# US 2025/0169120 A1 · High dose implantation for ultrathin semiconductor-on-insulator substrates

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0169120 A1
- Document ID: US20250169120A1
- Status: Published application
- Kind: A1
- Application number: 19/030,171
- Filed: 2025-01-17
- Published: 2025-05-22
- Earliest claimed: 2014-01-31
- Assignees: STMicroelectronics S.r.l.
- Applicants: Stmicroelectronics, Inc.
- Inventors: Jocelyne GIMBERT
- Web page: https://patentgrep.com/patent/US20250169120A1

## CPC

- H10D 30/797: {being in source or drain regions, e.g. SiGe source or drain}
- H10D 30/0275: {forming single crystalline semiconductor source or drain regions resulting in recessed gates, e.g. forming raised source or drain regions}
- H10D 30/0323: {comprising monocrystalline silicon}
- H10D 62/832: being Group IV materials comprising two or more elements, e.g. SiGe
- H10D 62/8325: {Silicon carbide}
- H10D 84/01: Manufacture or treatment
- H10D 84/0167: {Manufacturing their channels}
- H10D 84/017: {Manufacturing their source or drain regions, e.g. silicided source or drain regions}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 86/01: Manufacture or treatment
- H10D 86/201: {the substrates comprising an insulating layer on a semiconductor body, e.g. SOI (H10D86/40 take precedence)}
- H10P 30/204: {into Group IV semiconductors}
- H10P 30/208: {of electrically inactive species}
- H10P 30/21: {of electrically active species}
- H10P 30/28: characterised by an annealing step, e.g. for activation of dopants
- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 62/822: comprising only Group IV materials heterojunctions, e.g. Si/Ge heterojunctions
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Methods and structures for forming highly-doped, ultrathin layers for transistors formed in semiconductor-on-insulator substrates are described. High dopant concentrations may be achieved in ultrathin semiconductor layers to improve device characteristics. Ion implantation at elevated temperatures may mitigate defect formation for stoichiometric dopant concentrations up to about 30%. In-plane stressors may be formed adjacent to channels of transistors formed in ultrathin semiconductor layers.

## Claims

### Claim 1

A method, comprising:
forming a channel region by implanting a dopant in a first portion of an ultrathin semiconductor layer on an insulating layer on a substrate, the ultrathin semiconductor layer having a first surface and a second surface opposite the first surface, the dopant only being in the first portion of the ultrathin semiconductor layer between the first surface and the second surface; and
forming a transistor on the ultrathin semiconductor layer, the transistor including the channel region in the first portion of the ultrathin semiconductor layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the forming the channel region includes maintaining a semiconductor-on-insulator substrate at a temperature between approximately 350° C. and approximately 500° C. during the implanting.

### Claim 3 (depends on 1)

The method of claim 1, wherein the dopant is implanted at an energy between approximately 0.5 keV and approximately 3 keV.

### Claim 4 (depends on 1)

The method of claim 1, wherein the dopant is implanted at a dose between approximately 0.5×1016 cm−2 and approximately 2×1016 cm−2.

### Claim 5 (depends on 1)

The method of claim 1, wherein the forming the channel region includes:
forming, prior to the implanting the dopant, a thin implantation layer over the first portion of the ultrathin semiconductor layer; and
removing the thin implantation layer after the implanting the dopant, wherein the dopant is implanted through the thin implantation layer.

### Claim 6 (depends on 1)

The method of claim 1, wherein the forming the channel region includes:
forming, prior to the implanting the dopant, a hard mask over a second portion of the ultrathin semiconductor layer; and
removing the hard mask after the implanting the dopant.

### Claim 7

A method, comprising:
forming a doped channel in an ultrathin semiconductor layer on an insulating layer on a substrate, the doped channel being between undoped portions of the ultrathin semiconductor layer, wherein forming includes:
heating the substrate and implanting a dopant in the ultrathin semiconductor layer.

### Claim 8 (depends on 7)

The method of claim 7, wherein heating includes maintaining the substrate between approximately 350° C. and approximately 500° C. during the implanting.

### Claim 9 (depends on 7)

The method of claim 7, wherein the dopant is implanted at an energy between approximately 0.5 keV and approximately 3 keV.

### Claim 10 (depends on 7)

The method of claim 7, wherein the dopant is implanted at a dose between approximately 0.5×1016 cm−2 and approximately 2×1016 cm−2.

### Claim 11 (depends on 7)

The method of claim 7, wherein the forming the doped channel region includes:
forming, prior to the implanting the dopant, a thin implantation layer over the first portion of the ultrathin semiconductor layer; and
removing the thin implantation layer after the implanting the dopant, wherein the dopant is implanted through the thin implantation layer.

### Claim 12 (depends on 7)

The method of claim 7, wherein the forming the doped channel includes:
forming, prior to the implanting the dopant, a hard mask over a second portion of the ultrathin semiconductor layer; and
removing the hard mask after the implanting the dopant.

### Claim 13 (depends on 7)

The method of claim 7, wherein a doping level of the dopant is between approximately 15% and approximately 40%.

### Claim 14 (depends on 7)

The method of claim 7, further comprising, after implanting, a step of subjecting the substrate to rapid thermal annealing.

### Claim 15 (depends on 14)

The method of claim 14, wherein the substrate or ultrathin semiconductor layer has a peak temperature between about 500° C. to 1200° C. during the rapid thermal annealing.

### Claim 16

A device, comprising:
a substrate;
an insulating layer on the substrate;
an ultrathin semiconductor layer on the insulating layer, ultrathin semiconductor layer including:
a doped channel having a conductivity dopant, the doped channel in the ultrathin semiconductor layer;
a first undoped portion by the doped channel; and
a second undoped portion by the doped channel, the first portion being spaced from the second portion by the doped channel, the first portion, the second portion, and the channel being coplanar.

### Claim 17 (depends on 16)

The device of claim 16, wherein the dopant is Ge.

### Claim 18 (depends on 16)

The device of claim 16, wherein the ultrathin semiconductor is a silicon layer less than 10 nm.

### Claim 19 (depends on 16)

The device of claim 16, wherein the dopant is an element at a concentration between 15% and 40%.

### Claim 20 (depends on 16)

The device of claim 16, wherein the insulating layer has a thickness between 5 nm and 50 nm.