# US 2025/0187972 A1 · Phase separated glasses

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0187972 A1
- Document ID: US20250187972A1
- Status: Published application
- Kind: A1
- Application number: 18/847,431
- Filed: 2023-03-27
- Published: 2025-06-12
- Earliest claimed: 2022-04-01
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Venkatesh Botu; Ling Cai; Heath Aaron Filkins; Lisa Ann Lamberson; Aize Li; Charlene Marie Smith; Liping Xiong Smith
- Web page: https://patentgrep.com/patent/US20250187972A1

## CPC

- C03B 32/00: Thermal after-treatment of glass products not provided for in groups {C03B19/00} , C03B25/00 - C03B31/00 {or C03B37/00}, e.g. crystallisation, eliminating gas inclusions or other impurities; {Hot-pressing vitrified, non-porous, shaped glass products}
- C03C 3/093: containing zinc or zirconium
- C03B 17/064: {by the overflow downdraw fusion process; Isopipes therefor}
- C03C 3/091: containing aluminium
- C03C 3/095: containing rare earths
- C03C 4/16: for dielectric glass
- C03C 11/005: {obtained by leaching after a phase separation step}
- C03C 15/00: Surface treatment of glass, not in the form of fibres or filaments, by etching (etching or surface-brightening compositions, in general C09K13/00)
- C03C 23/007: {by thermal treatment}
- C03B 17/06: Forming glass sheets
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

A method of making a glass article using a phase separated silicate glass including a silica rich first phase and a boron rich second phase. The phase separated silica glass is etched with an etchant to remove at least a portion of the second phase and obtain a high silica content porous glass article. The porous glass article may be heat treated to consolidate the porous glass article to close the pores of the porous glass article and obtain a consolidated glass article with very low dielectric properties. Various glass compositions are disclosed that phase separate via spinodal decomposition.

## Claims

### Claim 1

A method of making a glass article, comprising
forming a molten glass, the molten glass undergoing spinodal decomposition to produce a phase separated molten glass comprising a first phase, a second phase, and a total SiO2 content in a range from about 59 mol % to about 69 mol % and a B2O3 content in a range from about 9 mol % to about 20 mol %;
drawing the phase separated molten glass into a glass sheet; and
exposing the glass sheet to a first acid solution at a temperature between about 60° C. to about 95° C. for about 16 hours to about 24 hours to remove at least a portion of the second phase from the glass sheet and obtain a porous glass sheet comprising a total silica content greater than about 95 mol %.

### Claim 2 (depends on 1)

The method of claim 1, wherein an open porosity of the porous glass sheet is greater than about 28%.

### Claim 3 (depends on 1)

The method of claim 1, wherein the first acid solution comprises about 5 wt % to about 40 wt % of at least one of HCl, H2SO4, HNO3, HF, or H3PO4.

### Claim 4 (depends on 3)

The method of claim 3, wherein the first acid solution comprises HCl.

### Claim 5 (depends on 4)

The method of claim 4, wherein the first acid solution comprises about 5 wt % HCl.

### Claim 6 (depends on 1)

The method of claim 1, wherein the first acid solution comprises about 5 wt % to about 40 wt % of at least one of citric acid or acetic acid.

### Claim 7 (depends on 1)

The method of claim 1, further comprising heating the porous glass sheet to a temperature between about 500° C. to about 700° C. for about 45 minutes to about 75 minutes.

### Claim 8 (depends on 1)

The method of claim 1, further comprising heating the porous glass sheet to a temperature between about 900° C. to about 1100° C. for about 1 hour to about 24 hours to consolidate the porous glass sheet and obtain a consolidated glass sheet, the consolidated glass sheet comprising a dielectric constant Dk less than about 4.0 when measured at 10 GHz using a split post dielectric resonator.

### Claim 9 (depends on 8)

The method of claim 8, wherein Dk is less than about 3.5 when measured at 10 GHz using the split post dielectric resonator.

### Claim 10 (depends on 8)

The method of claim 8, wherein the consolidated glass sheet comprises a loss tangent Df less than about 0.0075 when measured at 10 GHz using the split post dielectric resonator.

### Claim 11 (depends on 8)

The method of claim 8, wherein the consolidation temperature is equal to or greater than about 1000° C.

### Claim 12 (depends on 11)

The method of claim 11, wherein the consolidated glass sheet comprises a loss tangent Df less than about 0.003 when measured at 10 GHz using the split post dielectric resonator.

### Claim 13 (depends on 12)

The method of claim 12, wherein Df is less than about 0.001 when measured at 10 GHz.

### Claim 14 (depends on 1)

The method of claim 1, further comprising exposing the porous glass sheet to a second acid solution comprising HF for about 1 minute to about 15 minutes prior to the heat treating.

### Claim 15 (depends on 1)

The method of claim 1, wherein the drawing the molten glass into the glass sheet comprises flowing the molten glass over converging forming surfaces of a forming body as separate streams of molten glass, the separate streams of molten glass joining along a bottom edge of the forming body.

### Claim 16 (depends on 1)

The method of claim 1, wherein the drawing the molten glass into the glass sheet comprises flowing the molten glass from a slot positioned in a bottom of a vessel.

### Claim 17 (depends on 1)

A glass article made by the method of claim 1.

### Claim 18 (depends on 8)

A glass article made by the method of claim 8.

### Claim 19

A glass article comprising a spinodally decomposed glass including a first phase and a second phase, the glass comprising on an oxide basis:
SiO2 from about 57 mol % to about 70 mol %
Al2O3 from about 4.7 mol % to about 10.5 mol %
B2O3 from about 11.2 mol % to about 15.2 mol %
ZnO from about 1.2 mol % to about 7.4 mol %; and
one or more alkaline earth oxides (RO) totaling from about 3.7 mol % to about −20 mol %, wherein RO is selected from MgO, CaO, SrO, and BaO.

### Claim 20 (depends on 19)

The glass article of claim 19, wherein the glass comprises SnO from about 0.09 mol % to about 0.15 mol %.

### Claim 21 (depends on 19)

The glass article of claim 19, wherein the glass comprises MgO from about 1.5 mol % to about 9.6 mol %.

### Claim 22 (depends on 21)

The glass article of claim 21, wherein MgO/ZnO is from about 0 to about 3.7.

### Claim 23 (depends on 21)

The glass article of claim 21, wherein B2O3/ZnO is from about 1.6 to about 12.6

### Claim 24 (depends on 19)

The glass article of claim 19, wherein a dielectric constant Dk of the glass is from about 4.5 to about 6.3 when measured at 10 GHz using a split post dielectric resonator.

### Claim 25 (depends on 24)

The glass article of claim 24, wherein a loss tangent Df of the glass is from about 0.002 to about 0.005 when measured at 10 GHz using the split post dielectric resonator.

### Claim 26 (depends on 19)

The glass article of claim 19, further comprising at least one of La2O3, Y2O3, or Li2O in an amount less than about 3.0 mol %.

### Claim 27 (depends on 19)

The glass article of claim 19, further comprising CaO from about 0.05 mol % to about 4.8 mol %.

### Claim at position 28

28-44. (canceled)