# US 2025/0207236 A1 · Flat steel product having an al coating, method for the production thereof, steel component, and method for production thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0207236 A1
- Document ID: US20250207236A1
- Status: Published application
- Kind: A1
- Application number: 18/850,761
- Filed: 2022-04-20
- Published: 2025-06-26
- Earliest claimed: 2022-04-20
- Assignees: ThyssenKrupp Steel Europe AG
- Applicants: Thyssenkrupp Steel Europe AG
- Inventors: David Hoffmann; Fabian Junge
- Web page: https://patentgrep.com/patent/US20250207236A1

## CPC

- B32B 15/012: {one layer being formed of an iron alloy or steel, another layer being formed of aluminium or an aluminium alloy}
- C23C 2/12: Aluminium or alloys based thereon
- C22C 21/02: with silicon as the next major constituent
- C22C 21/10: with zinc as the next major constituent
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/28: with titanium or zirconium
- C22C 38/32: with boron
- C23C 2/02: Pretreatment of the material to be coated, e.g. for coating on selected surface areas (C23C2/30 takes precedence)
- C23C 2/06: Zinc or cadmium or alloys based thereon
- C23C 2/26: After-treatment (C23C2/14 takes precedence)
- C23C 2/28: Thermal after-treatment, e.g. treatment in oil bath
- C23C 2/40: Plates; Strips
- C23C 30/00: Coating with metallic material characterised only by the composition of the metallic material, i.e. not characterised by the coating process (C23C26/00, C23C28/00 take precedence)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A steel component includes a steel substrate composed of a steel having 0.1-3 wt. % of Mn and optionally up to 0.01 wt. % of B, and an Al-based protective coating applied to the steel substrate. The protective coating has an overall iron- and manganese-free proportion by mass of up to 30% of additional alloy constituents, by mass of Si in the protective coating as additional alloy constituent is between 3 wt. % and 15 wt. % Si, by mass of Mg in the protective coating as additional alloy constituent is up to 1.0 wt. % Mg, and by mass of Zn in the protective coating as additional alloy constituent is between 0.4 wt. % and 25.0 wt. % Zn. The protective coating has a near-surface first Zn-rich layer having a Zn content higher than an average Zn content of the protective coating, and the Zn content of the first Zn-rich layer is more than 5 wt. %.

## Claims

### Claim at position 1

-12. (canceled)

### Claim 13

A steel component comprising:
a steel substrate composed of a steel having 0.1-3% by weight of Mn, and
an Al-based protective coating applied to the steel substrate and having an overall iron- and manganese-free proportion by mass of up to 30% by weight of additional alloy constituents, wherein the additional alloy constituents include Si, Mg and Zn, wherein the iron- and manganese-free proportion by mass of Si in the Al-based protective coating as an additional alloy constituent is between 3% and 15% by weight, wherein the iron- and manganese-free proportion by mass of Mg in the Al-based protective coating as an additional alloy constituent is up to 1.0% by weight, wherein the iron- and manganese-free proportion by mass of Zn in the Al-based protective coating as an additional alloy constituent is between 0.4% and 25.0% by weight, wherein the Al-based protective coating has a near-surface first Zn-rich layer having a Zn content higher than an average Zn content of the Al-based protective coating, and wherein the Zn content of the first Zn-rich layer is more than 5% by weight, and wherein a layer thickness of the Al-based protective coating is at least 5 μm and the near-surface layer extends over a region having a thickness of 500 nm that adjoins a surface of the Al-based protective coating.

### Claim 14 (depends on 13)

The steel component of claim 13, wherein the steel further comprises up to 0.01% by weight of B.

### Claim 15 (depends on 13)

The steel component of claim 13, wherein the iron- and manganese-free proportion by mass of Si in the Al-based protective coating is between 6% and 12% by weight.

### Claim 16 (depends on 13)

The steel component of claim 13, wherein the iron- and manganese-free proportion by mass of Mg in the Al-based protective coating adds up to at least 0.10% or at least 0.15% by weight, and/or the iron- and manganese-free proportion by mass of Mg in the Al-based protective coating adds up to at most 0.50% or at most 0.35% by weight, and/or the iron- and manganese-free proportion by mass of Zn in the Al-based protective coating adds up to at least 0.6% or at least 1.0% by weight, and/or the iron- and manganese-free proportion by mass of Zn in the Al-based protective coating adds up to at most 5.0% or at most 2.3% by weight, and/or the Zn content of the first Zn-rich layer is more than 10.0% by weight or more than 18% by weight.

### Claim 17 (depends on 13)

The steel component of claim 13, wherein the surface of the Al-based protective coating is formed mainly from Zn accumulations in metallic and/or oxidic form.

### Claim 18 (depends on 13)

The steel component of claim 13, wherein the Al-based protective coating comprises a low-silicon phase (A) and a silicon-rich phase (R), where the silicon-rich phase has an insular distribution in the low-silicon phase, where the Zn content of the silicon-rich phase is less than 90% of an average Zn content of the Al-based protective coating, and the Zn content of the low-silicon phase is more than 105% of the average Zn content of the Al-based protective coating.

### Claim 19 (depends on 18)

The steel component of claim 18, wherein the Si content of the low-silicon phase is less than 10% by weight, less than 7% by weight, or less than 5% by weight.

### Claim 20 (depends on 18)

The steel component of claim 18, wherein the Si content of the silicon-rich phase is greater than 10% by weight or greater than 12% by weight.

### Claim 21

A flat steel product for hot forming, comprising:
a steel substrate composed of a steel having 0.1-3% by weight of Mn; and
an Al-based protective coating applied to the steel substrate and having an overall iron- and manganese-free proportion by mass of up to 30% of additional alloy constituents, wherein the additional alloy constituents include Si, Mg and Zn, wherein the iron- and manganese-free proportion by mass of Si in the Al-based protective coating as an additional alloy constituent is between 3% and 15% by weight, wherein the iron- and manganese-free proportion by mass of Mg in the Al-based protective coating as an additional alloy constituent is between 0.10% and 0.50% by weight, and wherein the iron- and manganese-free proportion by mass of Zn in the Al-based protective coating as an additional alloy constituent is between 0.4% and 5% by weight.

### Claim 22 (depends on 21)

The flat steel product of claim 21, wherein the steel further comprises up to 0.01% by weight of B.

### Claim 23 (depends on 21)

The flat steel product of claim 21, wherein the iron- and manganese-free proportion by mass of Si in the Al-based protective coating is between 6% and 12% by weight.

### Claim 24 (depends on 21)

The flat steel product of claim 21, wherein the iron- and manganese-free proportion by mass of Mg in the Al-based protective coating is between 0.1% and 0.35% by weight.

### Claim 25 (depends on 21)

The flat steel product of claim 21, wherein the iron- and manganese-free proportion by mass of Zn in the Al-based protective coating is between 0.4% and 2.3% by weight.

### Claim 26 (depends on 21)

The flat steel product of claim 21, wherein the Al-based protective coating has been applied by hot dip coating.

### Claim 27

A method of producing a phosphated steel component, comprising:
providing a steel substrate composed of a steel having 0.1-3% by weight of Mn; and
hot dip coating the steel substrate by means of a melt having an Al-based protective coating that has an overall iron- and manganese-free proportion by mass of up to 30% by weight of additional alloy constituents, wherein the additional alloy constituents include Si, Mg and Zn, wherein the iron- and manganese-free proportion by mass of Si in the Al-based protective coating as an additional alloy constituent is between 3% and 15% by weight, wherein the iron- and manganese-free proportion by mass of Mg in the Al-based protective coating as an additional alloy constituent is up to 1% by weight, wherein the iron- and manganese-free proportion by mass of Zn in the Al-based protective coating as an additional alloy constituent is between 0.4% and 25.0% or between 0.4% and 5% by weight.

### Claim 28 (depends on 27)

The method of claim 27, wherein the steel further comprises up to 0.01% by weight of B.

### Claim 29 (depends on 27)

The method of claim 27, wherein the iron- and manganese-free proportion by mass of Si in the Al-based protective coating is between 6% and 12% by weight.

### Claim 30 (depends on 27)

The method of claim 27, further comprising:
heating the coated steel substrate to a heating temperature of at least 700° C. for the hot forming operation and holding it at the heating temperature, such that diffusion results in concentration of Zn with formation of metallic and oxidic Zn accumulations at a surface of the Al-based protective coating;
hot forming the coated steel substrate to the steel component; and
phosphating the hot-formed steel component.

### Claim 31 (depends on 27)

The method of claim 27, wherein during the heating and holding, diffusion results in formation of a low-silicon phase (A) and a silicon-rich phase (R), where the silicon-rich phase has an insular distribution in the low-silicon phase, and where the Zn content of the low-silicon phase is between 25% and 60% by weight of the melt.

### Claim 32 (depends on 27)

The method of claim 27, wherein the heating temperature is greater than an austenitization (Ac3) temperature, such that the microstructure of the steel substrate is austenitic, and wherein the coated steel substrate is quenched after hot forming or in the course of hot forming, such that hardness microstructure is formed in the microstructure of the steel substrate of the flat steel product.