# US 2025/0205121 A1 · Dental bulk block and method of manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0205121 A1
- Document ID: US20250205121A1
- Status: Published application
- Kind: A1
- Application number: 19/078,204
- Filed: 2025-03-12
- Published: 2025-06-26
- Earliest claimed: 2021-06-15
- Assignees: Hass Co., Ltd.
- Applicants: Hass Co., Ltd.
- Inventors: Hyung Bong LIM; Yong Su KIM
- Web page: https://patentgrep.com/patent/US20250205121A1

## CPC

- A61K 6/833: Glass-ceramic composites
- A61K 6/836: Glass
- A61C 5/73: Composite crowns
- A61C 5/77: Methods or devices for making crowns
- A61C 13/0022: {Blanks or green, unfinished dental restoration parts}
- A61K 6/16: Refractive index
- A61K 6/17: Particle size
- C03B 32/02: Thermal crystallisation, e.g. for crystallising glass bodies into glass-ceramic articles {(C03B27/012 takes precedence)}
- C03C 4/0021: {for dental use}
- C03C 10/0027: {containing SiO2, Al2O3, Li2O as main constituents}
- C03B 19/02: by casting {molten glass, e.g. injection moulding}
- C03B 25/02: in a discontinuous way
- A61K: PREPARATIONS FOR MEDICAL, DENTAL OR TOILETRY PURPOSES (devices or methods specially adapted for bringing pharmaceutical products into particular physical or administering forms A61J3/00; chemical aspects of, or use of materials for deodorisation of air, for disinfection or sterilisation, or for bandages, dressings, absorbent pads or surgical articles A61L; soap compositions C11D)
- A61C: DENTISTRY; APPARATUS OR METHODS FOR ORAL OR DENTAL HYGIENE (non-driven toothbrushes A46B; {tongue scrapers A61B17/24;} preparations for dentistry A61K6/00; preparations for cleaning the teeth or mouth A61K8/00, A61Q11/00)
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

Provided is a dental bulk block comprising a crystalline phase includes lithium disilicate as a main crystalline phase and eucryptite as a sub-crystalline phase in an amorphous glass matrix that is a functionally graded material having a main crystalline size gradient with respect to the depth thereof, and having no interface at the point of change in the main crystalline size gradient value, and is useful for manufacturing artificial teeth having structural characteristics similar to those of natural teeth, is facile to machine into an artificial tooth prosthesis due to the inclusion of eucryptite as the sub-crystalline phase compared to when only lithium disilicate exists, and can not only shorten the manufacturing time, but also increase the structural stability in terms of force distribution through functional grading of mechanical properties.

## Claims

### Claim 1

A method of manufacturing a dental bulk block, the method comprising:
preparing a block having a predetermined shape by melting a glass composition including 69.0 to 78.0 wt % of SiO2, 12.0 to 14.0 wt % of Li2O, 5.5 to 10 wt % of Al2O3, 0.21 to 0.6 wt % of ZnO, 2.0 to 3.5 wt % of K2O, 0.3 to 1.0 wt % of Na2O, 0.1 to 0.5 wt % of SrO, 0.3 to 1.0 wt % of CaO, 0.1 to 2.0 wt % of La2O3, and 2.0 to 6.0 wt % of P2O5, wherein the molar ratio of Al2O3/(K2O+ZnO) is 1.2 to 2.2, followed by molding and cooling of the melted glass composition in a mold, followed by annealing from 480 to 250° C. at a predetermined rate for 20 minutes to 2 hours; and
heat-treating the block at a temperature in a range of 740 to 850° C. under a temperature gradient in a depth direction of the block.

### Claim 2 (depends on 1)

The method of claim 1, wherein the heat-treating of the block is performed by heating an upper layer of the block to a temperature in a range of 800 to 850° C. and heating a lower layer of the block to a temperature in a range of 740 to 760° C.

### Claim 3 (depends on 1)

The method of claim 1, wherein the heat-treating of the block is performed in a gradient heat treatment furnace at an operating temperature of 800 to 1,000° C. for 1 minute to 40 minutes.

### Claim 4 (depends on 1)

A dental bulk block made according to the method of claim 1, comprising a crystalline phase in an amorphous glass matrix,
wherein the crystalline phase comprises lithium disilicate as a main crystalline phase and eucryptite as a sub-crystalline phase,
wherein the main crystalline phase occupies at least 50 wt % of the entire crystalline phase and the sub-crystalline phrase occupies a remaining wt % of the entire crystalline phase unoccupied by the main crystalline phase, and
wherein the dental bulk block is a functionally graded material having a main crystalline size gradient with respect to a depth thereof and having no interface at a point of change in main crystalline size gradient value.