# US 2025/0207233 A1 · Hot stamping alloy, method of making hot stamped parts with such alloy, and parts made from such alloy

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0207233 A1
- Document ID: US20250207233A1
- Status: Published application
- Kind: A1
- Application number: 18/436,610
- Filed: 2024-02-08
- Published: 2025-06-26
- Earliest claimed: 2023-12-22
- Assignees: GM Global Technology Operations LLC
- Applicants: GM Global Technology Operations LLC
- Inventors: Zhou WANG; Zhenke TENG; Zhao LI; Jianfeng WANG
- Web page: https://patentgrep.com/patent/US20250207233A1

## CPC

- C22C 38/02: containing silicon
- C22C 38/38: with more than 1.5% by weight of manganese
- C21D 1/18: Hardening (C21D1/02 takes precedence); Quenching with or without subsequent tempering (quenching devices C21D1/62)
- C21D 1/76: Adjusting the composition of the atmosphere
- C21D 6/002: {containing Cr (C21D6/004 takes precedence)}
- C21D 6/005: {containing Mn}
- C21D 8/00: Modifying the physical properties of ferrous metals or ferrous alloys by deformation combined with, or followed by, heat treatment (hardening articles or materials formed by forging or rolling with no further heating beyond that required for the formation C21D1/02)
- C21D 9/0068: {for particular articles not mentioned below}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/04: containing manganese
- C22C 38/34: with more than 1.5% by weight of silicon
- C21D 1/673: for die quenching
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)

## Abstract

A metal alloy suitable for hot stamping comprises between about 0.05 and about 0.45 wt % carbon; between about 0.5 and about 4.5 wt % manganese; between about 0.5 and about 6 wt % chromium; between about 0.5 and about 2.5 wt % Si, between about 0.1 and about 0.5 wt % cerium, the balance being iron and impurities. A method of making a structural automobile part comprises heating a blank of the metal alloy and hot stamping the blank into the desired structural automotive part. A structural part is made by hot stamping a blank of the metal alloy.

## Claims

### Claim 1

A metal alloy suitable for hot stamping, the alloy comprising between about 0.05 and about 0.45 wt % carbon; between about 0.5 and about 4.5 wt % manganese; between about 0.5 and about 6 wt % chromium; between about 0.5 and about 2.5 wt % Si, between about 0.1 and about 0.5 wt % cerium, the balance being iron and impurities.

### Claim 2 (depends on 1)

The metal alloy according to claim 1 wherein the total of Cr and Si content is less than or equal to about 5 wt %.

### Claim 3 (depends on 2)

The metal alloy according to claim 2 wherein the ratio of Cr:Si is between about 1.25 and about 3.

### Claim 4 (depends on 1)

The metal alloy according to claim 1 wherein the ratio of Cr:Si is between about 1.25 and about 3.

### Claim 5

A method of making a structural automobile part comprising: heating a blank of a metal alloy comprising between about 0.05 and about 0.45 wt % carbon; between about 0.5 and about 4.5 wt % manganese; between about 0.5 and about 6 wt % chromium; between about 0.5 and about 2.5 wt % Si, between about 0.1 and about 0.5 wt % cerium, the balance being iron and impurities; and hot stamping the blank into the desired structural automotive part.

### Claim 6 (depends on 5)

The method of claim 5 wherein the heating occurs in the space bounded by the time, temperature points (300 s, 870° C.), (200 s, 980° C.), (800 s, 870° C.), and (1000 s, 980° C.).

### Claim 7 (depends on 5)

The method of claim 5 wherein the heating occurs in the space bounded by the time, temperature points (300 s, 870° C.), (200 s, 980° C.), (1000 s, 870° C.), and (800 s, 980° C.).

### Claim 8 (depends on 5)

The method of claim 5 wherein the heating occurs in an inert atmosphere.

### Claim 9 (depends on 5)

The method according to claim 5 wherein the composition of the blank has a total of Cr and Si content is less than or equal to about 5 wt %.

### Claim 10 (depends on 9)

The method according to claim 9 wherein the composition of the blank has a ratio of Cr:Si is between about 1.25 and about 3.

### Claim 11 (depends on 5)

The method according to claim 5 wherein the ratio of Cr:Si is between about 1.25 and about 3.

### Claim 12

An automotive structural part made of between about 0.05 and about 0.45 wt % carbon; between about 0.5 and about 4.5 wt % manganese; between about 0.5 and about 6 wt % chromium; between about 0.5 and about 2.5 wt % Si, between about 0.1 and about 0.5 wt % cerium, the balance being iron and impurities, shaped by hot stamping with a uniform oxidation thickness after hot stamping of 0.5 μm.

### Claim 13 (depends on 12)

The automotive structural part according to claim 12 wherein the total of Cr and Si content is less than or equal to about 5 wt %.

### Claim 14 (depends on 13)

The automotive structural part according to claim 13 wherein the ratio of Cr:Si is between about 1.25 and about 3.

### Claim 15 (depends on 12)

The automotive structural part according to claim 12 wherein the ratio of Cr:Si is between about 1.25 and about 3.

### Claim 16 (depends on 11)

The automotive structural part according to claim 11, wherein the part is an automotive pillar, a door beam, or a bumper beam.