# US 2025/0169125 A1 · High electron mobility transistor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0169125 A1
- Document ID: US20250169125A1
- Status: Published application
- Kind: A1
- Application number: 18/923,571
- Filed: 2024-10-22
- Published: 2025-05-22
- Earliest claimed: 2023-11-20
- Assignees: Hiper Semiconductor Inc.
- Applicants: HiPer Semiconductor Inc.
- Inventors: PO-JUNG LIN; WEI-CHEN YANG
- Web page: https://patentgrep.com/patent/US20250169125A1

## CPC

- H10D 62/106: {having supplementary regions doped oppositely to or in rectifying contact with regions of the semiconductor bodies, e.g. guard rings with PN or Schottky junctions}
- H10D 62/854: further characterised by the dopants
- H10D 30/475: {having wider bandgap layer formed on top of lower bandgap active layer, e.g. undoped barrier HEMTs such as i-AlGaN/GaN HEMTs}
- H10D 62/357: {of FETs}
- H10D 62/60: Impurity distributions or concentrations
- H10D 62/8503: {Nitride Group III-V materials, e.g. AlN or GaN}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A high electron mobility transistor includes a substrate, a nucleation layer, a buffer layer, a channel layer, and a barrier layer. The buffer layer includes a first buffer region, a second buffer region and a third buffer region. The first buffer region includes a first III-nitride stacked layer disposed on the nucleation layer and a second III-nitride stacked layer disposed on the first III-nitride stacked layer. The second buffer region is doped with carbon and iron. The third buffer region is doped with carbon and iron and has a carbon concentration greater than an iron concentration of the third buffer region. The second III-nitride stacked layer is doped with carbon and iron and has a carbon concentration greater than an iron concentration of the second III-nitride stacked layer.

## Claims

### Claim 1

A high electron mobility transistor, comprising:
a substrate;
a nucleation layer disposed on the substrate;
a buffer layer, comprising:
a first buffer region comprising a first III-nitride stacked layer and a second III-nitride stacked layer, wherein the first III-nitride stacked layer is disposed on the nucleation layer, and the second III-nitride stacked layer is disposed on the first III-nitride stacked layer;
a second buffer region disposed on the first buffer region, wherein the second buffer region is doped with carbon (C) and iron (Fe); and
a third buffer region disposed on the second buffer region, wherein the third buffer region is doped with carbon (C) and iron (Fe);
a channel layer disposed on the buffer layer; and
a barrier layer disposed on the channel layer;
wherein the third buffer region is located between the second buffer region and the channel layer; a carbon (C) concentration of the third buffer region is greater than an iron (Fe) concentration of the third buffer region; the iron (Fe) concentration of the third buffer region gradually decreases in a direction from the second buffer region to the channel layer; an average Al composition of the first III-nitride stacked layer is greater than an average Al composition of the second III-nitride stacked layer;
wherein the second III-nitride stacked layer is doped with carbon (C) and iron (Fe); a carbon (C) concentration of the second III-nitride stacked layer is greater than an iron (Fe) concentration of the second III-nitride stacked layer.

### Claim 2 (depends on 1)

The high electron mobility transistor as claimed in claim 1, wherein the second buffer region comprises a first buffer sub-layer; a carbon (C) concentration of the first buffer sub-layer is greater than an iron (Fe) concentration of the first buffer sub-layer.

### Claim 3 (depends on 1)

The high electron mobility transistor as claimed in claim 1, wherein the second buffer region comprises at least one second buffer sub-layer and at least one third buffer sub-layer that are stacked; a carbon (C) concentration of the at least one second buffer sub-layer is greater than an iron (Fe) concentration of the at least one second buffer sub-layer; an iron (Fe) concentration of the at least one third buffer sub-layer is greater than a carbon (C) concentration of the at least one third buffer sub-layer.

### Claim 4 (depends on 3)

The high electron mobility transistor as claimed in claim 3, wherein a thickness of the at least one second buffer sub-layer is greater than a thickness of the at least one third buffer sub-layer.

### Claim 5 (depends on 3)

The high electron mobility transistor as claimed in claim 3, wherein the carbon (C) concentration of the at least one third buffer sub-layer is less than 1E17 cm−3; the iron (Fe) concentration of the at least one third buffer sub-layer is greater than 1E17 cm−3.

### Claim 6 (depends on 3)

The high electron mobility transistor as claimed in claim 3, wherein the carbon (C) concentration of the at least one second buffer sub-layer is greater than 5E18 cm−3.

### Claim 7 (depends on 1)

The high electron mobility transistor as claimed in claim 1, wherein the second III-nitride stacked layer is located between the first III-nitride stacked layer and the second buffer region; the average Al composition of the first III-nitride stacked layer is greater than 25%; the average Al composition of the second III-nitride stacked layer is less than 25%.

### Claim 8 (depends on 1)

The high electron mobility transistor as claimed in claim 1, wherein the first III-nitride stacked layer and the second III-nitride stacked layer respectively comprise at least one III-nitride semiconductor layer made of AlXGa1-XN (0≤X≤1).

### Claim 9 (depends on 1)

The high electron mobility transistor as claimed in claim 1, wherein the channel layer is doped with iron (Fe); an iron (Fe) concentration of the channel layer decreases in a direction away from the buffer layer.

### Claim 10 (depends on 1)

The high electron mobility transistor as claimed in claim 1, wherein a thickness of the third buffer region is between 1 nm and 1000 nm.

### Claim 11 (depends on 1)

The high electron mobility transistor as claimed in claim 1, wherein the iron (Fe) concentration of the third buffer region near the channel layer ranges between 1E18 cm−3 and 1E17 cm−3.

### Claim 12 (depends on 1)

The high electron mobility transistor as claimed in claim 1, wherein the channel layer forms a two-dimensional electron gas (2DEG) near an interface between the barrier layer and the channel layer; an iron (Fe) concentration of the channel layer near the interface between the barrier layer and the channel layer is less than 5E17 cm−3.