# US 2025/0210367 A1 · Atomic layer etching of silicon oxide at cryogenic temperature

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0210367 A1
- Document ID: US20250210367A1
- Status: Published application
- Kind: A1
- Application number: 18/392,785
- Filed: 2023-12-21
- Published: 2025-06-26
- Earliest claimed: 2023-12-21
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Sonam Dorje SHERPA; Mir ABDULLA AL GALIB; Alok RANJAN
- Web page: https://patentgrep.com/patent/US20250210367A1

## CPC

- H10P 50/283: {by chemical means}
- H01J 37/321: {the radio frequency energy being inductively coupled to the plasma}
- H01J 37/32449: {Gas control, e.g. control of the gas flow}
- H01J 37/32724: {Temperature}
- H01J 37/32816: {Pressure}
- H10P 50/692: {characterised by their composition, e.g. multilayer masks or materials}
- H01J 2237/3341: Reactive etching
- H01J 2237/3346: Selectivity
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

Embodiments of the disclosure include a method for forming a feature on a substrate includes exposing a portion of a silicon containing layer formed over the substrate through an opening formed though a masking layer to a carbon-free fluorine containing gas to convert the exposed portion of the silicon containing layer to a reactive portion, and etching the reactive portion by exposing the reactive portion of the silicon containing layer to a plasma formed from an inert gas.

## Claims

### Claim 1

A method for forming a feature on a substrate comprising:
exposing a portion of a silicon containing layer formed over the substrate through an opening formed though a masking layer to a carbon-free fluorine containing gas to convert the exposed portion of the silicon containing layer to a reactive portion; and
etching the reactive portion by exposing the reactive portion of the silicon containing layer to a plasma formed from an inert gas.

### Claim 2 (depends on 1)

The method of claim 1, wherein the inert gas is argon.

### Claim 3 (depends on 1)

The method of claim 1, where the carbon-free fluorine containing gas is hydrogen fluoride (HF).

### Claim 4 (depends on 1)

The method of claim 1, wherein the exposing the portion of the silicon containing layer and the etching the reactive portion are cyclically repeated.

### Claim 5 (depends on 1)

The method of claim 1, further comprising:
maintaining a substrate support, upon which the substrate is supported, at a temperature below 0° C. while the portion of the silicon containing layer is exposed to the carbon-free fluorine containing gas.

### Claim 6 (depends on 1)

The method of claim 1, wherein a pressure of the carbon-free containing gas exposed to the silicon containing layer is between 5 mTorr and 300 mTorr.

### Claim 7 (depends on 1)

The method of claim 1, wherein a flow rate of the carbon-free containing gas exposed to the silicon containing layer is between 50 sccm and 1000 sccm.

### Claim 8 (depends on 1)

The method of claim 1, wherein the silicon containing layer is fabricated from silicon (Si), silicon nitride (SiN), or silicon oxide (SiO).

### Claim 9

A method for forming a feature on a substrate comprising:
exposing a portion of a silicon containing layer formed over the substrate through a masking layer formed over the silicon containing layer to hydrogen fluoride (HF) vapor to convert the exposed portion of the silicon containing layer to a reactive portion; and
etching the reactive portion by exposing the reactive portion of the silicon containing layer to a plasma formed from argon (Ar).

### Claim 10 (depends on 9)

The method of claim 9, wherein the exposing the portion of the silicon containing layer and the etching the reactive portion are cyclically repeated.

### Claim 11 (depends on 9)

The method of claim 9, further comprising:
maintaining a substrate support, upon which the substrate is supported, at a temperature below 0° C. while the portion of the silicon containing layer is exposed to HF vapor.

### Claim 12 (depends on 9)

The method of claim 9, wherein a pressure of the HF exposed to the silicon containing layer is between 5 mTorr and 300 mTorr.

### Claim 13 (depends on 9)

The method of claim 9, wherein the silicon containing layer is fabricated from silicon (Si), silicon nitride (SiN), or silicon oxide (SiO).

### Claim 14

A processing chamber comprising:
a controller; and
a memory for storing instructions, which, when executed by the controller, causes the controller to perform a method for forming a feature on a substrate, the method comprising:
exposing a portion of a silicon containing layer formed over the substrate through an opening formed though a masking layer to a carbon-free fluorine containing gas to convert the exposed portion of the silicon containing layer to a reactive portion; and
etching the reactive portion by exposing the reactive portion of the silicon containing layer to a plasma formed from an inert gas.

### Claim 15 (depends on 14)

The processing chamber of claim 14, wherein the inert gas is argon.

### Claim 16 (depends on 14)

The processing chamber of claim 14, where the carbon-free fluorine containing gas is hydrogen fluoride (HF).

### Claim 17 (depends on 14)

The processing chamber of claim 14, wherein the instructions further comprise instructions to cyclically repeat the exposing the portion of the silicon containing layer and the etching the reactive portion.

### Claim 18 (depends on 14)

The processing chamber of claim 14, wherein the instructions further comprise instructions to:
maintain a substrate support, upon which the substrate is supported, at a temperature below 0° C. while the portion of the silicon containing layer is exposed to the carbon-free fluorine containing gas.

### Claim 19 (depends on 14)

The processing chamber of claim 14, wherein a pressure of the carbon-free fluorine containing gas exposed to the silicon containing layer is between 5 mTorr and 300 mTorr.

### Claim 20 (depends on 14)

The processing chamber of claim 14, wherein the silicon containing layer is fabricated from silicon (Si), silicon nitride (SiN), or silicon oxide (SiO).