# US 2025/0171924 A1 · Aluminum bonding wire coated by photo-curing polymer, preparation method, and application therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0171924 A1
- Document ID: US20250171924A1
- Status: Published application
- Kind: A1
- Application number: 18/957,464
- Filed: 2024-11-22
- Published: 2025-05-29
- Earliest claimed: 2023-11-27
- Assignees: China Academy of Machinery Zhengzhou Research Institute of Mechanical Engineering Co., Ltd.
- Applicants: China Academy of Machinery Zhengzhou Research Institute of Mechanical Engineering Co., Ltd.
- Inventors: Yafang CHENG; Sujuan ZHONG; Jie LIU; Peng GUO; Yuanyuan DONG; Peiyan LI
- Web page: https://patentgrep.com/patent/US20250171924A1

## CPC

- C25D 11/24: Chemical after-treatment
- C09D 5/08: Anti-corrosive paints
- C25D 11/045: {for forming AAO templates}
- H10W 72/5524: {comprising aluminium [Al]}
- H10W 72/555: {of outermost layers of multilayered bond wires, e.g. material of a coating}
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Provided are an aluminum bonding wire coated by a photo-curing polymer, a preparation method, and an application therefor. The aluminum bonding wire coated by the photo-curing polymer includes an aluminum-based material and an anodic aluminum oxide layer coating outside the aluminum-based material, wherein the anodic aluminum oxide layer includes a plurality of closely arrayed alumina micropores, and a photo-curing polymer layer is attached to the interiors of the alumina micropores and the surface of the alumina microporous layer.

## Claims

### Claim 1

An aluminum bonding wire coated by a photo-curing polymer, comprising an aluminum-based material and an anodic aluminum oxide layer coating outside the aluminum-based material, wherein the anodic aluminum oxide layer comprises a plurality of closely arrayed alumina micropores, and a photo-curing polymer layer is attached to interiors of the alumina micropores and surfaces of the alumina micropores.

### Claim 2 (depends on 1)

The aluminum bonding wire coated by the photo-curing polymer according to claim 1, wherein the photo-curing polymer layer is made of following components according to part by mass:
base polymers 80˜100 parts, photo-curing agents 20˜50 parts, photo-radical initiator 0.2˜0.5 parts, and antioxidant 0.5˜1 part.

### Claim 3 (depends on 2)

The aluminum bonding wire coated by the photo-curing polymer according to claim 2, wherein the base polymers comprise: at least one of a photo-curing acrylic prepolymer system, a photo-curing silicone prepolymer system, and a photo-curing carbamate prepolymer system.

### Claim 4 (depends on 1)

The aluminum bonding wire coated by the photo-curing polymer according to claim 1, wherein a thickness of the photo-curing polymer layer is 2.5˜10 μm.

### Claim 5 (depends on 1)

The aluminum bonding wire coated by the photo-curing polymer according to claim 1, wherein the aluminum-based material comprises: a pure aluminum wire and/or an aluminum alloy wire.

### Claim 6 (depends on 1)

A preparation method for the aluminum bonding wire coated by the photo-curing polymer according to claim 1, comprising following steps:
anodizing the aluminum-based material in an electrolyte, so that the anodic aluminum oxide layer comprising the plurality of closely arrayed alumina micropores is formed on an outer wall of the aluminum-based material; and
performing photo curing after putting a photo-curing material liquid into the alumina micropores.

### Claim 7 (depends on 6)

The preparation method for the aluminum bonding wire coated by the photo-curing polymer according to claim 6, wherein a voltage of the anodizing is 50˜100 VDC.

### Claim 8 (depends on 6)

The preparation method for the aluminum bonding wire coated by the photo-curing polymer according to claim 6, wherein a pH of the electrolyte is <5.

### Claim 9 (depends on 6)

The preparation method for the aluminum bonding wire coated by the photo-curing polymer according to claim 6, wherein a wavelength of a light source for the photo curing is 360˜450 nm.

### Claim 10 (depends on 1)

A lead wire material for an electronic packaging, comprising the aluminum bonding wire coated by the photo-curing polymer according to claim 1.

### Claim 11 (depends on 1)

The aluminum bonding wire coated by the photo-curing polymer according to claim 1, wherein a thickness of the anodic aluminum oxide layer is 2˜9 μm.

### Claim 12 (depends on 1)

The aluminum bonding wire coated by the photo-curing polymer according to claim 1, wherein a diameter of the alumina micropores is 80˜200 nm.

### Claim 13 (depends on 1)

The aluminum bonding wire coated by the photo-curing polymer according to claim 1, wherein a wire diameter of the aluminum-based material is 100˜500 μm.

### Claim 14 (depends on 6)

The preparation method for the aluminum bonding wire coated by the photo-curing polymer according to claim 6, wherein a duration of the anodizing is 1˜3 min.

### Claim 15 (depends on 6)

The preparation method for the aluminum bonding wire coated by the photo-curing polymer according to claim 6, wherein a temperature of the electrolyte is 10˜50° C.