# US 2025/0205685 A1 · Composite oxide, preparation method for composite oxide, hydrogenation catalyst and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0205685 A1
- Document ID: US20250205685A1
- Status: Published application
- Kind: A1
- Application number: 18/850,098
- Filed: 2022-11-04
- Published: 2025-06-26
- Earliest claimed: 2022-03-24
- Assignees: China Petroleum & Chemical Corporation; Sinopec Beijing Research Institute of Chemical Industry
- Applicants: China Petroleum & Chemical Corporation; Sinopec (Beijing) Research Institute of Chemical Industry Co., Ltd.
- Inventors: Zhou DU; Yanhui LIU; Fuchun ZHANG; Zongyu LIU; Jing JI; Yumei REN; Guang YANG
- Web page: https://patentgrep.com/patent/US20250205685A1

## CPC

- B01J 21/063: {Titanium; Oxides or hydroxides thereof}
- B01J 6/00: {Heat treatments such as} Calcining; Fusing {; Pyrolysis (furnaces F27D)}
- B01J 21/00: Catalysts comprising the elements, oxides, or hydroxides of magnesium, boron, aluminium, carbon, silicon, titanium, zirconium, or hafnium
- B01J 21/04: Alumina
- B01J 21/06: Silicon, titanium, zirconium or hafnium; Oxides or hydroxides thereof
- B01J 23/755: Nickel
- B01J 35/00: Catalysts, in general, characterised by their form or physical properties
- B01J 35/30: characterised by their physical properties
- B01J 35/60: characterised by their surface properties or porosity
- B01J 35/613: {10-100 m2/g}
- B01J 35/615: {100-500 m2/g}
- B01J 35/633: {less than 0.5 ml/g}
- B01J 35/635: {0.5-1.0 ml/g}
- B01J 35/647: {2-50 nm}
- B01J 37/031: {Precipitation}
- B01J 37/04: Mixing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/06: Washing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- C07C 5/08: of carbon-to-carbon triple bonds
- C07C 5/09: to carbon-to-carbon double bonds
- C07C 11/167: 1, 3-Butadiene
- C07C 2521/04: Alumina
- C07C 2521/06: Silicon, titanium, zirconium or hafnium; Oxides or hydroxides thereof
- C07C 2523/755: Nickel
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS

## Abstract

A composite oxide contains 60-95 wt % of aluminum oxide and 5-40 wt % of titanium dioxide. The specific surface area of the composite oxide determined by means of BET method is expressed as X m2/g. The average pore diameter of the composite oxide determined by means of nitrogen adsorption isothermal curve method is expressed as Y nm. The ratio of X to Y is 5-30. By means of the determination of X-ray diffraction method, titanium dioxide in an anatase crystalline phase in the composite oxide accounts for 95-100 wt % of the total titanium dioxide. X is in the range of 50-200, preferably X is in the range of 60-180, more preferably in the range of 80-150, and Y is in the range of 5-25 nm. A hydrogenation catalyst that contains the composite oxide shows a high vinyl acetylene conversion rate and a high 1,3-butadiene selectivity.

## Claims

### Claim 1

A composite oxide, comprising 60 to 95 wt % of aluminum oxide and 5 to 40 wt % of titanium dioxide, wherein the composite oxide has a specific surface area expressed as X m2/g as measured by a BET method and an average pore diameter expressed as Y nm as measured by a nitrogen adsorption isotherm method, with a ratio of X to Y being in a range of from 5 to 30, wherein in the composite oxide, titanium dioxide in an anatase crystal phase accounts for 95 wt % to 100 wt % of the total titanium dioxide, as measured by X-ray diffraction method, and wherein X is in a range of from 50 to 200, preferably from 60 to 180, and more preferably from 80 to 150, and Y is in a range of from 5 to 25 nm.

### Claim 2 (depends on 1)

The composite oxide according to claim 1, wherein the composite oxide has a pore volume expressed as Z mL/g, wherein Z is in a range of from 0.3 to 0.5, and wherein a ratio of X to Z is from 220 to 400, and preferably from 250 to 350.

### Claim 3 (depends on 1)

The composite oxide according to claim 1, having at least one of the following features:
X is from 90 to 150;
Y is from 9 to 20, and preferably from 12 to 16;
at least 85% of pores have a pore diameter in a range of 10 to 20 nm;
Z is from 0.3 to 0.4; and/or the composite oxide comprises 5 wt % to 21 wt % of titanium dioxide; and
the composite oxide has a coral thicket-like 3D layered structure.

### Claim 4

A method for preparing a composite oxide, comprises the following steps:
I, dissolving a soluble aluminum source in water to form an aluminum source solution, dissolving a titanium source in an acid solution to form a titanium source solution, and mixing an ammonium salt and an alkali liquid to form a mixed alkali solution;
II, (a) adding the titanium source solution and the mixed alkali solution to the aluminum source solution, and maintaining a resulting mixed solution at a first pH value for a first period of time; (b) adding an additional amount of the mixed alkali solution to the mixed solution, and maintaining a resulting mixed solution at a second pH value for a second period of time; (c) adding an additional amount of the titanium source solution to the mixed solution, and maintaining a resulting mixed solution at a third pH value for a third period of time;
III, after step II(c), raising the temperature of the mixed solution and maintaining that temperature for a fourth period of time to obtain a precipitate; and
IV, drying and calcining the precipitate to obtain a composite oxide comprising alumina and titanium dioxide, with washing and filtering being preferably conducted prior to the drying.

### Claim 5 (depends on 4)

The method according to claim 4, wherein in step II, the first pH value is less than 5, and preferably 3 to 4, the second pH value is greater than 8.5, and preferably 9 to 10, and the third pH value is greater than 7 and less than 9, and preferably 7.5 to 8.5.

### Claim 6 (depends on 4)

The method according to claim 4, wherein each of the first, second and third periods of time is from 5 to 20 minutes, and preferably from 10 to 15 minutes; and/or the fourth period of time is from 20 to 60 minutes.

### Claim 7 (depends on 4)

The method according to claim 4, wherein in step II, an operating temperature is 25° C. to 60° C.; and/or in step III, the temperature is raised to 80° C. to 150° C.; and/or in step IV, a drying temperature is 110° C. to 130° C., and/or a calcining temperature is 800° C. to 1000° C.

### Claim 8

(canceled)

### Claim 9 (depends on 1)

A hydrogenation catalyst, comprising the composite oxide of claim 1 and an active component, preferably the active component is nickel, and preferably the catalyst has a nickel content of 8 to 25 wt %, and more preferably 12 to 20 wt %.

### Claim 10 (depends on 9)

A process for selective hydrogenation of alkynes, comprising subjecting a distillate oil to selective hydrogenation of alkynes in the presence of the hydrogenation catalyst of claim 9 to increase the production of butadiene, wherein the distillate oil comprises a C4 distillate oil, preferably a high-alkyne tail gas co-produced in a butadiene extraction unit; preferably, in the process of selective hydrogenation of alkynes, a reaction temperature is 20° C. to 40° C., a molar ratio of hydrogen to alkynes is 1:1 to 2.5:1, a pressure is 0.5 MPa to 0.8 MPa, and a circulation ratio is 10:1 to 30:1.