# US 2025/0169230 A1 · Quantum Dot Patterned Film and Preparation Method Thereof, Electron Transport Layer, and Quantum Dot Electroluminescent Device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0169230 A1
- Document ID: US20250169230A1
- Status: Published application
- Kind: A1
- Application number: 18/943,666
- Filed: 2024-11-11
- Published: 2025-05-22
- Earliest claimed: 2023-11-21
- Assignees: Leyard Optoelectronic Co., Ltd.
- Applicants: Leyard Optoelectronic Co., Ltd.
- Inventors: Jun LI; Xiaoyu YANG; Li MA; Changjun LU
- Web page: https://patentgrep.com/patent/US20250169230A1

## CPC

- G03F 7/0002: {Lithographic processes using patterning methods other than those involving the exposure to radiation, e.g. by stamping}
- H10H 20/816: having carrier transport control structures, e.g. highly-doped semiconductor layers or current-blocking structures
- B82Y 20/00: Nanooptics, e.g. quantum optics or photonic crystals
- B82Y 40/00: Manufacture or treatment of nanostructures
- H05B 33/145: {Arrangements of the electroluminescent material}
- H10K 50/00: Organic light-emitting devices (integrated devices or assemblies of multiple devices H10K59/00, H10K65/00; organic semiconductor lasers H01S5/36)
- H10K 50/115: comprising active inorganic nanostructures, e.g. luminescent quantum dots
- H10K 50/16: Electron transporting layers
- H10K 71/00: Manufacture or treatment specially adapted for the organic devices covered by this subclass
- H10K 71/20: Changing the shape of the active layer in the devices, e.g. patterning
- H10K 71/40: Thermal treatment, e.g. annealing in the presence of a solvent vapour
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- H05B: ELECTRIC HEATING; ELECTRIC LIGHT SOURCES NOT OTHERWISE PROVIDED FOR; CIRCUIT ARRANGEMENTS FOR ELECTRIC LIGHT SOURCES, IN GENERAL
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES

## Abstract

The present disclosure provides quantum dot patterned film and preparation method thereof, electron transport layer, and quantum dot electroluminescent device. The preparation method includes: S1, attaching a quantum dot precursor solution to a functional transport layer substrate to obtain a wet film having a quantum dot layer; S2, attaching a photosensitive ligand to a patterned surface of a prefabricated nano stamp to obtain a photosensitive ligand stamp having a ligand layer; S3, contacting the quantum dot layer of the wet film with the ligand layer of the photosensitive ligand stamp, performing imprinting treatment, so as to obtain a ligand exchange quantum dot film; and S4, performing on the ligand exchange quantum dot film to obtain the quantum dot patterned film. The preparation method solves the problems in the related art that the preparation process of the quantum dot patterned film is complex and the production yield is relatively low.

## Claims

### Claim 1

A preparation method of a quantum dot patterned film, comprising:
S1, attaching a quantum dot precursor solution to a functional transport layer substrate to obtain a wet film having a quantum dot layer;
S2, attaching a photosensitive ligand to a patterned surface of a prefabricated nano stamp to obtain a photosensitive ligand stamp having a ligand layer;
S3, contacting the quantum dot layer of the wet film with the ligand layer of the photosensitive ligand stamp, performing imprinting treatment, and removing the stamp after completing the imprinting treatment, so as to obtain a ligand exchange quantum dot film; and
S4, sequentially performing exposure treatment and development treatment on the ligand exchange quantum dot film to obtain the quantum dot patterned film.

### Claim 2 (depends on 1)

The preparation method according to claim 1, wherein the pressure of the imprinting treatment is 0 MPa-100 MPa, and/or the time of the imprinting treatment is 1 min-20 min.

### Claim 3 (depends on 1)

The preparation method according to claim 1, wherein the preparation method further comprises: performing first annealing treatment on a system subjected to the imprinting treatment during or after the imprinting treatment process, and/or the temperature of the first annealing treatment being 50° C.-300° C., and/or the time of the first annealing treatment being 1 min-5 min.

### Claim 4 (depends on 1)

The preparation method according to claim 1, wherein the preparation method further comprises:
a process of performing modification treatment on the prefabricated nano stamp by using an ultraviolet-ozone cleaning process;
wherein the modification treatment is performed at a power of 55 W-100 W by using ultraviolet wavelengths of 254 nm and 185 nm, and/or the time of the modification treatment is 10 min-30 min;
and/or the material of the prefabricated nano stamp is selected from any one or more of Polydimethylsiloxane (PDMS), Polymethyl Methacrylate (PMMA), and sapphire Al2O3.

### Claim 5 (depends on 1)

The preparation method according to claim 1, wherein the thickness of the ligand layer is 5 nm-100 nm, and/or a thickness ratio of the quantum dot layer to the ligand layer is 10-80:5-100; and/or the material of the functional transport layer substrate is selected from any one or more of transparent conductive glass, an oxide material, and an organic polymer material;
and/or quantum dots in the quantum dot precursor solution are selected from any one or more of group II-VI quantum dots, group III-V quantum dots, and perovskite quantum dots.

### Claim 6 (depends on 1)

The preparation method according to claim 1, wherein the preparation method further comprises: performing second annealing treatment on the ligand exchange quantum dot film between the exposure treatment and the development treatment, and/or the temperature of the second annealing treatment being 100° C.-150° C., and/or the time of the second annealing treatment being 1 min-10 min; and/or performing the exposure treatment by using ultraviolet light with a wavelength of less than 480 nm, and/or the time of the exposure treatment being 10 min-30 min.

### Claim 7 (depends on 1)

The preparation method according to claim 1, wherein the photosensitive ligand is a ligand compound that generates free radicals at an ultraviolet wavelength of less than 380 nm, and the photosensitive ligand is a benzophenone-based photosensitive molecular compound and/or a photogenerated nitrene molecular compound.

### Claim 8 (depends on 1)

A quantum dot patterned film, wherein the quantum dot patterned film is prepared by the preparation method according to claim 1.

### Claim 9 (depends on 8)

An electron transport layer, comprising a quantum dot film, wherein the quantum dot film is the quantum dot patterned film according to claim 8.

### Claim 10 (depends on 9)

A quantum dot electroluminescent device, comprising an electron transport layer, wherein the electron transport layer is the electron transport layer according to claim 9.

### Claim 11 (depends on 5)

The preparation method according to claim 5, wherein the transparent conductive glass is selected from any one or more of Indium Tin Oxide, Fluorine-doped Tin Oxide and Indium Zinc Oxide.

### Claim 12 (depends on 5)

The preparation method according to claim 5, wherein the oxide material is selected from any one or more of Al2O3, TiO2, SnO2, and ZnO.

### Claim 13 (depends on 5)

The preparation method according to claim 5, wherein the organic polymer material is preferably PMMA and/or PDMS.

### Claim 14 (depends on 5)

The preparation method according to claim 5, wherein the quantum dots are selected from any one or more of CdS, CdSe, ZnS, ZnSe, InP, CsPbI3 and CsPbBr3.

### Claim 15 (depends on 1)

The preparation method according to claim 1, wherein the preparation method further comprises: washing the quantum dot film, the washing process is guaranteed to be performed at room temperature.

### Claim 16 (depends on 15)

The preparation method according to claim 15, wherein the washing manner is to spin coat the quantum dot film at 3000 rpm/s-10000 rpm/s.