# US 2025/0170637 A1 · Soluble core for high-pressure casting and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0170637 A1
- Document ID: US20250170637A1
- Status: Published application
- Kind: A1
- Application number: 18/842,701
- Filed: 2023-02-28
- Published: 2025-05-29
- Earliest claimed: 2022-03-03
- Inventors: Kyoko Hirokawa; Jun Su Kim
- Web page: https://patentgrep.com/patent/US20250170637A1

## CPC

- B22C 9/105: {Salt cores}
- B22C 1/00: Compositions of refractory mould or core materials; Grain structures thereof (refractory materials in general C04B35/00); Chemical or physical features in the formation or manufacture of moulds
- B22D 21/007: {with low melting point, e.g. Al 659 degrees C, Mg 650 degrees C}
- B22D 29/003: {using heat}
- B22C: FOUNDRY MOULDING (moulding refractory materials in general B28B)
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)

## Abstract

According to the method for manufacturing a soluble core for high pressure casting, the method for manufacturing a core by dispersing a heat-resistant hard ceramic powder in a water-soluble chemical salt having a melting point 140° C. to 260° C. lower than a melting point of a cast metal and a heat capacity of 90 J/(mol·K) or more is a very useful technology that can easily manufacture a core for high pressure casting of metals such as aluminum and magnesium, and a method for extracting a core from casting can also be simply performed by heating and extracting the core at a temperature equal to or lower than the melting point of the cast metal, and since the core material can be recycled, it is very advantageous in terms of productivity and economy.

## Claims

### Claim 1

A method for manufacturing a soluble core for high pressure casting, comprising:
a step of manufacturing a water-soluble chemical salt mixture having a melting temperature of 390° C. to 520° C.;
a step of uniformly dispersing and mixing a heat-resistant hard powder into the above water-soluble chemical salt mixture to manufacture a molten chemical salt having a heat capacity of 90 J/(mol·K) or more; and
a step of injecting the manufactured molten chemical salt into a core mold and solidifying the molten chemical salt to manufacture a core.

### Claim 2 (depends on 1)

The method for manufacturing a soluble core for high pressure casting according to claim 1,
wherein the water-soluble chemical salt mixture includes any one or more selected from the group consisting of a chloride-based chemical salt, a carbide-based chemical salt, and a sulfide-based chemical salt.

### Claim 3 (depends on 2)

The method for manufacturing a soluble core for high pressure casting according to claim 2,
wherein the chloride-based chemical salt includes any one or more selected from the group consisting of NaCl, KCl, MnCl2, CaCl, MgCl2, and LiCl,
the carbide-based chemical salt includes any one or more selected from the group consisting of K2CO3, Li2CO3 and Na2CO3, and
the sulfide-based chemical salt includes any one or more selected from the group consisting of K2SO4, Na2SO4, and Li2SO4.

### Claim 4 (depends on 2)

The method for manufacturing a soluble core for high pressure casting according to claim 2,
wherein the water-soluble chemical salt mixture is selected from the group consisting of water-soluble chemical salt mixtures of KCl:MnCl2:NaCl in a ratio of 45.5:33.5:20, CaCl2:KCl:MgCl2:NaCl in a ratio of 41.6:2.2:8.8:47.4, CrCl2:KCl in a ratio of 60:40, K2CO3:Li2CO3:Na2CO3 in a ratio of 25:43.5:31.5, K2CO3:MgCO3 in a ratio of 55:45, K2SO4:Li2SO4 in a ratio of 18:82, K2SO4:Na2SO4 in a ratio of 75:25, LiCl:Li2SO4:Li2CO3 in a ratio of 52.9:27.2:19.8, LiCl:Li2SO4:NaCl in a ratio of 54.8:29:16.1, LiCl:Li2CO3:Li2SO4 in a ratio of 52.9:19.8:27.2, and CaSO4:LiCl in a ratio of 14:86, in terms of a mixing ratio (Mol %).

### Claim 5 (depends on 1)

The method for manufacturing a soluble core for high pressure casting according to claim 1,
wherein the heat-resistant hard powder includes any one or more selected from the group consisting of TiO2, Al2O3, and ZrSiO4.

### Claim 6 (depends on 1)

The method for manufacturing a soluble core for high pressure casting according to claim 1,
wherein the water-soluble chemical salt mixture has a melting point 140° C. to 260° C. lower than a melting point of a cast metal.

### Claim 7 (depends on 1)

The method for manufacturing a soluble core for high pressure casting according to claim 1,
wherein a cast metal is an aluminum alloy or a magnesium alloy.

### Claim 8 (depends on 1)

The method for manufacturing a soluble core for high pressure casting according to claim 1, further comprising:
a step of installing the manufactured core in a high pressure casting mold, performing high pressure casting of a molten metal, and then performing heating to a temperature equal to or less than the melting point of the cast alloy to extract the molten core.

### Claim 9

A soluble core for high pressure casting formed of a molten chemical salt having a heat capacity of 90 J/(mol·K) or more obtained by uniformly dispersing and mixing a heat-resistant hard powder into a water-soluble chemical salt mixture having a melting point 140° C. to 260° C. lower than a melting point of a cast metal, which includes any one or more selected from the group consisting of a chloride-based chemical salt, a carbide-based chemical salt, and a sulfide-based chemical salt.

### Claim 10 (depends on 9)

The soluble core for high pressure casting according to claim 9,
wherein the chloride-based chemical salt includes any one or more selected from the group consisting of NaCl, KCl, MnCl2, CaCl, MgCl2, and LiCl,
the carbide-based chemical salt includes any one or more selected from the group consisting of K2CO3, Li2CO3 and Na2CO3, and
the sulfide-based chemical salt includes any one or more selected from the group consisting of K2SO4, Na2SO4, and Li2SO4.

### Claim 11 (depends on 9)

The soluble core for high pressure casting according to claim 9,
wherein the water-soluble chemical salt is selected from the group consisting of water-soluble chemical salt mixtures of KCl:MnCl2:NaCl in a ratio of 45.5:33.5:20, CaCl2:KCl:MgCl2:NaCl in a ratio of 41.6:2.2:8.8:47.4, CrCl2:KCl in a ratio of 60:40, K2CO3:Li2CO3:Na2CO3 in a ratio of 25:43.5:31.5, K2CO3:MgCO3 in a ratio of 55:45, K2SO4:Li2SO4 in a ratio of 18:82, K2SO4:Na2SO4 in a ratio of 75:25, LiCl:Li2SO4:Li2CO3 in a ratio of 52.9:27.2:19.8, LiCl:Li2SO4:NaCl in a ratio of 54.8:29:16.1, LiCl:Li2CO3:Li2SO4 in a ratio of 52.9:19.8:27.2, and CaSO4:LiCl in a ratio of 14:86, in terms of a mixing ratio (Mol %).

### Claim 12 (depends on 9)

A method for extracting a soluble core for high pressure casting,
wherein the soluble core for high pressure casting according to claim 9 is heated to a temperature equal to or less than the melting point of a product after high pressure casting, melted, extracted, and then washed with water.