# US 2025/0178267 A1 · Method for producing selectively metallised three-dimensional items with a masking coating composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0178267 A1
- Document ID: US20250178267A1
- Status: Published application
- Kind: A1
- Application number: 18/843,693
- Filed: 2023-03-03
- Published: 2025-06-05
- Earliest claimed: 2022-03-04
- Assignees: Jet Metal Technologies
- Applicants: Jet Metal Technologies
- Inventors: Samuel Paul Henry STREMSDOERFER; Emilie LAI
- Web page: https://patentgrep.com/patent/US20250178267A1

## CPC

- B29C 51/264: {Auxiliary operations prior to the thermoforming operation, e.g. cutting (B29C51/42, B29C51/46 take precedence)}
- C09D 5/008: {Temporary coatings (C09D5/20 takes precedence)}
- B29C 51/02: Combined thermoforming and manufacture of the preform
- B29C 51/16: Lining or labelling
- B29C 51/162: {of deep containers or boxes}
- B29C 51/266: {Auxiliary operations after the thermoforming operation (B29C51/42, B29C51/44, B29C51/46 take precedence)}
- B29C 51/42: Heating or cooling
- B29C 51/46: Measuring, controlling or regulating
- C08F 265/06: Polymerisation of acrylate or methacrylate esters on to polymers thereof
- C09D 4/06: {Organic non-macromolecular compounds having at least one polymerisable carbon-to-carbon unsaturated bond} in combination with a macromolecular compound other than an unsaturated polymer of groups C09D159/00 - C09D187/00
- C09D 175/04: Polyurethanes
- C25D 5/022: {using masking means}
- C25D 5/56: of plastics
- H05K 1/0284: {Details of three-dimensional rigid printed circuit boards (H05K1/119 takes precedence; shaping of the substrate H05K3/0014)}
- H05K 3/0014: {Shaping of the substrate, e.g. by moulding}
- H05K 3/143: {Masks therefor (H05K3/048 takes precedence)}
- B29K 2025/00: Use of polymers of vinyl-aromatic compounds {or derivatives thereof} as moulding material
- B29K 2033/08: {Polymers of acrylic acid esters, e.g. PMA, i.e. polymethylacrylate}
- B29K 2033/12: {Polymers of methacrylic acid esters, e.g. PMMA, i.e. polymethylmethacrylate}
- B29K 2067/00: Use of polyesters {or derivatives thereof}, as moulding material
- B29K 2075/00: Use of {PU, i.e.} polyureas or polyurethanes {or derivatives thereof}, as moulding material
- B29K 2077/00: Use of {PA, i.e.} polyamides, e.g. polyesteramides {or derivatives thereof}, as moulding material
- B29K 2105/16: Fillers
- B29K 2705/00: Use of metals, their alloys or their compounds, for preformed parts, e.g. for inserts
- B29K 2995/0006: Dielectric
- B29K 2995/0007: Insulating
- B29L 2031/3425: {Printed circuits}
- B29L 2031/3456: {Antennas, e.g. radomes}
- B29L 2031/779: {Heating equipment}
- H05K 1/0313: {Organic insulating material}
- H05K 2201/0129: Thermoplastic polymer, e.g. auto-adhesive layer; Shaping of thermoplastic polymer
- H05K 2201/0158: Polyalkene or polyolefin, e.g. polyethylene [PE], polypropylene [PP]
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES

## Abstract

The invention relates to a composition for making a film-forming masking coating adhering to at least part of a surface of a substrate intended to be thermoformed for manufacturing a selectively metallized three-dimensional item, said composition comprising at least one organic polymer matrix formed of one or more organic monomers and/or polymers, said polymer matrix being curable to form said masking coating that, after curing, for a thickness of between 0.1 μm and 50 μm, has a deformation ratio at break higher than 30%, at a temperature of between 20° C. and 270° C. The invention is particularly adapted for making a composition suitable for making a coating on the surface of a substrate intended to be thermoformed.

## Claims

### Claim 1

A method for manufacturing a selectively metallized three-dimensional item, comprising at least:
a step of depositing a composition in the liquid or paste state on a surface of a thermoformable substrate, said composition comprising at least one organic polymer matrix formed of one or more organic monomers and/or polymers, said composition comprising neither electrically conductive particles nor magnetic particles,
a step of curing said composition so deposited onto the substrate to form a film-forming masking coating adhering to the latter, said masking coating having a thickness of between 0.1 μm and 30 μm,
a step of thermoforming the substrate so coated with the film-forming masking coating,
a step of metallizing the substrate to form a metal deposit on the latter;
and a step of eliminating the masking coating using an alkaline solution, posteriorly or concomitantly to the substrate metallization step.

### Claim 2 (depends on 1)

The manufacturing method according to claim 1, characterized in that, in the thermoforming step, the substrate is heated to a thermoforming temperature of between 20° C. and 270° C., preferably between 50° C. and 250° C., more preferentially between 70° C. and 230° C.

### Claim 3 (depends on 2)

The manufacturing method according to claim 2, characterized in that, at the thermoforming temperature, the masking coating has a deformation ratio at break that is higher than 30%, the deformation ratio at break being measured using a test of thermoforming a substrate coated with a grid pattern of masking coating, where the steps of the manufacturing method are reproduced so that:
the deposition step and the curing step enable to obtain a substrate coated with the masking coating according to a pattern of masking coating squares, said squares being of same size and being regularly spaced apart by grid lines non covered with the masking coating, said squares being for example of 5 mm side and said grid lines being for example of 300 μm wide,
in the step of thermoforming the substrate so coated with the pattern of masking coating squares, the substrate is deformed into shapes of different heights, in order to obtain a pattern of deformed masking coating squares,
in the step of metallizing the substrate, the metal deposit is made on the substrate at said grid lines, to form metallized grid lines,
in the step of eliminating the masking coating, the pattern of deformed masking coating squares is removed from the substrate, to form a pattern of deformed substrate squares free from masking coating, said free deformed squares being separated from each other by the metallized grid lines;
the measurement of the deformation ratio at break is made from the free deformed square of smallest width in which a short-circuit or metal bridge exists between two non-secant, opposite metallized grid lines of said square, the deformation ratio at break being calculated as follows:
(
Width
⁢
of
⁢
the
⁢
deformed
⁢
square
Intial
⁢
width
⁢
of
⁢
the
⁢
square
-
1
)
×
100
=
deformation
⁢
ratio
.

### Claim 4 (depends on 3)

The manufacturing method according to claim 3, characterized in that the deformation ration at break is higher than 100%, preferentially higher than 300%, more preferentially higher than 600%, even more preferentially higher than 1,000%.

### Claim 5 (depends on 1)

The manufacturing method according to claim 1, characterized in that, at the end of the deposition step and the curing step, the masking coating adheres to at least a first area of the substrate, whereas at the end of the metallization step and the elimination step, the metal deposit adheres to at least a second area and a third area of the substrate, separated from each other by said first area, no short-circuit or metal bridge connecting said second and third areas through said first area.

### Claim 6 (depends on 1)

The manufacturing method according to claim 1, characterized in that said organic matrix comprises at least one monomer and/or polymer chosen among: acrylic compounds, polyesters, vinyl compounds, styrenic compounds, polyamides, acrylate compounds, and/or cationic or anionic polymers.

### Claim 7 (depends on 1)

The manufacturing method according to claim 1, characterized in that said organic matrix comprises at least one or more of the following compounds: PETIA (pentaerythritol triacrylate), HDDA (hexanediol diacrylate), IBOA (isobornyl acrylate), TMPTA (trimethylolpropane triacrylate), TPGDA (tripropylene glycol diacrylate), HEMA (hydroxyethyl methacrylate), vinyl acetate and chloride copolymer, acrylic resin, polyvinyl alcohol, polyvinylpyrrolidone, polyurethane, styrene acrylic copolymer, aliphatic urethane acrylate, polyester acrylate, polyester, methyl methacrylate and ethyl acrylate copolymer, methyl methacrylate and butyl methacrylate copolymer, monofunctional acrylate monomer, and/or trifunctional acrylate monomer.

### Claim 8 (depends on 1)

The manufacturing method according to claim 1, characterized in that said organic matrix comprises at least a methyl methacrylate and ethyl acrylate copolymer, preferably forming between 10 and 20% of the total weight of the composition, a methyl methacrylate and butyl methacrylate copolymer, preferably forming between 10 and 20% of the total weight of the composition, and a polyamide, preferably forming between 5 and 25% of the total weight of the composition.

### Claim 9 (depends on 1)

The manufacturing method according to claim 1, characterized in that said organic matrix comprises at least polyurethane, preferably forming between 10 and 25% of the total weight of the formulation, a trifunctional acrylate monomer preferably forming between 5 and 20% of the total weight of the composition, and a monofunctional acrylate monomer preferably forming between 5 and 15% of the total weight of the composition.

### Claim 10 (depends on 1)

The manufacturing method according to claim 1, characterized in that the organic polymer matrix and/or the masking coating is alkali-sensitive.

### Claim 11 (depends on 1)

The manufacturing method according to claim 1, characterized in that the organic polymer matrix and/or the coating is soluble and/or dispersible in a liquid, for example an aqueous solution, having a pH equal to or greater than 9.

### Claim 12 (depends on 1)

The manufacturing method according to claim 1, characterized in that the organic polymer matrix forms between 20 and 80% of the total weight of the composition.

### Claim 13 (depends on 1)

The manufacturing method according to claim 1, characterized in that the composition further comprises one or more solvents, said solvent(s) forming between 15 and 80% of the total weight of the composition, preferably between 20 and 75% of the total weight of the composition, for example between 30 and 60% of the total weight of the composition.

### Claim 14 (depends on 13)

The manufacturing method according to claim 13, characterized in that said solvent(s) comprise at least one or more of the following compounds: isopropanol, butanol, methoxypropanol, ethyl acetate, butyl acetate, cyclohexane, 2-butoxyethanol acetate, 2-methoxy-1-methylethyl acetate, propylene carbonate, isopropyl myristate, diethylene glycol monoethyl ether acetate, glycerol, heavy naphtha, hexane, and/or methylcyclohexane.

### Claim 15 (depends on 13)

The manufacturing method according to claim 13, characterized in that said solvent(s) comprise at least water.

### Claim 16 (depends on 1)

The manufacturing method according to claim 1, characterized in that it is devoid of metal and/or electrically conductive particles.

### Claim 17 (depends on 1)

The manufacturing method according to claim 1, characterized in that the coating is electrically insulating and/or dielectric.

### Claim 18 (depends on 1)

The manufacturing method according to claim 1, characterized in that the composition further comprises at least one dispersed organic or inorganic solid, said solid being preferably formed by powder particles dispersed within other constituents of said composition.

### Claim 19 (depends on 18)

The manufacturing method according to claim 18, characterized in that said solid comprises a mineral filler, an organic filler and/or a fibrous filler.

### Claim 20 (depends on 18)

The manufacturing method according to claim 18, characterized in that said solid comprises at least one or more of the following compounds: silica, calcium carbonate, barium sulphate, aluminium hydroxide, and/or a wax.

### Claim 21 (depends on 18)

The manufacturing method according to claim 18, characterized in that said solid forms between 0.5% and 50%, preferably between 1% and 40%, more preferably between 1.5% and 30%, even more preferably between 2% and 20% of the total weight of the composition.

### Claim 22 (depends on 1)

The manufacturing method according to claim 1, characterized in that the composition comprises at least one radical, cationic or anionic photo-initiator, capable of cross-linking part at least of the polymer matrix when the composition is subjected to ultra-violets.

### Claim 23 (depends on 22)

The coating manufacturing method according to claim 22, characterized in that the photo-initiator agent forms between 0.5% and 15%, preferably between 1% and 10%, more preferentially between 1 and 7%, of the total weight of the composition.

### Claim 24 (depends on 22)

The coating manufacturing method according to claim 22, characterized in that the photo-initiator agent comprises at least one of the following compounds: benzophenone, 1-hydroxy-cyclohexyl-phenyl-ketone, dimethylhydroxyacetophenone, diphenyl (2,4,6-trimethylbenzoyl) phosphine oxide, 1-chloro-4-propoxythioxanthone, 2,2-dimethoxy-1,2-phenylacetophenone.

### Claim 25 (depends on 1)

The manufacturing method according to claim 1, characterized in that the composition comprises at least one or more of the following additional compounds: rheology agent, wetting agent, defoamer, dispersant, surfactant, stabiliser, colouring agent, amine synergist.

### Claim 26 (depends on 25)

The manufacturing method according to claim 25, characterized in that the additional compound(s) form between 0.01% and 10% of the total weight of the composition.

### Claim 27 (depends on 26)

The manufacturing method according to claim 26, characterized in that the masking coating has a glass transition temperature and/or melting temperature below the glass transition temperature of the substrate.

### Claim 28 (depends on 1)

The manufacturing method according to claim 1, characterized in that said deposition step is carried out at least in part by screen printing and/or direct printing.

### Claim 29 (depends on 1)

The manufacturing method according to claim 1, characterized in that the masking coating has a thickness of between 1 μm and 20 μm, preferably between 3 μm and 10 μm.

### Claim 30 (depends on 1)

The manufacturing method according to claim 1, characterized in that the masking coating has at least a first portion and a second portion, distinct from each other, the first portion thickness being different from the second portion thickness.

### Claim 31 (depends on 1)

The manufacturing method according to claim 1, characterized in that, in said thermoforming step, the substrate surface so covered with the masking coating is deformed.

### Claim 32 (depends on 1)

The manufacturing method according to claim 1, characterized in that the thermoforming step is carried out before the metallization step.

### Claim 33 (depends on 1)

The method according to claim 1, characterized in that the thermoforming step is carried out after the metallization step.

### Claim 34 (depends on 1)

The manufacturing method according to claim 1, characterized in that the thermoforming step is carried out before the elimination step.

### Claim 35 (depends on 1)

The method according to claim 1, characterized in that the metal deposit is made of solid metal.

### Claim 36 (depends on 1)

The method according to claim 1, characterized in that the metal deposit has, at the end of the metallization step, a thickness of between 10 nm and 5 μm, preferably between 10 nm and 1 μm, and still preferably between 10 nm and 500 nm.