# US 2025/0191842 A1 · Capacitor manufacturing process capable of controlling capacitor resistance and without welding tin-copper conductive sheet

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0191842 A1
- Document ID: US20250191842A1
- Status: Published application
- Kind: A1
- Application number: 19/055,737
- Filed: 2025-02-18
- Published: 2025-06-12
- Earliest claimed: 2022-08-23
- Assignees: Suzhou Josun Precision Stamping Co., Ltd.
- Applicants: Suzhou Josun Precision Stamping Co., Ltd .
- Inventors: Fan WANG; Chengxiang WANG
- Web page: https://patentgrep.com/patent/US20250191842A1

## CPC

- H01G 4/18: of synthetic material, e.g. derivatives of cellulose (H01G4/16 takes precedence)
- C23C 14/16: on metallic substrates or on substrates of boron or silicon
- C23C 18/1651: {Two or more layers only obtained by electroless plating}
- C23C 18/1653: {Two or more layers with at least one layer obtained by electroless plating and one layer obtained by electroplating}
- C23C 18/1834: {Use of organic or inorganic compounds other than metals, e.g. activation, sensitisation with polymers}
- C23C 18/32: Coating with nickel, cobalt or mixtures thereof with phosphorus or boron (C23C18/50 takes precedence)
- C23C 18/38: Coating with copper
- C23C 18/42: Coating with noble metals
- C23C 18/54: Contact plating, i.e. electroless electrochemical plating
- C23C 28/023: {only coatings of metal elements only}
- C25D 5/10: Electroplating with more than one layer of the same or of different metals (for bearings C25D7/10)
- C25D 5/12: at least one layer being of nickel or chromium
- C25D 7/00: Electroplating characterised by the article coated
- H01G 4/005: Electrodes
- H01G 4/008: Selection of materials
- H01G 4/228: Terminals
- H01G 4/2325: {characterised by the material of the terminals}
- H01G 4/30: Stacked capacitors (H01G4/33 takes precedence)
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR

## Abstract

The present invention discloses a capacitor manufacturing process capable of controlling capacitor resistance and without welding a tin-copper conductive sheet. The manufacturing process includes the following working steps: (1) electroplating, involving: electroplating a capacitor base layer, for being compatible with different metal materials; (2) vacuum plating, involving: vacuum plating a metal layer, for being compatible with different metal materials and non-metal materials; and (3) electroplating, involving: electroplating a metal outer layer, for reducing a capacitor resistance value and further controlling the capacitor resistance to be less than 3 milliohms. The beneficial effects of the present invention lie in that: by adopting a process, different metal materials and non-metal materials can be directly combined at the same time, and a capacitor can be directly welded onto a circuit board so as to meet the use requirements.

## Claims

### Claim 1

A capacitor manufacturing process capable of controlling capacitor resistance and without welding a tin-copper conductive sheet, comprising the following working steps:
(1) electroplating, involving: electroplating a capacitor base layer, for being compatible with different metal materials;
(2) vacuum plating, involving: vacuum plating a metal layer, for being compatible with different metal materials and non-metal materials; and
(3) electroplating, involving: electroplating a metal outer layer, for reducing a capacitor resistance value and further controlling the capacitor resistance to be less than 3 milliohms; wherein
the step (1) electroplating a capacitor base layer comprises the following working steps:
1) washing and degreasing, involving: removing oil stains generated during a manufacturing procedure on a surface of a product by using ultrasonic waves and a degreasing agent;
2) washing, involving: washing with pure water at room temperature, for removing a residual degreasing agent on the surface of the product;
3) zinc deposition, involving: soaking in a zinc solution for zinc deposition to facilitate subsequent electroplating;
4) washing and activation, involving: activating the product by using a sulfuric acid pure water solution containing 5%-10% of sulfuric acid, allowing a metal surface layer of the product to maintain an active state for electroplating, wherein the washing refers to performing washing in pure water at room temperature, and the washing refers to flipping the product in the pure water to clean the surface of the product;
5) electroless nickel plating, wherein an electroless nickel solution for the electroless nickel plating comprises 25 g/L-28 g/L nickel sulfate, 23 g/L-28 g/L sodium hypophosphite, and a remaining amount of ionized water;
6) washing and activation, involving: activating the product by using a sulfuric acid pure water solution containing 5%-10% of sulfuric acid, allowing a metal surface layer of the product to maintain an active state for electroplating, wherein the washing refers to performing washing in pure water at room temperature, and the washing refers to flipping the product in the pure water to clean the surface of the product; and
7) gold plating, involving: performing electroplating in a gold solution at 35-75° C. for 5-10 min or using chemical plating;
the step (2) vacuum plating a metal layer comprises the following working steps:
8) washing and drying, involving: washing a residual electroplating solution on the surface of the product with pure water, wherein the washing refers to flipping the product in the pure water to clean the surface of the product; and drying the product with hot air to remove residual moisture on the surface of the product;
9) vacuum electroplating a metal layer, wherein production starts in a state when a furnace temperature of a vacuum furnace is 150-280° C. and a vacuum degree is controlled to be 3.0×10−3 Pa, and an operating time is 30-60 min;
10) cooling and discharging, involving: after the furnace temperature drops to below 100° C., releasing air to make vacuum pressure return to a normal atmospheric pressure state to open the furnace; and
11) inspection, involving: checking whether different metal materials and non-metal materials in the product are compatible by using inspection equipment; wherein the step (3) electroplating a metal outer layer comprises the following steps:
12) washing and activation, involving: activating the product by using a sulfuric acid pure water solution containing 5%-10% of sulfuric acid, allowing a metal surface layer of the product to maintain an active state for electroplating, wherein the washing refers to performing washing in pure water at room temperature and to flipping the product in the pure water to clean the surface of the product;
13) copper plating, involving: electroplating the product in a copper solution at 35-75° C. for 40-90 min or using chemical plating;
14) washing and activation, involving: activating the product by using a sulfuric acid pure water solution containing 5%-10% of sulfuric acid, allowing a metal surface layer of the product to maintain an active state for electroplating, wherein the washing refers to performing washing in pure water at room temperature and to flipping the product in the pure water to clean the surface of the product;
15) Ni plating, involving: performing electroplating in a nickel solution at 35-75° C. for 15-30 min;
16) washing and activation, involving: activating the product by using a sulfuric acid pure water solution containing 5%-10% of sulfuric acid, allowing a metal surface layer of the product to maintain an active state for electroplating, wherein the washing refers to performing washing in pure water at room temperature and to flipping the product in the pure water to clean the surface of the product;
17) Ag plating or Au plating, wherein the Ag plating refers to performing electroplating in a silver solution at 35-75° C. for 5-10 min or using chemical plating; and the Au plating refers to performing electroplating in a gold solution at 30-60° C. for 5-10 min or using chemical plating;
18) washing and drying, involving: washing a residual electroplating solution on the surface of the product with pure water, wherein the washing refers to flipping the product in the pure water to clean the surface of the product; and drying the product with hot air to remove residual moisture on the surface of the product; and
19) inspection, involving: inspecting whether resistance of the product is less than 3 milliohms by using inspection equipment.

### Claim 2 (depends on 1)

The capacitor manufacturing process capable of controlling capacitor resistance and without welding a tin-copper conductive sheet according to claim 1, wherein the activation in step (1) and step (3) refers to performing activation in an activation solution at room temperature.

### Claim 3 (depends on 2)

The capacitor manufacturing process capable of controlling capacitor resistance and without welding a tin-copper conductive sheet according to claim 2, wherein a temperature of a solution within the ultrasonic waves in step (1) is 50-80° C., and the time is 15 min.

### Claim 4 (depends on 3)

The capacitor manufacturing process capable of controlling capacitor resistance and without welding a tin-copper conductive sheet according to claim 3, wherein a cleaning time in step (1), step (2), and step (3) is 1-2 min.

### Claim 5 (depends on 4)

The capacitor manufacturing process capable of controlling capacitor resistance and without welding a tin-copper conductive sheet according to claim 4, wherein vacuum electroplated metal in step (2) is any one of Ag, Au, Cu.

### Claim 6 (depends on 1)

A capacitor, wherein the capacitor is manufactured by adopting the manufacturing process according to claim 1.