# US 2025/0169264 A1 · Stretchable otft element, skin attachable temperature sensor and the manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0169264 A1
- Document ID: US20250169264A1
- Status: Published application
- Kind: A1
- Application number: 18/939,784
- Filed: 2024-11-07
- Published: 2025-05-22
- Earliest claimed: 2023-11-21
- Assignees: University-Industry Cooperation Group of Kyung Hee University
- Applicants: University-Industry Cooperation Group of Kyung Hee University
- Inventors: Jin Young OH; Min Woo JEONG; Jun Su KIM
- Web page: https://patentgrep.com/patent/US20250169264A1

## CPC

- H10K 10/466: {Lateral bottom-gate IGFETs comprising only a single gate}
- H10K 71/12: using liquid deposition, e.g. spin coating
- H10K 71/164: {using vacuum deposition}
- H10K 71/611: {using printing deposition, e.g. ink jet printing}
- H10K 85/113: {Heteroaromatic compounds comprising sulfur or selene, e.g. polythiophene}
- H10K 85/20: Carbon compounds, e.g. carbon nanotubes or fullerenes
- H10K 85/6576: {comprising only sulfur in the heteroaromatic polycondensed ring system, e.g. benzothiophene}
- G01K 7/015: {using microstructures, e.g. made of silicon}
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES
- G01K: MEASURING TEMPERATURE; MEASURING QUANTITY OF HEAT; THERMALLY-SENSITIVE ELEMENTS NOT OTHERWISE PROVIDED FOR (radiation pyrometry G01J5/00)

## Abstract

Provided is a stretchable organic thin film field effect transistor (OTFT) element with high sensitivity and low power characteristic as a temperature sensor element that resolved instability caused by charge trap density induced as strain or heat in a sub-threshold region.

## Claims

### Claim 1

A stretchable organic thin film field effect transistor (OTFT) element comprising:
a gate electrode;
a dielectric layer stacked with elastomer on the gate electrode;
an active layer stacked on the dielectric layer; and
a source electrode and a drain electrode formed to be spaced part from each other on the active layer,
wherein the active layer is formed as an elastomer matrix organic semiconductor nanofiber blend film in which organic semiconductor nanofiber is mixed within an elastomer matrix.

### Claim 2 (depends on 1)

The stretchable OTFT element of claim 1, wherein an organic semiconductor that forms the organic semiconductor nanofiber is DPPT-TT that is represented by Formula 1 below.

### Claim 3 (depends on 1)

The stretchable OTFT element of claim 1, wherein the elastomer is styrene-ethylene-butylene-styrene (SEBS) organic elastomer that is represented by Formula 2 below.

### Claim 4 (depends on 3)

The stretchable OTFT element of claim 3, wherein the SEBS has a composition ratio of 18:82 to 20:80 for (x+o) to (m+n).

### Claim 5 (depends on 1)

The stretchable OTFT element of claim 1, wherein the elastomer matrix organic semiconductor nanofiber blend film is manufactured by dissolving DPPT-TT represented by Formula 1 below and SEBS represented by Formula 2 below in a material of Formula 3 below at a concentration of 0.6 to 0.8% by weight at a weight ratio of 1 to 3:7 to 9.

### Claim 6 (depends on 1)

The stretchable OTFT element of claim 1, further comprising:
a substrate on which the gate electrode is formed,
wherein the substrate is manufactured by mixing a material of Formula 2 below with a material of Formula 4 below at a centration of 90 to 110 mg/mL and then performing spin coating on a rigid substrate.

### Claim 7 (depends on 1)

The stretchable OTFT element of claim 1, wherein the dielectric layer is a SEBS matrix manufactured by mixing a material of Formula 2 below with a material of Formula 4 below at a concentration of 50 to 70 mg/mL and then performing spin coating on a rigid substrate.

### Claim 8 (depends on 1)

The stretchable OTFT element of claim 1, further comprising:
a substrate on which the gate electrode is formed,
wherein the gate electrode and the source electrode and the drain electrode are formed on the substrate and the active layer, respectively, by a transfer printing method that uses metallization of a thermally evaporated metal conductor.

### Claim 9

A skin attachable temperature sensor comprising:
a substrate formed of elastomer;
a first electrode layer formed on the substrate by including at least one gate electrode;
a dielectric layer stacked with the elastomer on the substrate and the first electrode layer;
an active layer stacked on the dielectric layer;
a second electrode layer stacked on the active layer by including at least one source electrode and drain electrode; and
a capsule layer configured to seal the top of the second electrode layer,
wherein the active layer is formed as an elastomer matrix organic semiconductor nanofiber blend film in which organic semiconductor nanofiber is mixed within an elastomer matrix.

### Claim 10 (depends on 9)

The skin attachable temperature sensor of claim 9, wherein an organic semiconductor that forms the organic semiconductor nanofiber is DPPT-TT that is represented by Formula 1 below.

### Claim 11 (depends on 9)

The skin attachable temperature sensor of claim 9, the elastomer is styrene-ethylene-butylene-styrene (SEBS) organic elastomer that is represented by Formula 2 below.

### Claim 12 (depends on 11)

The skin attachable temperature sensor of claim 11, wherein the SEBS has a composition ratio of 18:82 to 20:80 for (x+o) to (m+n).

### Claim 13 (depends on 9)

The skin attachable temperature sensor of claim 9, wherein the elastomer matrix organic semiconductor nanofiber blend film is manufactured by dissolving DPPT-TT represented by Formula 1 below and SEBS represented by Formula 2 in a material of Formula 3 below at a concentration of 0.6 to 0.8% by weight at a weight ratio of 1 to 3:7 to 9.

### Claim 14 (depends on 9)

The skin attachable temperature sensor of claim 9, wherein the substrate is manufactured by mixing a material of Formula 2 below with a material of Formula 4 below at a centration of 90 to 110 mg/mL and then performing spin coating on a rigid substrate.

### Claim 15 (depends on 9)

The skin attachable temperature sensor of claim 9, wherein the dielectric layer is a SEBS matrix manufactured by mixing a material of Formula 2 below with a material of Formula 4 below at a concentration of 50 to 70 mg/mL and then performing spin coating on a rigid substrate.

### Claim 16 (depends on 9)

The skin attachable temperature sensor of claim 9, wherein the first electrode layer and the second electrode layer are formed on the substrate and the active layer, respectively, by a transfer printing method that uses metallization of a thermally evaporated metal conductor.

### Claim 17

A method of manufacturing a skin attachable temperature sensor, the method comprising:
a substrate, dielectric layer, and active layer manufacturing operation of simultaneously or sequentially manufacturing a substrate, a dielectric layer, and an active layer on each of separated wafers or glass substrates;
a first electrode layer forming operation of forming stretchable at least one gate electrode on the substrate through thermal evaporation under vacuum using a patterning mask;
a second electrode layer forming operation of forming at least one source electrode and drain electrode on the active layer; and
a dielectric layer and active layer transferring operation of transferring the dielectric layer on the substrate on which the first electrode layer is formed and transferring the active layer on the dielectric layer such that the second electrode layer is present on the top,
wherein, in the substrate, dielectric layer, and active layer manufacturing operation, the active layer is manufactured by mixing organic semiconductor nanofiber of Formula 1 below and elastomer of Formula 2 below in a solvent that contains a material of Formula 3 below.

### Claim 18 (depends on 17)

The method of claim 17, wherein, in the substrate, dielectric layer, and active layer manufacturing operation, the substrate is manufactured as a stretchable substrate by mixing the material of Formula 2 above with a material of Formula 4 below at a concentration of 90 to 110 mg/mL and then performing spin coating on a rigid substrate.

### Claim 19 (depends on 17)

The method of claim 17, wherein, in the substrate, dielectric layer, and active layer manufacturing operation, the dielectric layer is formed as a SEBS matrix by mixing the material of Formula 2 above with a material of Formula 4 below at a concentration of 50 to 70 mg/mL and then performing spin coating on a rigid substrate.

### Claim 20 (depends on 17)

The method of claim 17, wherein, in the substrate, dielectric layer, and active layer manufacturing operation, the active layer is manufactured as a DPPT-TT: SEBS blend film in which an organic semiconductor nanofiber film is formed as the active layer by dissolving DPPT-TT represented by Formula 1 above and SEBS represented by Formula 2 above with the material of Formula 3 above at a concentration of 0.6 to 0.8% by weight at a weight ratio of 1 to 3:7 to 9 for the total weight on a rigid substrate and then generating a filtration solution and by spin-coating and then annealing the filtration solution.