# US 2025/0167245 A1 · Lithium secondary battery and method of producing lithium secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0167245 A1
- Document ID: US20250167245A1
- Status: Published application
- Kind: A1
- Application number: 18/887,479
- Filed: 2024-09-17
- Published: 2025-05-22
- Earliest claimed: 2023-11-17
- Assignees: Toyota Jidosha Kabushiki Kaisha
- Applicants: Toyota Jidosha Kabushiki Kaisha
- Inventors: Ryo ASAKURA; Shinya SHIOTANI; Sakina KANEKO
- Web page: https://patentgrep.com/patent/US20250167245A1

## CPC

- H01M 4/628: {Inhibitors, e.g. gassing inhibitors, corrosion inhibitors}
- H01M 4/0445: {Forming after manufacture of the electrode, e.g. first charge, cycling}
- H01M 4/0447: {of complete cells or cells stacks}
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/366: {as layered products}
- H01M 4/382: {Lithium (H01M4/405 takes precedence)}
- H01M 4/387: {Tin or alloys based on tin}
- H01M 4/405: {Alloys based on lithium}
- H01M 4/466: {Magnesium based}
- H01M 10/052: Li-accumulators
- H01M 10/446: {Initial charging measures}
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

An object of the present disclosure is to provide a lithium secondary battery in which the cycle characteristics can be improved while increasing the reversible capacity. A lithium secondary battery comprising a negative electrode current collector layer, a first lithium-tin alloy layer, a lithium-magnesium alloy layer, an electrolyte layer, a positive electrode active material layer; and a positive electrode current collector layer, in the order mentioned.

## Claims

### Claim 1

A lithium secondary battery comprising a negative electrode current collector layer, a first lithium-tin alloy layer, a lithium-magnesium alloy layer, an electrolyte layer, a positive electrode active material layer; and a positive electrode current collector layer, in the order mentioned.

### Claim 2 (depends on 1)

The lithium secondary battery according to claim 1, wherein, in a fully-charged state, the first lithium-tin alloy layer has a thickness of 0.1 to 15 μm.

### Claim 3 (depends on 1)

The lithium secondary battery according to claim 1, wherein, in a fully-charged state, the lithium-magnesium alloy layer has a thickness of 0.1 to 40 μm.

### Claim 4 (depends on 1)

The lithium secondary battery according to claim 1, comprising the negative electrode current collector layer, the first lithium-tin alloy layer, the lithium-magnesium alloy layer, a second lithium-tin alloy layer, the electrolyte layer, the positive electrode active material layer, and the positive electrode current collector layer, in the order mentioned.

### Claim 5 (depends on 4)

The lithium secondary battery according to claim 4, wherein, in a fully-charged state,
the first lithium-tin alloy layer has a thickness of 0.1 to 15 μm, and
the second lithium-tin alloy layer has a thickness of 0.1 to 15 μm.

### Claim 6 (depends on 1)

A method of producing the lithium secondary battery according to claim 1, the method comprising the following steps of:
obtaining a preliminary lithium secondary battery by laminating the negative electrode current collector layer, a tin-containing first metal layer, a magnesium-containing second metal layer, the electrolyte layer, the positive electrode active material layer retaining lithium, and the positive electrode current collector layer, in the order mentioned; and
performing a charging operation of the preliminary lithium secondary battery to: (i) allow tin of the first metal layer to react with lithium migrating from the positive electrode active material layer, and thereby form the lithium-tin alloy layer; and (ii) allow magnesium of the second metal layer to react with lithium migrating from the positive electrode active material layer, and thereby form the lithium-magnesium alloy layer.

### Claim 7 (depends on 4)

A method of producing the lithium secondary battery according to claim 4, the method including the following steps of:
obtaining the preliminary lithium secondary battery by laminating the negative electrode current collector layer, a tin-containing first metal layer, a magnesium-containing second metal layer, a tin-containing third metal layer, the electrolyte layer, the positive electrode active material layer retaining lithium, and the positive electrode current collector layer, in the order mentioned; and
performing a charging operation of the preliminary lithium secondary battery to: (i) allow tin of the first metal layer to react with lithium migrating from the positive electrode active material layer, and thereby form the first lithium-tin alloy layer; (ii) allow magnesium of the second metal layer to react with lithium migrating from the positive electrode active material layer, and thereby form the lithium-magnesium alloy layer; and (iii) allow tin of the third metal layer to react with lithium migrating from the positive electrode active material layer, and thereby forming the second lithium-tin alloy layer.