# US 2025/0207247 A1 · Methods that utilize photosensitive organometallic oxides formed by chemical vapor polymerization

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0207247 A1
- Document ID: US20250207247A1
- Status: Published application
- Kind: A1
- Application number: 19/048,395
- Filed: 2025-02-07
- Published: 2025-06-26
- Earliest claimed: 2022-08-02
- Assignees: Tokyo Electron Limited
- Applicants: Tokyo Electron Limited
- Inventors: Kandabara Tapily; Nobuo Matsuki
- Web page: https://patentgrep.com/patent/US20250207247A1

## CPC

- C23C 16/045: {Coating cavities or hollow spaces, e.g. interior of tubes; Infiltration of porous substrates}
- C23C 16/04: Coating on selected surface areas, e.g. using masks
- C23C 16/407: {of zinc, germanium, cadmium, indium, tin, thallium or bismuth}
- C23C 16/50: using electric discharges {(generation and control of plasma in discharge tubes for surface treatment H01J37/32, H01J37/34)}
- C23C 16/56: After-treatment
- G03F 7/0007: {Filters, e.g. additive colour filters; Components for display devices}
- G03F 7/0035: {Multiple processes, e.g. applying a further resist layer on an already in a previously step, processed pattern or textured surface}
- G03F 7/0042: {with inorganic or organometallic light-sensitive compounds not otherwise provided for, e.g. inorganic resists (G03F7/075 takes precedence)}
- G03F 7/167: {from the gas phase, by plasma deposition (G03F7/2035 takes precedence)}
- G03F 7/168: {Finishing the coated layer, e.g. drying, baking, soaking}
- G03F 7/70033: {by plasma extreme ultraviolet [EUV] sources}
- H10P 50/73: {using masks for insulating materials}
- H10P 76/20: of masks comprising organic materials
- H10P 76/4085: {characterised by the processes involved to create the masks}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

New gap fill materials and methods for filling gaps within patterned layers are provided herein. In various embodiments, a non-solid organometallic oxide polymer containing liquid-like oligomer units is deposited on a patterned layer via chemical vapor polymerization (CVP). The patterned layer comprises a plurality of structures, which are spaced apart and separated by gaps. During deposition, the liquid-like oligomer units flow into the gaps between the plurality of structures to completely fill the gaps with the non-solid organometallic oxide polymer. Heat-treating the semiconductor substrate further polymerizes the non-solid organometallic oxide polymer to form a photosensitive organometallic oxide polymer film on the patterned layer and within the gaps between the plurality of structures.

## Claims

### Claim 1

A method for filling gaps within a patterned layer formed on a semiconductor substrate, the method comprising:
providing the semiconductor substrate, wherein the patterned layer formed on the semiconductor substrate comprises a plurality of structures, which are spaced apart and separated by gaps;
depositing a non-solid organometallic oxide polymer containing liquid-like oligomer units on the patterned layer via chemical vapor polymerization (CVP), wherein the liquid-like oligomer units flow into the gaps between the plurality of structures during said depositing, and wherein a capillary effect within the gaps causes the liquid-like oligomer units to completely fill the gaps with the non-solid organometallic oxide polymer; and
heat-treating the semiconductor substrate to further polymerize the non-solid organometallic oxide polymer and form a photosensitive organometallic oxide polymer film on the patterned layer and within the gaps between the plurality of structures.

### Claim 2 (depends on 1)

The method of claim 1, wherein the photosensitive organometallic oxide polymer film contains a central metal atom of tin (Sn), zirconium (Zr), indium (In), antimony (Sb), bismuth (Bi), zinc (Zn), hafnium (Hf), or aluminum (Al), or combinations thereof.

### Claim 3 (depends on 1)

The method of claim 1, wherein said depositing the non-solid organometallic oxide polymer comprises:
exposing the semiconductor substrate to a plasma-excited vapor comprising a metal precursor having carbon-carbon double bonds to form the non-solid organometallic oxide polymer on the patterned layer and within the gaps between the plurality of structures.

### Claim 4 (depends on 3)

The method of claim 3, wherein said exposing the semiconductor substrate to the plasma-excited vapor comprises:
maintaining an ion energy of less than 50 eV in the plasma-excited vapor; and
maintaining a substrate temperature of less than 150° C. during the exposing.

### Claim 5 (depends on 3)

The method of claim 3, wherein said exposing the semiconductor substrate to the plasma-excited vapor comprises:
maintaining an ion energy of between 0 eV and 5 eV in the plasma-excited vapor; and
maintaining a substrate temperature within a range between −50° C. and 0° C. during the exposing.

### Claim 6 (depends on 3)

The method of claim 3, wherein the metal precursor includes a metal alkoxide.

### Claim 7 (depends on 3)

The method of claim 3, wherein the metal precursor contains tin (Sn), and wherein the metal precursor:
(a) has a formula SnαOβ (O—CmHn)ΓCxHy, where m, n, and α are arbitrary integers of 1 or more, β, Γ, x, and y are arbitrary integers of 0 or more, and β and Γ are not 0 at the same time;
(b) is SnR1(O—R2)3, SnR12(O—R2)2, or SnHR1(O—R2)2, where R1: CH3, C2H3, C3H5, C4H7, or C6H6, and R2: CH3, C2H5, C3H7, or C4H9;
(c) is SnCH3tBu(O—tBu)2, SntBu(O—tBu)3, SntBu(O—C3H7)3, SntBu(O—C2H5)3, SntBu(O—CH3)3, SnCH3C2H3(O—tBu)2, or SnCH3(C2H3)(O—CH3)2;
(d) is Sn(C2H4O2) or Sn(OR)2, where R is selected from CH3, C2H5 and C4H9;
(e) is a mixture of Sn(N(CH3)2)4 and HOCH2CH2OH;
(f) has a formula SnxCyHz, where x, y, and z are arbitrary integers of 1 or more; or
(g) is Sn(CH3)4, Sn(C2H5)4, SnH(CH3)3, or SnH(C2H5)3.

### Claim 8 (depends on 3)

The method of claim 3, wherein the plasma-excited vapor comprises the metal precursor and an additive precursor, wherein the metal precursor has a formula SnαOβ (O—CmHn)ΓCxHy, and wherein the additive precursor has a formula SnαCxHy, where m, n, and α are arbitrary integers of 1 or more.

### Claim 9 (depends on 3)

The method of claim 3, wherein the metal precursor contains a metal (M) and has a formula MαOβ (O—CmHn)ΓCxHy, where m, n, and α are arbitrary integers of 1 or more, β, Γ, x, and y are arbitrary integers of 0 or more, and β and Γ are not 0 at the same time.

### Claim 10 (depends on 9)

The method of claim 9, wherein the plasma-excited vapor comprises the metal precursor and one or more additive precursors, and wherein the one or more additive precursors comprise:
(a) a precursor containing a metal (M) and having a formula MαCxHy, where m, n, and α are arbitrary integers of 1 or more; and/or
(b) a nitrogen containing precursor.

### Claim 11 (depends on 3)

The method of claim 3, wherein said heat-treating the semiconductor substrate comprises:
heat-treating the semiconductor substrate to a substrate temperature between about 0° C. and about 400° C. to further polymerize the non-solid organometallic oxide polymer and form the photosensitive organometallic oxide polymer film with polymerized carbon-carbon bonds on the patterned layer and within the gaps between the plurality of structures.

### Claim 12 (depends on 11)

The method of claim 11, wherein said heat-treating the semiconductor substrate utilizes a plasma.

### Claim 13

A method utilized in a self-aligned multi-patterning (SAMP) process flow, the method comprising:
forming a patterned layer on one or more underlying layers formed on a semiconductor substrate, wherein the patterned layer comprises a plurality of structures, which are formed during the SAMP process flow and separated by gaps;
depositing a non-solid organometallic oxide polymer containing liquid-like oligomer units on the patterned layer via chemical vapor polymerization (CVP), wherein the liquid-like oligomer units flow into the gaps between the plurality of structures during said depositing, and wherein a capillary effect within the gaps causes the liquid-like oligomer units to completely fill the gaps with the non-solid organometallic oxide polymer;
heat-treating the semiconductor substrate to further polymerize the non-solid organometallic oxide polymer and form a photosensitive organometallic oxide polymer film on the patterned layer and within the gaps between the plurality of structures;
selectively exposing the photosensitive organometallic oxide polymer film to extreme ultraviolet (EUV) radiation, wherein said selectively exposing changes an etch selectivity of a portion of the photosensitive organometallic oxide polymer film formed within one or more of the gaps; and
selectively etching the photosensitive organometallic oxide polymer film, wherein said selectively etching removes the portion of the photosensitive organometallic oxide polymer film from the one or more of the gaps to create one or more features on the one or more underlying layers.

### Claim 14 (depends on 13)

The method of claim 13, wherein said selectively etching removes the portion of the photosensitive organometallic oxide polymer film from the one or more of the gaps to create a contact hole pattern on the one or more underlying layers, and wherein the method further comprises utilizing the contact hole pattern to form contact holes within the one or more underlying layers.

### Claim 15 (depends on 13)

The method of claim 13, wherein the photosensitive organometallic oxide polymer film contains a central metal atom of tin (Sn), zirconium (Zr), indium (In), antimony (Sb), bismuth (Bi), zinc (Zn), hafnium (Hf), or aluminum (Al), or combinations thereof.

### Claim 16 (depends on 13)

The method of claim 13, wherein said depositing the non-solid organometallic oxide polymer comprises:
exposing the semiconductor substrate to a plasma-excited vapor comprising a metal precursor having carbon-carbon double bonds to form the non-solid organometallic oxide polymer on the patterned layer and within the gaps between the plurality of structures.

### Claim 17 (depends on 16)

The method of claim 16, wherein said exposing the semiconductor substrate to the plasma-excited vapor comprises:
maintaining an ion energy of less than 50 eV in the plasma-excited vapor; and
maintaining a substrate temperature of less than 150° C. during the exposing.

### Claim 18 (depends on 16)

The method of claim 16, wherein said exposing the semiconductor substrate to the plasma-excited vapor comprises:
maintaining an ion energy of between 0 eV and 5 eV in the plasma-excited vapor; and
maintaining a substrate temperature within a range between −50° C. and 0° C. during the exposing.

### Claim 19 (depends on 16)

The method of claim 16, wherein the metal precursor includes a metal alkoxide.

### Claim 20 (depends on 16)

The method of claim 16, wherein the metal precursor contains tin (Sn), and wherein the metal precursor:
(a) has a formula SnαOβ (O—CmHn)ΓCxHy, where m, n, and α are arbitrary integers of 1 or more, β, Γ, x, and y are arbitrary integers of 0 or more, and β and Γ are not 0 at the same time;
(b) is SnR1(O—R2)3, SnR12(O—R2)2, or SnHR1(O—R2)2, where R1: CH3, C2H3, C3H5, C4H7, or C6H6, and R2: CH3, C2H5, C3H7, or C4H9;
(c) is SnCH3tBu(O—tBu)2, SntBu(O—tBu)3, SntBu(O—C3H7)3, SntBu(O—C2H5)3, SntBu(O—CH3)3, SnCH3C2H3(O—tBu)2, or SnCH3(C2H3)(O—CH3)2;
(d) is Sn(C2H4O2) or Sn(OR)2, where R is selected from CH3, C2H5and C4H9;
(e) is a mixture of Sn(N(CH3)2)4 and HOCH2CH2OH;
(f) has a formula SnxCyHz, where x, y, and z are arbitrary integers of 1 or more; or
(g) is Sn(CH3)4, Sn(C2H5)4, SnH(CH3)3, or SnH(C2H5)3.

### Claim 21 (depends on 16)

The method of claim 16, wherein the plasma-excited vapor comprises the metal precursor and an additive precursor, wherein the metal precursor has a formula SnαOβ (O—CmHn)ΓCxHy, and wherein the additive precursor has a formula SnαCxHy, where m, n, and α are arbitrary integers of 1 or more.

### Claim 22 (depends on 16)

The method of claim 16, wherein the metal precursor contains a metal (M) and has a formula MαOβ (O—CmHn)ΓCxHy, where m, n, and α are arbitrary integers of 1 or more, β, Γ, x, and y are arbitrary integers of 0 or more, and β and Γ are not 0 at the same time.

### Claim 23 (depends on 22)

The method of claim 22, wherein the plasma-excited vapor comprises the metal precursor and one or more additive precursors, and wherein the one or more additive precursors comprise:
(a) a precursor containing a metal (M) and having a formula MαCxHy, where m, n, and α are arbitrary integers of 1 or more; and/or
(b) a nitrogen containing precursor.

### Claim 24 (depends on 16)

The method of claim 16, wherein said heat-treating the semiconductor substrate comprises:
heat-treating the semiconductor substrate to a substrate temperature between about 0° C. and about 400° C. to further polymerize the non-solid organometallic oxide polymer and form the photosensitive organometallic oxide polymer film with polymerized carbon-carbon bonds on the patterned layer and within the gaps between the plurality of structures.

### Claim 25 (depends on 24)

The method of claim 24, wherein said heat-treating the semiconductor substrate utilizes a plasma.