# US 2025/0167395 A1 · Separator and secondary battery comprising the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0167395 A1
- Document ID: US20250167395A1
- Status: Published application
- Kind: A1
- Application number: 18/954,544
- Filed: 2024-11-21
- Published: 2025-05-22
- Earliest claimed: 2023-11-22
- Assignees: SK Innovation Co., Ltd.; SK ie technology Co., Ltd.
- Applicants: SK Innovation Co., Ltd.; SK Ie Technology Co., Ltd.
- Inventors: Sang Yoon JI; Won Sub KWACK; Dong Il JANG; Soon Bo LEE
- Web page: https://patentgrep.com/patent/US20250167395A1

## CPC

- H01M 50/403: Manufacturing processes of separators, membranes or diaphragms
- H01M 50/446: Composite material consisting of a mixture of organic and inorganic materials
- H01M 10/052: Li-accumulators
- H01M 50/42: Acrylic resins
- H01M 50/434: Ceramics
- H01M 50/443: Particulate material
- H01M 50/449: having a layered structure
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Separator for a secondary battery and secondary battery comprising the separator. The separator comprises a porous substrate, and an inorganic particle layer on at least one surface of the porous substrate, wherein the inorganic particle layer has a surface roughness (Ra) of 180 nm to 230 nm. The separator improves heat resistance, charge/discharge characteristics, and life characteristics of the secondary battery.

## Claims

### Claim 1

A separator comprising:
a porous substrate; and
an inorganic particle layer comprising inorganic particles on at least one surface of the porous substrate,
wherein the inorganic particle layer has a surface roughness (Ra) of 180 nm to 230 nm.

### Claim 2 (depends on 1)

The separator of claim 1, wherein the inorganic particles comprise one or more selected from the group consisting of boehmite, CeO2, MgO, CaO, ZnO, Al2O3, TiO2, BaTiO3, HfO2, SrTiO3, SnO2, NiO, ZrO2, Y2O3, and SiC.

### Claim 3 (depends on 1)

The separator of claim 1, wherein the inorganic particle layer further comprises a binder.

### Claim 4 (depends on 3)

The separator of claim 3, wherein the binder comprises one or more selected from the group consisting of ester-based polymers, amide-based polymers, imide-based polymers, acryl-based polymers, acrylamide-based polymers, vinylalcohol-based polymers, fluorine-based polymers, and vinylpyrrolidone-based polymers.

### Claim 5 (depends on 3)

The separator of claim 3, wherein the binder is comprised at 0.1 parts by weight to 20.0 parts by weight with respect to 100 parts by weight of the inorganic particles.

### Claim 6 (depends on 3)

The separator of claim 3, wherein the binder has a weight average molecular weight of 10,000 g/mol to 2,000,000 g/mol.

### Claim 7 (depends on 1)

The separator of claim 1, wherein the inorganic particles comprise one or more types of inorganic particles having average particle diameters (D50) different from each other.

### Claim 8 (depends on 1)

The separator of claim 1, wherein the inorganic particles have an average particle diameter (D50) of 0.05 μm to 2.0 μm.

### Claim 9 (depends on 1)

The separator of claim 1, wherein the inorganic particle layer has a thickness of 0.1 μm to 10.0 μm.

### Claim 10 (depends on 1)

The separator of claim 1, wherein the inorganic particle layer has a coating density of 0.8 g/(m2·μm) or more.

### Claim 11 (depends on 1)

The separator of claim 1, wherein the separator has shrinkage rates in the machine direction (MD) and in the transverse direction (TD) after being allowed to stand at 150° C. for 60 minutes of 5.0% or less.

### Claim 12 (depends on 1)

The separator of claim 1, wherein the separator has a moisture content of 300 ppm to 1000 ppm, the moisture content being measured by heating the separator to 150° C. after drying the separator at 80° C. for 12 hours in a dry room having a dew point of −40° C. or lower and then leaving the separator in the dry room for 30 minutes.

### Claim 13 (depends on 1)

The separator of claim 1, wherein the separator has a change rate of the surface roughness (Ra) of 15% or less, when a secondary battery manufactured using the separator is charged and discharged for 600 cycles.

### Claim 14 (depends on 1)

A secondary battery comprising the separator according to claim 1.

### Claim 15 (depends on 14)

The secondary battery of claim 14, wherein the secondary battery has a capacity change rate after 100 cycles of charge and discharge of 20% or less.

### Claim 16 (depends on 14)

The secondary battery of claim 14, wherein the secondary battery is a lithium-ion secondary battery.

### Claim 17 (depends on 14)

The secondary battery of claim 14, further comprising an anode, a cathode, with the separator disposed between the anode and cathode,
wherein the cathode comprises a nickel-cobalt-manganese (NCM)-based lithium oxide with an increased nickel content.

### Claim 18 (depends on 14)

The separator of claim 14, wherein the porous substrate of the separator is a polyolefin based polymer and the inorganic particles layer comprises a binder,
wherein the inorganic particles comprise one or more selected from the group consisting of boehmite, CeO2, MgO, CaO, ZnO, Al2O3, TiO2, BaTiO3, HfO2, SrTiO3, SnO2, NiO, ZrO2, Y2O3, and SiC, and