein the cathode active material (β) has a pressed density in a range of from 2.50 to 2.80 g/cm3, determined at 250 MPa,
in a weight ratio in a range of from 1:5 to 5:1,
(NiaCobMnc)1−dM1d (I),
wherein
a is in a range of from 0.30 to 0.38,
b is in a range of from zero to 0.05,
c is in a range of from 0.60 to 0.70, and
d is in a range of from zero to 0.05,
M1 is selected from Al, Ti, Zr, W, Mo, Mg, B, and combinations of at least two of the foregoing, and
a
+
b
+
c
=
1.

### Claim 8 (depends on 7)

A mixture according to claim 7, wherein TM in the cathode active materials (α) and (β) are substantially the same.

### Claim 9 (depends on 7)

A mixture according to claim 7, wherein a BET surface of the cathode active material (α) is lower than a BET surface of the cathode active material (β), wherein determined by nitrogen adsorption after outgassing of a sample at 200° C. for 30 minutes or more and beyond this accordance with DIN ISO 9277:2010.

### Claim 10 (depends on 7)

A mixture according to claim 7, wherein at least one of the cathode active material (α) or the cathode active material (β) has an average particle diameter (D50) in a range of from 4 to 7 μm.

### Claim 11 (depends on 7)

A mixture according to any of the claim 7, wherein the cathode active material (β) is coated with a layer containing Al2O3 or a Li—Al oxide compound.

### Claim 12 (depends on 7)

A cathode comprising:
(A) at least one mixture according to claim 7;
(B) carbon in electrically conductive form; and
(C) a binder polymer.

### Claim 13 (depends on 12)

An electrochemical cell comprising at least one cathode according to claim 12.