# US 2025/0205697 A1 · Highly efficient photocatalyst material for decomposing organic hazardous substances and method for synthesizing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0205697 A1
- Document ID: US20250205697A1
- Status: Published application
- Kind: A1
- Application number: 18/988,887
- Filed: 2024-12-20
- Published: 2025-06-26
- Earliest claimed: 2023-12-21
- Assignees: Korea Institute of Energy Technology; Korea University Research and Business Foundation, Sejong Campus
- Applicants: Korea Institute of Energy Technology; Korea University Research and Business Foundation, Sejong Campus
- Inventors: Dong Han SEO; Sun Woo KIM; Jae Muk LIM; Jun Sub KIM; Young Jin KIM; Abouelanwar Ali Mahmoud Mohamed; Jong Min OH
- Web page: https://patentgrep.com/patent/US20250205697A1

## CPC

- B01J 37/349: {making use of flames, plasmas or lasers}
- B01J 21/063: {Titanium; Oxides or hydroxides thereof}
- B01J 21/08: Silica
- B01J 35/39: Photocatalytic properties
- B01J 37/343: {of ultrasonic wave energy}
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS

## Abstract

An embodiment of the disclosure provides a highly efficient photocatalyst material for decomposing organic hazardous substances, the highly efficient photocatalyst material including: silica having micropores formed; and a quantum dot substance surrounding the silica, wherein the quantum dot substance is coexistence of a TiO2 quantum dot and a TiO2−x quantum dot, and the X is a real number greater than 0 and less than 2.

## Claims

### Claim 1

A highly efficient photocatalyst material for decomposing organic hazardous substances, the highly efficient photocatalyst material comprising:
silica having nanopores formed; and
a quantum dot substance surrounding the silica,
wherein the quantum dot substance is coexistence of a TiO2 quantum dot and a TiO2−x quantum dot, and the X is a real number greater than 0 and less than 2.

### Claim 2 (depends on 1)

The highly efficient photocatalyst material of claim 1, wherein a porosity of nanopores formed in the silica is 2 nm to 100 nm.

### Claim 3 (depends on 1)

The highly efficient photocatalyst material of claim 1, wherein the TiO2−x quantum dot comprises an oxygen defect or a hydroxyl group (—OH).

### Claim 4 (depends on 1)

The highly efficient photocatalyst material of claim 1, wherein the TiO2 quantum dot has a multi-crystal structure comprising a rutile crystal structure and an anatase crystal structure.

### Claim 5 (depends on 1)

The highly efficient photocatalyst material of claim 1, wherein in the entire photocatalyst material, a ratio of the presence of the TiO2 quantum dot and TiO2−x quantum dot is 2:8 to 8:2.

### Claim 6 (depends on 1)

The highly efficient photocatalyst material of claim 1, wherein through a Ti—O—Si bond formed by bonding of the silica and the TiO2−x quantum dot surrounding the silica, reduction of the TiO2−x quantum dot having a defect to the TiO2 quantum dot in an oxygen-containing environment is suppressed.

### Claim 7 (depends on 1)

The highly efficient photocatalyst material of claim 1, wherein the photocatalyst material exhibits a catalytic activity across a UV-A and visible wavelength range.

### Claim 8

A method for synthesizing a highly efficient photocatalyst material for decomposing organic hazardous substances, the method comprising:
forming a bio-silica solution by dispersing bio-silica in a solvent;
adding an aqueous solution comprising a Ti3+ precursor to the formed bio-silica solution to form a mixed solution; and
performing a low-temperature atmospheric pressure plasma process which is applying low-temperature atmospheric pressure air plasma to the formed mixed solution.

### Claim 9 (depends on 8)

The method of claim 8, wherein the forming of the bio-silica solution disperses the bio-silica in a solvent through an ultrasonic disperser.

### Claim 10 (depends on 8)

The method of claim 8, wherein the forming of the mixed solution makes a mass ratio of the Ti3+ precursor to the bio-silica be 0.02 wt % to 20 wt %.

### Claim 11 (depends on 8)

The method of claim 8, wherein in the forming of the mixed solution, an added TiCl3 aqueous solution has a concentration of 10% to 15%.

### Claim 12 (depends on 8)

The method of claim 8, wherein the performing of the low-temperature atmospheric pressure plasma process is performed for 10 minutes or less.

### Claim 13 (depends on 8)

The method of claim 8, wherein the performing of the low-temperature atmospheric pressure plasma process is performing a reaction to simultaneously synthesize a TiO2 quantum dot and a TiO2−x quantum dot from a TiCl3 substance, and the X is a real number greater than 0 and less than 2.

### Claim 14 (depends on 13)

The method of claim 13, wherein the performing of the low-temperature atmospheric pressure plasma process makes, in the entire synthesized photocatalyst material, a ratio of the presence of the TiO2 quantum dot and TiO2−x quantum dot be 2:8 to 8:2.