# US 2025/0210375 A1 · Surface treatment composition and method for producing wafer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0210375 A1
- Document ID: US20250210375A1
- Status: Published application
- Kind: A1
- Application number: 18/845,594
- Filed: 2023-04-05
- Published: 2025-06-26
- Earliest claimed: 2022-04-11
- Assignees: Central Glass Company, Limited
- Applicants: Central Glass Company, Limited
- Inventors: Yuzo OKUMURA; Yoshiharu TERUI; Ayaka YOSHIDA
- Web page: https://patentgrep.com/patent/US20250210375A1

## CPC

- H10W 74/01: Manufacture or treatment
- B05D 1/60: {Deposition of organic layers from vapour phase (vapour phase deposition in general C23C14/00, C23C16/00)}
- C09D 5/00: Coating compositions, e.g. paints, varnishes or lacquers, characterised by their physical nature or the effects produced {(electrically insulating plastics, resins or waxes H01B3/30)}; Filling pastes
- C09D 7/20: Diluents or solvents
- H10P 70/15: {by wet cleaning only (H10P70/52 takes precedence)}
- H10P 70/20: {Cleaning during device manufacture}
- H10P 70/50: {characterised by the part to be cleaned}
- H10W 42/00: Arrangements for protection of devices (arrangements for thermal protection H10W40/00)
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The present invention is a surface treatment composition which is supplied as vapor to the surface of a wafer having an uneven pattern on the surface and is used for forming a water-repellent protective film on the surface, the surface treatment composition including a silylating agent and a solvent, in which the silylating agent includes a silicon compound represented by (R1)3Si-X (R1's are each independently a group selected from the group consisting of a hydrocarbon group having 1 to 10 carbon atoms and a hydrocarbon group having 1 to 10 carbon atoms in which some or all hydrogen atoms are substituted with fluorine atoms, and X is an amino group), and in which the solvent includes 75% by mass or more of a hydrocarbon solvent in 100% by mass of the total amount of the solvent.

## Claims

### Claim 1

A surface treatment composition which is supplied as vapor to a surface of a wafer having an uneven pattern on the surface and is used for forming a water-repellent protective film on the surface, the surface treatment composition comprising:
a silylating agent; and
a solvent,
wherein the silylating agent includes a silicon compound represented by Formula (1),
(R1)3Si-X (1)
(R1's are each independently a group selected from the group consisting of a hydrocarbon group having 1 to 10 carbon atoms and a hydrocarbon group having 1 to 10 carbon atoms in which some or all hydrogen atoms are substituted with fluorine atoms, and X is an amino group), and
wherein the solvent includes 75% by mass or more of a hydrocarbon solvent in 100% by mass of a total amount of the solvent.

### Claim 2 (depends on 1)

The surface treatment composition according to claim 1,
wherein a content of the hydrocarbon solvent is 97% by mass or more in 100% by mass of the total amount of the solvent.

### Claim 3 (depends on 1)

The surface treatment composition according to claim 1,
wherein the hydrocarbon solvent includes an aromatic hydrocarbon.

### Claim 4 (depends on 1)

The surface treatment composition according to claim 1,
wherein a content of the silylating agent in 100% by mass of the surface treatment composition is 0.3% by mass or more and 30% by mass or less.

### Claim 5 (depends on 1)

The surface treatment composition according to claim 1,
wherein a boiling point difference between a boiling point of the solvent and a boiling point of the silylating agent (boiling point of the solvent−boiling point of the silylating agent) at 1 atm is 20° C. or more.

### Claim 6 (depends on 1)

The surface treatment composition according to claim 1,
wherein the silicon compound includes one or two or more selected from the group consisting of trimethylsilyldimethylamine, trimethylsilyldiethylamine, N-(trimethylsilyl)-tert-butylamine, hexamethyldisilazane, and compounds in which at least one trimethylsilyl group of these trimethylsilylamines is substituted with any of an ethyldimethylsilyl group, a propyldimethylsilyl group, a butyldimethylsilyl group, a hexyldimethylsilyl group, an octyldimethylsilyl group, and a decyldimethylsilyl group.

### Claim 7 (depends on 1)

The surface treatment composition according to claim 1,
wherein a water contact angle on a surface of a silicon wafer after surface treatment is greater than 80°, as measured by a procedure as below,
(procedure)
a smooth silicon wafer having a thermal oxide film layer on a surface is immersed in a 1% by mass hydrofluoric acid aqueous solution at 25° C. for 10 minutes and immersed and cleaned in pure water at 25° C. for 1 minute and 2-propanol (iPA) at 25° C. for 1 minute,
after cleaning, the silicon wafer is arranged horizontally in a state of being filled to the brim with iPA and the vapor of the surface treatment composition is supplied to the silicon wafer,
subsequently, on the surface of the silicon wafer, the vapor is changed into a liquid state and the iPA held on the surface is replaced with the liquid,
subsequently, the silicon wafer is immersed in iPA at 25° C. for 1 minute,
thereafter, air is blown onto the silicon wafer to remove the iPA on the surface, and
with respect to the silicon wafer surface obtained through the above steps, the water contact angle described above is measured in accordance with “Wettability test method for substrate glass surface” of JIS R 3257:1999 using 2 μl of pure water.

### Claim 8 (depends on 1)

The surface treatment composition according to claim 1,
wherein the surface treatment composition does not include a non-cyclic carbonate ester or includes 2% by mass or less of a non-cyclic carbonate ester in 100% by mass of the surface treatment composition.

### Claim 9 (depends on 1)

The surface treatment composition according to claim 1,
wherein the surface treatment composition does not include a catalyst or includes a catalyst in a content of 2% by mass or less in 100% by mass of the surface treatment composition.

### Claim at position 10

10-11. (canceled)

### Claim 12

A method for producing a wafer comprising:
a step of preparing a wafer having an uneven pattern on a surface;
a step of supplying a cleaning liquid to the surface of the wafer to carry out cleaning; and
a step of supplying vapor of a surface treatment composition to the surface holding the cleaning liquid, changing the state of the vapor to a liquid on the surface, replacing the cleaning liquid with the liquid, and forming a water-repellent protective film on at least a part of the surface,
wherein the surface treatment composition includes a silylating agent, and a solvent,
wherein the silylating agent includes a silicon compound represented by Formula (1),
(R1)3Si-X (1)
(R1's are each independently a group selected from the group consisting of a hydrocarbon group having 1 to 10 carbon atoms and a hydrocarbon group having 1 to 10 carbon atoms in which some or all hydrogen atoms are substituted with fluorine atoms, and X is an amino group), and
wherein the solvent includes 75% by mass or more of a hydrocarbon solvent in 100% by mass of a total amount of the solvent.

### Claim 13 (depends on 12)

The method for producing a wafer according to claim 12,
wherein a content of the hydrocarbon solvent is 97% by mass or more in 100% by mass of the total amount of the solvent.

### Claim 14 (depends on 12)

The method for producing a wafer according to claim 12,
wherein, in the surface treatment composition, the hydrocarbon solvent includes an aromatic hydrocarbon.

### Claim 15 (depends on 12)

The method for producing a wafer according to claim 12,
wherein, in the surface treatment composition, a content of the silylating agent is 0.3% by mass or more and 30% by mass or less in 100% by mass of the surface treatment composition.

### Claim 16 (depends on 12)

The method for producing a wafer according to claim 12,
wherein, in the surface treatment composition, a boiling point difference between a boiling point of the solvent and a boiling point of the silylating agent (boiling point of the solvent−boiling point of the silylating agent) at 1 atm is 20° C. or more.

### Claim 17 (depends on 12)

The method for producing a wafer according to claim 12,
wherein, in the surface treatment composition, the silicon compound includes one or two or more selected from the group consisting of trimethylsilyldimethylamine, trimethylsilyldiethylamine, N-(trimethylsilyl)-tert-butylamine, hexamethyldisilazane, and compounds in which at least one trimethylsilyl group of these trimethylsilylamines is substituted with any of an ethyldimethylsilyl group, a propyldimethylsilyl group, a butyldimethylsilyl group, a hexyldimethylsilyl group, an octyldimethylsilyl group, and a decyldimethylsilyl group.

### Claim 18 (depends on 12)

The method for producing a wafer according to claim 12,
wherein the surface treatment composition does not include a non-cyclic carbonate ester or includes 2% by mass or less of a non-cyclic carbonate ester in 100% by mass of the surface treatment composition.

### Claim 19 (depends on 12)

The method for producing a wafer according to claim 12,
wherein the surface treatment composition does not include a catalyst or includes a catalyst in a content of 2% by mass or less in 100% by mass of the surface treatment composition.

### Claim 20

(canceled)

### Claim 21 (depends on 12)

The method for producing a wafer according to claim 12,
wherein, in the surface treatment composition, a total content of Na, Mg, Ca, Mn, Fe, Cu, Li, Al, Cr, Ni, Zn, and Ag measured using inductively coupled plasma mass spectrometry is 100 mass ppb or less in the surface treatment composition.

### Claim 22 (depends on 12)

The method for producing a wafer according to claim 12,
wherein the vapor of the surface treatment composition is supplied in a state where iPA is held on the surface of the wafer.

### Claim 23 (depends on 12)

The method for producing a wafer according to claim 12, further comprising:
a step of mixing materials of each component of the surface treatment composition,
wherein a total amount of moisture in the materials is 2000 ppm by mass or less with respect to a total amount of the materials.