# US 2025/0188642 A1 · Method of forming a high-temperature superconducting single crystal and a high-temperature superconducting single crystal formed thereby

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0188642 A1
- Document ID: US20250188642A1
- Status: Published application
- Kind: A1
- Application number: 18/734,576
- Filed: 2024-06-05
- Published: 2025-06-12
- Earliest claimed: 2023-12-12
- Assignees: Hyundai Motor Company; Kia Corporation; Seoul National University R&Db Foundation
- Applicants: Hyundai Motor Company; Kia Corporation; Seoul National University R&Db Foundation
- Inventors: Kyung Sik Choi; Hoo Dam Lee; Tae Gyu Lee; Hyung Kwan Jang; Byung Ho Min; Jun Hyeok Choi; Kee Hoon Kim; Yeahan Sur; Jungwoo Lee; Sukho Kim; Chung Ha Park
- Web page: https://patentgrep.com/patent/US20250188642A1

## CPC

- C30B 11/14: characterised by the seed, e.g. its crystallographic orientation
- C30B 11/003: {Heating or cooling of the melt or the crystallised material}
- C30B 29/225: {based on rare earth copper oxides, e.g. high T-superconductors}
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

A method of forming a high-temperature superconducting single crystal is capable of facilitating a high-temperature superconducting single crystal containing rare-earth metals to grow using a multilayer seed. The method includes: preparing a rare earth barium copper oxide (ReBCO)-based precursor containing rare-earth metals; preparing a plurality of seeds that differ in lattice constant; placing the prepared seeds on top of the precursor through stacking; melting a portion of the precursor by heating the precursor to a peritectic temperature thereof or higher; and growing a single crystal by cooling the precursor to a crystal growth temperature thereof to match a crystal orientation of the seeds. Despite being used to increase the area and maintain the soundness of the single-crystalline specimen in most single-crystal growth, a buffer herein is to facilitate a single crystal of a new composition to grow.

## Claims

### Claim 1

A method of forming a high-temperature superconducting single crystal, the method comprising:
placing a plurality of seeds that differ in lattice constant on a rare earth metal barium copper oxide (ReBCO)-based precursor containing a rare-earth metal;
melting a portion of the ReBCO-based precursor by heating the ReBCO-based precursor to a peritectic temperature thereof or higher; and
growing a single crystal by cooling the ReBCO-based precursor to a crystal growth temperature thereof to match a crystal orientation of the plurality of seeds.

### Claim 2 (depends on 1)

The method of claim 1, wherein the ReBCO-based precursor is a gadolinium holmium barium copper oxide ((Gd,Ho)BCO)-based precursor comprising Gd and Ho as the rare-earth metals.

### Claim 3 (depends on 2)

The method of claim 2, wherein the (Gd,Ho)BCO-based precursor is (Gd1-xHox)Ba2Cu3O7-δ (where 0.4<x<0.6, and δ<7) (where Ba=barium, Cu=copper, 0=oxygen).

### Claim 4 (depends on 1)

The method of claim 1, wherein the ReBCO-based precursor is prepared by:
mixing gadolinium (III) oxide (Gd2O3), barium carbonate (BaCO3), copper (II) oxide (CuO), and Ho-containing powders according to chemical composition amounts to prepare a mixed powder; and
shaping the mixed powder by applying a pressure to prepare the precursor.

### Claim 5 (depends on 1)

The method of claim 1, wherein:
the plurality of seeds comprises seed crystals and buffer crystals; and
a difference in lattice constant between the ReBCO-based precursor and the buffer crystals is smaller than a difference in lattice constant between the precursor and the seed crystals.

### Claim 6 (depends on 5)

The method of claim 5, wherein a difference in peritoneal temperature between the ReBCO-based precursor and the buffer crystals is smaller than a difference in peritectic temperature between the ReBCO-based precursor and the seed crystals.

### Claim 7 (depends on 5)

The method of claim 5, wherein the difference in lattice constant between the ReBCO-based precursor and the buffer crystals is at a level of 0.8% or less.

### Claim 8 (depends on 5)

The method of claim 5, wherein the seed crystals are NdBa2Cu3O7-δ (where δ<7).

### Claim 9 (depends on 5)

The method of claim 5, wherein the buffer crystals are GdBa2Cu3O7-δ (where δ<7).

### Claim 10 (depends on 5)

The method of claim 5, wherein in placing the plurality of seeds, the buffer crystals are placed closer to the ReBCO-based precursor and the seed crystals are placed further from the ReBCO-based precursor.

### Claim 11 (depends on 1)

The method of claim 1, wherein melting the portion of the ReBCO-based precursor comprises:
a first heating process in which the ReBCO-based precursor is heated to a first heating temperature; and
a second heating process in which the ReBCO-based precursor is heated to a second heating temperature higher than the first heating temperature.

### Claim 12 (depends on 11)

The method of claim 11, wherein:
the first heating temperature is lower than the peritectic temperature of the ReBCO-based precursor; and
the second heating temperature is higher than the peritectic temperature of the ReBCO-based precursor and lower than a peritectic temperature of the seed crystals.

### Claim 13 (depends on 1)

The method of claim 1, wherein the growing comprises:
a first growth process in which the plurality of seeds is cooled to a first growth temperature;
a second growth process in which the plurality of seeds is cooled to a second growth temperature lower than the first growth temperature to grow the single crystal; and
a third growth process in which the grown single crystal is cooled to room temperature.

### Claim 14 (depends on 13)

The method of claim 13, wherein:
the first growth temperature of the first growth process is the peritectic temperature of the ReBCO-based precursor; and
the second growth temperature of the second growth process is the crystal growth temperature, which is lower than the peritectic temperature of the ReBCO-based precursor.

### Claim 15 (depends on 13)

The method of claim 13, wherein a cooling rate of the first growth process is higher than a cooling rate of the second growth process.

### Claim 16 (depends on 1)

A high-temperature superconducting single crystal formed according to the method of claim 1.

### Claim 17 (depends on 16)

The high-temperature superconducting single crystal of claim 16, wherein the high-temperature superconducting single crystal is (Gd1-xHox)Ba2Cu3O7-δ (where 0.4<x<0.6, and δ<7).