# US 2025/0210585 A1 · Direct bonding of semiconductor elements

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0210585 A1
- Document ID: US20250210585A1
- Status: Published application
- Kind: A1
- Application number: 18/395,347
- Filed: 2023-12-22
- Published: 2025-06-26
- Earliest claimed: 2023-12-22
- Assignees: Adeia Semiconductor Bonding Technologies Inc.
- Applicants: Adeia Semiconductor Bonding Technologies Inc.
- Inventors: Gaius Gillman FOUNTAIN, JR.; George Carlton HUDSON
- Web page: https://patentgrep.com/patent/US20250210585A1

## CPC

- H10P 14/6927: {the material being a silicon oxynitride, e.g. SiON or SiON:H}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10W 72/01351: {Changing the shapes of die-attach connectors}
- H10W 72/073: {of die-attach connectors}
- H10W 72/07311: {Treating the bonding area before connecting, e.g. by applying flux or cleaning}
- H10W 72/07331: {Connecting techniques}
- H10W 72/351: {Materials of die-attach connectors}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

In the present disclosure, a first semiconductor element of a bonded structure comprises a semiconductor-containing oxynitride bonding layer formed on a first substrate layer comprising a semiconductor material, e.g., a single crystal silicon. The semiconductor-containing oxynitride bonding layer is formed by exposing an upper surface of the first substrate layer to products of plasma containing nitrogen and oxygen at controlled plasma conditions. The second semiconductor element of the bonded structure may have a second substrate layer comprising a semiconductor material, e.g., a single crystal silicon, and a semiconductor-containing oxynitride bonding layer formed over the second substrate layer in the same way as the first semiconductor element. In some embodiments, the second semiconductor element may have a bonding layer comprising a dielectric material. After initial direct bonding of the first and second semiconductor elements, the bonded structure may go through an annealing process to strengthen the bonding.

## Claims

### Claim 1

A method for forming a bonding layer on an upper surface of a semiconductor substrate, the method comprising:
exposing the upper surface of the semiconductor substrate to products of at least one plasma containing nitrogen and oxygen to form a semiconductor-containing oxynitride layer on the upper surface of the semiconductor substrate; and
preparing the upper surface for direct bonding to a semiconductor element, the preparing the upper surface comprising planarizing the upper surface.

### Claim 2 (depends on 1)

The method of claim 1, wherein the semiconductor substrate comprises bare silicon.

### Claim 3 (depends on 1)

The method of claim 1, wherein the semiconductor-containing oxynitride layer comprises silicon oxynitride.

### Claim 4 (depends on 1)

The method of claim 1, wherein exposing the upper surface of the semiconductor substrate to products of at least one plasma comprises exposing the upper surface of the semiconductor substrate to products of a remote plasma system.

### Claim 5 (depends on 1)

The method of claim 1, wherein exposing the upper surface of the semiconductor substrate to products of at least one plasma comprises exposing the upper surface of the semiconductor substrate to products of an in situ plasma system.

### Claim 6 (depends on 1)

The method of claim 1, wherein exposing the upper surface of the semiconductor substrate to products of at least one plasma comprises flowing the products of a plasma containing nitrogen and/or oxygen over the upper surface of the semiconductor at a flow rate of about 50 sccm to 200 sccm nitrogen and/or about 10 sccm to 50 sccm oxygen, wherein when the plasma contains both nitrogen and oxygen a ratio of nitrogen flow rate to oxygen flow rate ranges from 1:1 to 10:1.

### Claim 7 (depends on 1)

The method of claim 1, wherein exposing the upper surface of the semiconductor substrate to products of at least one plasma comprises performing the plasma process at a temperature in the range of 100° C.-300° C.

### Claim 8

(canceled)

### Claim 9 (depends on 1)

The method of claim 1, wherein exposing the upper surface of the semiconductor substrate to products of at least one plasma comprises performing the plasma process at a pressure in the range of 0.5-2 Torr.

### Claim 10 (depends on 1)

The method of claim 1, wherein exposing the upper surface of the semiconductor substrate to products of at least one plasma comprises performing the plasma process at a cyclic electrical power in the range of 50 W-200 W and at a cyclic frequency in the range of 40 KHz-1 MHz.

### Claim 11 (depends on 1)

A method for forming a bonded structure, comprising:
direct bonding the semiconductor-containing bonding layer formed on the semiconductor substrate according to the method of claim 1 to a second semiconductor element.

### Claim 12 (depends on 11)

The method of claim 11, wherein the semiconductor substrate comprises silicon, wherein a second semiconductor substrate of the second semiconductor element comprises silicon, and wherein direct bonding the semiconductor-containing bonding layer to the second semiconductor element comprises direct bonding the semiconductor-containing bonding layer to the second semiconductor substrate.

### Claim 13 (depends on 11)

The method of claim 11, further comprising:
forming a dielectric bonding layer over the second semiconductor substrate of the second semiconductor element; and
wherein direct bonding the semiconductor-containing bonding layer to the second semiconductor element comprises direct bonding the semiconductor-containing bonding layer to the dielectric bonding layer.

### Claim 14 (depends on 11)

The method of claim 11, further comprising:
forming a second semiconductor-containing bonding layer over the second semiconductor substrate of the second semiconductor element by exposing an upper surface of the second semiconductor substrate to products of at least one plasma containing nitrogen and oxygen; and
wherein direct bonding the semiconductor-containing bonding layer to the second semiconductor element comprises direct bonding the semiconductor-containing bonding layer to the second semiconductor-containing bonding layer.

### Claim 15

A method for forming a bonded structure, comprising:
providing a first semiconductor element having a base substrate layer comprising a semiconductor material;
forming a first bonding layer comprising a semiconductor-containing oxynitride material over the base substrate layer, the first bonding layer having a thickness in the range of 0.5 nm-10 nm, the first bonding layer having a first bonding surface;
providing a second semiconductor element having a second bonding surface; and
directly bonding the first bonding surface of the first semiconductor element to the second bonding surface of the second semiconductor element.

### Claim 16 (depends on 15)

The method of claim 15, wherein forming the first bonding layer comprises exposing an upper surface of the first semiconductor element to a nitrogen and oxygen containing plasma.

### Claim at position 17

-18. (canceled)

### Claim 19 (depends on 15)

The method of claim 15, further comprising forming a second bonding layer over a base substrate layer of the second semiconductor element, the base substrate layer of the second semiconductor element comprising a semiconductor material.

### Claim 20 (depends on 19)

The method of claim 19, wherein the second bonding layer comprises semiconductor-containing oxynitride material.

### Claim 21 (depends on 19)

The method of claim 19, wherein the second bonding layer comprises dielectric material.

### Claim 22 (depends on 21)

The method of claim 21, wherein the dielectric material is an oxide material.

### Claim 23 (depends on 15)

The method of claim 15, further comprising:
annealing the bonded structure at a temperature in the range of 100° C.-300° C. for a duration of 10 minutes to 1 hour.

### Claim 24 (depends on 23)

The method of claim 23, wherein the annealing the bonded structure comprises a temperature in the range of 150° C.-250° C. for a duration of 15 minutes to 30 minutes.

### Claim at position 24

-34. (canceled)