# US 2025/0207016 A1 · Lower-cost, higher efficiency, environmentally friendly, self-dispersible recovery, and stimulation fluid for enhanced oil recovery (eor) and improved oil recovery (ior)

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0207016 A1
- Document ID: US20250207016A1
- Status: Published application
- Kind: A1
- Application number: 19/060,295
- Filed: 2025-02-21
- Published: 2025-06-26
- Earliest claimed: 2022-01-15
- Assignees: Innovative Oil and Gas Solutions
- Inventors: Naveed Aslam
- Web page: https://patentgrep.com/patent/US20250207016A1

## CPC

- C09K 8/92: characterised by their form or by the form of their components, e.g. encapsulated material (C09K8/70 takes precedence)
- C09K 8/032: {Inorganic additives}
- C09K 8/58: Compositions for enhanced recovery methods for obtaining hydrocarbons, i.e. for improving the mobility of the oil, e.g. displacing fluids
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

In one aspect, a tunable bi-functional self-dispersible fluid (TBSF) for well stimulation and hydrocarbon recovery is provided. The TBSF includes a fluid and crumpled graphene oxide balls. The fluid includes water, carbon dioxide, liquified natural gas, natural gas liquid, nitrogen, or a combination of two or more thereof. Said crumpled graphene oxide balls are dispersed in the fluid and include a first and second fraction of crumpled graphene oxide balls. The first and second fractions of crumpled graphene oxide balls are hydrophilic and hydrophobic, respectively. Said crumpled graphene oxide balls each include a shell-like structure and inner hollow core. Said crumpled graphene oxide balls include iron-oxide coupled to the graphene oxide. The crumpled graphene oxide balls may include iron oxide and is magnetic. The first and second fractions of crumpled graphene oxide balls are present in said crumpled graphene oxide balls at 20-40 wt % and 60-80 wt %, respectively.

## Claims

### Claim 1

A tunable bi-functional self-dispersible fluid for well stimulation and hydrocarbon recovery, comprising:
a fluid;
a plurality of crumpled graphene oxide balls;
wherein
the fluid comprises one or more of water, carbon dioxide, a liquified natural gas (LNG), a natural gas liquid (NGL), and nitrogen;
said crumpled graphene oxide balls
are dispersed in the fluid;
comprise a first and second fraction of crumpled graphene oxide balls;
the first fraction of crumpled graphene oxide balls is hydrophilic; and
the second fraction of crumpled graphene oxide balls are hydrophobic.

### Claim 2 (depends on 1)

The tunable bi-functional self-dispersible fluid of claim 1, wherein
said crumpled graphene oxide balls each comprise:
a shell-like structure; and
an inner hollow core.

### Claim 3 (depends on 1)

The tunable bi-functional self-dispersible fluid of claim 1, wherein
said crumpled graphene oxide balls comprise iron-oxide coupled thereto.

### Claim 4 (depends on 1)

The tunable bi-functional self-dispersible fluid of claim 1, wherein
said crumpled graphene oxide balls comprise iron oxide and are magnetic.

### Claim 5 (depends on 1)

The tunable bi-functional self-dispersible fluid of claim 1, wherein
the first fraction of crumpled graphene oxide balls is present in said crumpled graphene oxide balls at 20-40 wt %; and
the second fraction of crumpled graphene oxide balls is present in said crumpled graphene oxide balls at 60-80 wt %.

### Claim 6

A method for preparing a tunable bi-functional self-dispersible fluid, comprising:
providing a fluid;
providing a plurality of crumpled graphene oxide balls, wherein said crumpled graphene oxide balls comprise a first fraction of crumpled graphene oxide balls and a second fraction of crumpled graphene oxide balls, wherein the first fraction of crumpled graphene oxide balls is hydrophilic, and wherein the second fraction of crumpled graphene oxide balls are hydrophobic; and
combining said crumpled graphene oxide balls with the fluid in a manner to disperse said crumpled graphene oxide balls with the fluid.

### Claim 7 (depends on 6)

The method of claim 6, wherein
the step of providing the plurality of crumpled graphene oxide balls comprises:
combining graphene oxide with water to create a suspension;
applying the suspension within a tube comprising an inlet positioned opposite an outlet;
positioning the tube within a furnace in a manner such that the tube is increasingly heated from the inlet to the outlet thereby thermally reducing the graphene oxide to generate said crumpled graphene oxide balls; and
collecting said crumpled graphene oxide balls.

### Claim 8 (depends on 7)

The method of claim 7, wherein
the first fraction is generated by thermal reduction at about 200° C.; and
the second fraction is generated by thermal reduction at about 800° C.

### Claim 9 (depends on 6)

The method of claim 6, wherein
the fluid comprises one or more of water, carbon dioxide, a liquified natural gas (LNG), a natural gas liquid (NGL), and nitrogen.

### Claim 10 (depends on 6)

The method of claim 6, wherein
said crumpled graphene oxide balls comprise a third fraction of crumpled graphene oxide balls; and
the third fraction of crumpled graphene oxide balls are oleophilic.

### Claim 11 (depends on 7)

The method of claim 7, wherein
the tube is increasingly heated from about 200° C. to about 800° C.

### Claim 12 (depends on 6)

The method of claim 6, wherein
said crumpled graphene oxide balls each comprise:
a shell-like structure; and
an inner hollow core.

### Claim 13 (depends on 6)

The method of claim 6, wherein
the crumpled graphene oxide balls comprise graphene oxide; and
the graphene oxide is coupled to iron oxide.

### Claim 14 (depends on 6)

The method of claim 6, wherein
the first fraction of crumpled graphene oxide balls is present in said crumpled graphene oxide balls at 20-40 wt %; and
the second fraction of crumpled graphene oxide balls are present in said crumpled graphene oxide balls at 60-80 wt %.