# US 2025/0188282 A1 · Green high viscosity toughness asphalt modifier, modified asphalt, bituminous concrete and preparation methods thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0188282 A1
- Document ID: US20250188282A1
- Status: Published application
- Kind: A1
- Application number: 19/059,833
- Filed: 2025-02-21
- Published: 2025-06-12
- Earliest claimed: 2024-03-18
- Assignees: Changsha University of Science and Technology
- Applicants: Changsha University of Science & Technology
- Inventors: Chengdong Xia; Dikuan Wang; Songtao Lv; Zhen Leng; Jianlong Zheng
- Web page: https://patentgrep.com/patent/US20250188282A1

## CPC

- C08L 95/00: Compositions of bituminous materials, e.g. asphalt, tar, pitch
- C08J 3/005: {Processes for mixing polymers}
- C08J 3/226: {using a polymer as a carrier}
- C08K 3/346: {Clay}
- C08K 9/04: Ingredients treated with organic substances {(treated with macromolecular compounds C08K9/08)}
- C08L 17/00: Compositions of reclaimed rubber
- C08L 23/06: Polyethylene
- C08L 23/12: Polypropene
- C08J 2395/00: Bituminous materials, e.g. asphalt, tar or pitch
- C08J 2417/00: Characterised by the use of reclaimed rubber
- C08J 2423/06: Polyethene
- C08J 2423/12: Polypropene
- C08K 2201/011: Nanostructured additives
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2205/035: containing four or more polymers in a blend
- C08L 2205/08: containing additives to improve the compatibility between two polymers
- C08L 2207/20: Recycled plastic
- C08L 2207/322: Liquid component is processing oil
- C08L 2310/00: Masterbatches
- C08L 2555/86: Polymers containing aliphatic hydrocarbons only, e.g. polyethylene, polypropylene or ethylene-propylene-diene copolymers
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

A green high viscosity toughness asphalt modifier includes following raw material components by weight: 70-232 parts of waste rubber and plastic mixture; 4-10 parts of nano-clay material; and 15-50 parts of compatilizer. A preparation method of the green high viscosity toughness asphalt modifier includes steps of (1) preparing masterbatch by a first melt blending extrusion, which includes weighing the nano-clay material, the waste rubber and plastic mixture and the compatilizer in accordance with a weight ratio of 1:(2-4):(1-2), mixing evenly at high speed, extruding and granulating for obtaining the masterbatch; and (2) performing a second melt blending extrusion, which includes mixing evenly the waste rubber and plastic mixture, the masterbatch obtained by the step (1) and the compatilizer with a weight ratio of (5-9):(1-5):(1-3) at high speed, extruding and granulating for obtaining the asphalt modifier.

## Claims

### Claim 1

A green high viscosity toughness asphalt modifier, which comprises following raw material components by weight:
70-232 parts of waste rubber and plastic mixture;
4-10 parts of nano-clay material; and
15-50 parts of compatilizer, wherein:
the waste rubber and plastic mixture consists of waste rubber and waste plastics with a mass ratio in a range of 1:(0.8-1.5);
the waste rubber is waste rubber powder with a particle size in a range of 40 to 120 meshes, wherein a content of rubber hydrocarbon in the waste rubber is larger than 50%;
the waste plastics are waste polyethylene particles or waste polypropylene particles with a particle size in a range of 10 to 15 meshes;
the nano-clay material is at least one member selected from a group consisting of nano-organic montmorillonite, nano-rectorite, and nano-vermiculite;
the asphalt modifier is prepared by secondary melt blending extrusion method, wherein the secondary melt blending extrusion method comprises steps of:
(1) preparing masterbatch by a first melt blending extrusion, which comprises weighing the nano-clay material, the waste rubber and plastic mixture and the compatilizer in accordance with a weight ratio of 1:(2-4):(1-2), mixing evenly at high speed, extruding and granulating for obtaining the masterbatch; and
(2) performing a second melt blending extrusion, which comprises mixing evenly the waste rubber and plastic mixture, the masterbatch obtained by the step (1) and the compatilizer with a weight ratio of (5-9):(1-5):(1-3) at high speed, extruding and granulating for obtaining the asphalt modifier.

### Claim 2 (depends on 1)

The green high viscosity toughness asphalt modifier according to claim 1, wherein the compatilizer is aromatic oil with a content of aromatic hydrocarbon larger than 80%.

### Claim 3 (depends on 1)

The green high viscosity toughness asphalt modifier according to claim 1, wherein in the step (1), mixing evenly at high speed is performed in a high-speed mixer, a rotational speed of the high-speed mixer is controlled in a range of 300-450 r/min, and a rotational time thereof is controlled in a range of 15-20 min.

### Claim 4 (depends on 1)

The green high viscosity toughness asphalt modifier according to claim 1, wherein in the step (2), mixing evenly at high speed is performed in a high-speed mixer, a rotational speed of the high-speed mixer is controlled in a range of 300-450 r/min, and a rotational time thereof is controlled in a range of 15-20 min.

### Claim 5 (depends on 1)

The green high viscosity toughness asphalt modifier according to claim 1, wherein in the step (1), extruding is performed by a twin-screw extruder; a cylinder of the twin-screw extruder has a feeding section, a discharge section and at least one middle section, a temperature of the feeding section and the discharge section is 170° C., a temperature of the at least one middle section is 175° C., and a rotational speed of a twin-screw is in a range of 100-180 r/min.

### Claim 6 (depends on 1)

The green high viscosity toughness asphalt modifier according to claim 1, wherein in the step (2), extruding is performed by a twin-screw extruder; a cylinder of the twin-screw extruder has a feeding section, a discharge section and at least one middle section, a temperature of the feeding section and the discharge section is 170° C., a temperature of the at least one middle section is 175° C., and a rotational speed of a twin-screw is in a range of 100-180 r/min.

### Claim 7 (depends on 1)

The green high viscosity toughness asphalt modifier according to claim 1, wherein:
the step (1) further comprises steps of cooling by a sink after extruding, and then pulling to a granulator before granulating, wherein a rotational speed of the granulator is in a range of 200 to 400 r/min;
the step (2) further comprises steps of cooling by the sink after extruding, and then pulling to the granulator before granulating, wherein the rotational speed of the granulator is in the range of 200 to 400 r/min.

### Claim 8 (depends on 1)

The green high viscosity toughness asphalt modifier according to claim 1, wherein a particle size of the masterbatch prepared by the step (1) is controlled in a range of 10 to 15 meshes, and a particle size of the asphalt modifier prepared by the step (2) is controlled in a range of 10 to 15 meshes.

### Claim 9 (depends on 1)

A green high viscosity toughness modified asphalt, which comprises matrix asphalt and the green high viscosity toughness asphalt modifier according to claim 1, wherein a weight ratio of the green high viscosity toughness asphalt modifier and the matrix asphalt is in a range of (15-20):(80-85).

### Claim 10 (depends on 9)

A preparation method of the green high viscosity toughness modified asphalt according to claim 9, wherein the preparation method comprises steps of:
(1) heating the matrix asphalt till melting;
(2) adding the green high viscosity toughness asphalt modifier into the molten matrix asphalt, and stirring with a temperature in a range of 175-180° C.;
(3) shearing at high speed for 20-30 min with a temperature in a range of 175-180° C.;
(4) dispersing the sheared asphalt for 10-15 min at a rotational speed in a range of 300-500 r/min with a temperature in a range of 175-180° C.; and
(5) performing heat preservation on a product of the step (4) with a temperature in a range of 175-185° C., and developing for 60-70 min in a closed state for obtaining the modified asphalt.

### Claim 11 (depends on 10)

The preparation method according to claim 10, wherein:
in the step (1), the matrix asphalt is heated at a temperature in a range of 135-140° C. for 30-40 min till melting; and
in the step (2), shearing is performed at a speed in a range of 4500-6000 r/min.