Aircraft fluid resistant sealant for use on aircraft parts
AssigneeThe Patent Well LLC
InventorsJeff Busby, Michael Dry, Kent Boomer, Matt Boyd, Chad Knight, Peter Sibello
Life of this patent
Estimating the term…
Loading patent…
AssigneeThe Patent Well LLC
InventorsJeff Busby, Michael Dry, Kent Boomer, Matt Boyd, Chad Knight, Peter Sibello
Estimating the term…
A number of sealants are provided that are resistant to degradation by aircraft fluids. In some embodiments, the sealants are resistant to degradation by Jet A fluid and at least one of the three types of hydraulic fluids typically used in aircraft. These embodiments are also typically cure in place from a two-part polyurethane or polyurea mix, with cure to a visibly clear coating. In some embodiments, they may be sprayed on an aircraft surface or applied by hand (brush or injectable). In other of these embodiments, the sealants comprise, at least in part, a cured, soft, tacky polyurethane gel that is resistant to at least one of a synthetic hydrocarbon based or mineral oil based hydraulic fluid.
An assembly for engagement with a spray gun, the assembly comprising:
An assembly for use with a spray gun, the spray gun for applying a sealant coating, the assembly comprising:
An assembly for use with a spray gun, the spray gun for applying a sealant coating, the assembly comprising:
A method of using an assembly having first compartment and a second compartment, the first compartment containing a first polymer component, the second compartment containing a second polymer component, the compartments dimensioned to engage a spray gun, and a mixing nozzle fluidly engaged to the first and second compartments, the mixing nozzle configured to receive and when the assembly is engaged with the spray gun and the spray gun is energized, combine the first and second components to form an uncured sealant mix and emit the uncured sealant mix, under pressure, from a tip of the mixing nozzle at a removed end thereof capable of curing to form a visibly clear, cured in place, sealant coat on an aircraft workpiece, the clear sealant coat free of VOC's, with a gel time 30 minutes or less and is Flame Retardant under 14 CFR 25.853a, Appendix F, Part 1(A)(1)(ii) (12 second vertical burn), the method including:
A method of using an assembly having first compartment and a second compartment, the first compartment containing a first polymer component, the second compartment containing a second polymer component, the compartments dimensioned to engage a spray gun, and a mixing nozzle fluidly engaged to the first and second compartments, the mixing nozzle configured to receive and when the assembly is engaged with the spray gun and the spray gun is energized, combine the first and second components to form an uncured sealant mix and emit the uncured sealant mix, under pressure, from a tip of the mixing nozzle at a removed end thereof capable of curing to form a visibly clear, cured in place, sealant coat on an aircraft workpiece, the clear sealant coat free of VOC's, with a gel time 30 minutes or less and is Flame Retardant under 14 CFR 25.853a, Appendix F, Part 1(A)(1)(ii) (12 second vertical burn), the method including:
Dependencies are inferred from the claim text.