# US 2025/0179223 A1 · Method for reduction of discoloration in latex polymers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0179223 A1
- Document ID: US20250179223A1
- Status: Published application
- Kind: A1
- Application number: 18/686,028
- Filed: 2022-09-01
- Published: 2025-06-05
- Earliest claimed: 2021-09-29
- Assignees: Sabic Global Technologies B.V.
- Applicants: Sabic Global Technologies B.V.
- Inventors: Nasser Mansour Alsubaie; Dejin Li
- Web page: https://patentgrep.com/patent/US20250179223A1

## CPC

- C08F 6/22: Coagulation
- C08F 297/048: {polymerising vinyl aromatic monomers, conjugated dienes and polar monomers}
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

A method comprising providing a polymer latex comprising particles of polymer in aqueous dispersion, adding a peroxide in an amount of 0.005 to 5, preferably 0.01 to 4, parts by weight peroxide per 100 parts by weight of dried polymer to the polymer latex at a pH of at least 8.5, preferably at least 9, and, after the contacting, coagulating the polymer latex.

## Claims

### Claim 1

A method comprising
providing a polymer latex comprising polymer particles in an aqueous dispersion, wherein the polymer particles comprise polymers of one or more of vinyl aromatic monomers, acrylic monomers,
adding a peroxide in an amount of 0.005 to 5 parts by weight peroxide per 100 parts by weight of dried polymer to the polymer latex at a pH of at least 8.5, and,
after adding the peroxide, coagulating the polymer latex,
wherein a contact time defined as a time from initiation of the adding of the peroxide until the initiation of coagulating is at least 2 minutes.

### Claim 2 (depends on 1)

The method of claim 1 wherein the contact time is at least 5 minutes.

### Claim 3 (depends on 1)

The method of claim 1 wherein the contact time is up to 24 hours.

### Claim 4 (depends on 1)

The method of claim 1 wherein coagulating occurs within 3 hours, after initiation of the adding of the peroxide.

### Claim 5 (depends on 1)

The method of claim 1 further comprising drying the coagulated polymer latex.

### Claim 6 (depends on 1)

The method of claim 1 wherein the providing comprises emulsion polymerizing to form the polymer latex.

### Claim 7 (depends on 1)

The method of claim 1 wherein the polymer latex is a latex of a copolymer of a styrenic monomer and one or more of acrylonitrile monomers and conjugated diene monomers.

### Claim 8 (depends on 1)

The method of claim 1 wherein the polymer latex is stored at a temperature of 20 to 70° C. prior to adding the peroxide.

### Claim 9 (depends on 1)

The method of claim 1 wherein two or more batches of the polymer latex are combined to form the provided polymer latex.

### Claim 10 (depends on 1)

The method of claim 1 comprising mixing during the contact time.

### Claim 11 (depends on 1)

The method of claim 1 wherein the pH is no greater than 12.

### Claim 12 (depends on 1)

The method of claim 1 wherein the polymer latex comprises 30 to 45 weight percent solids in aqueous solution.

### Claim 13 (depends on 1)

The method of claim 1 wherein the adding of the peroxide at a pH of at least 8.5 before the coagulating increases L* by at least 2, decreases a* by at least 1.5, and/or decreases yellowness index by at least 1 of the polymer as compared to a polymer that is otherwise the same but is not contacted with peroxide at a pH of at least 8.5 before coagulation.

### Claim 14 (depends on 1)

The method of claim 1 wherein the peroxide comprises an organic peroxide, an organic hydroperoxide, hydrogen peroxide or a combination thereof.

### Claim 15 (depends on 1)

The method of claim 1 further comprising compounding the polymer latex with a second polymer.

### Claim 16

A method comprising
providing a polymer latex comprising polymer particles in an aqueous dispersion, wherein the polymer particles comprise a copolymer of a styrenic monomer, an acrylonitrile monomer, and a conjugated diene monomer,
adding a peroxide comprising hydrogen peroxide in an amount of 0.005 to 5 parts by weight peroxide per 100 parts by weight of dried polymer to the polymer latex at a pH of at least 9 and at most 12, and,
after adding the peroxide, coagulating the polymer latex,
wherein a contact time defined as a time from initiation of the adding of the peroxide until the initiation of coagulating is at least 10 minutes and up to 1 hour.

### Claim 17 (depends on 16)

The method of claim 16, wherein the polymer latex comprises 30 to 45 weight percent solids in an aqueous solution.

### Claim 18 (depends on 1)

The method of claim 1, wherein the peroxide is added to the polymer latex in an amount of is 0.01 to 1 part by weight based on 100 parts of dried polymer.

### Claim 19

A method comprising
providing a polymer latex comprising polymer particles in an aqueous dispersion, wherein the polymer particles comprise an acrylonitrile-butadiene-styrene copolymer;
adding a peroxide comprising hydrogen peroxide in an amount of 0.01 to 0.5 part by weight peroxide per 100 parts by weight of dried polymer to the polymer latex at a pH of at least 9 and at most 12, and
after adding the peroxide, coagulating the polymer latex,
wherein a contact time defined as a time from initiation of the adding of the peroxide until the initiation of coagulating is at least 10 minutes and up to 1 hour,
wherein the polymer latex comprises 30 to 45 weight percent solids in an aqueous solution.

### Claim 20 (depends on 19)

The method of claim 19, wherein the polymer after coagulating has an L* that is higher by at least 3 than the L* of a polymer that is otherwise the same but that is not contacted with the peroxide at a pH of at least 9 and at most 12 prior to coagulation.