# US 2025/0167239 A1 · Electrode Composition and Electrode Comprising Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0167239 A1
- Document ID: US20250167239A1
- Status: Published application
- Kind: A1
- Application number: 18/839,949
- Filed: 2023-03-15
- Published: 2025-05-22
- Earliest claimed: 2022-04-05
- Assignees: Bayerische Motoren Werke Aktiengesellschaft
- Applicants: Bayerische Motoren Werke Aktiengesellschaft
- Inventors: Sung-Jin KIM; Thomas WOEHRLE
- Web page: https://patentgrep.com/patent/US20250167239A1

## CPC

- H01M 4/625: {Carbon or graphite}
- H01M 4/0435: {Rolling or calendering}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 50/105: Pouches or flexible bags
- H01M 4/622: {being polymers}
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

An electrode composition for a lithium-ion battery is provided, the electrode composition comprising: (A) at least one electrode active material and (B) at least one mixture of conductive carbon blacks comprising at least a first conductive carbon black and a second conductive carbon black, the first conductive carbon black differing from the second conductive carbon black. An electrode comprising the electrode composition is further provided. A lithium-ion battery comprising the electrode is further provided. A process for the production of an electrode is further provided.

## Claims

### Claim at position 1

1-12. (canceled)

### Claim 13

An electrode composition for a lithium-ion battery, wherein the electrode composition comprises:
(A) at least one active electrode material; and
(B) at least one mixture of conductive carbon blacks that comprises at least a first conductive carbon black and a second conductive carbon black, the first conductive carbon black differing from the second conductive carbon black.

### Claim 14 (depends on 13)

The electrode composition according to claim 13, wherein the first conductive carbon black and the second conductive carbon black differ in at least one property selected from the group consisting of: mean particle diameter; particle size distribution; secondary structure; specific BET surface area; electrical conductivity; oil absorption coefficient; bulk density; tap density; mode of production; impurities; and surface nature.

### Claim 15 (depends on 13)

The electrode composition according to claim 13, wherein the first conductive carbon black and the second conductive carbon black each have a particle size distribution with a mean particle diameter in a range from 1 to 1000 nm, wherein the mean particle diameter of the first conductive carbon black differs from the mean particle diameter of the second conductive carbon black by at least 10%, and wherein the particle diameter is measured by electron microscopy.

### Claim 16 (depends on 13)

The electrode composition according to claim 13, wherein the at least one mixture of conductive carbon blacks has a bimodal particle size distribution.

### Claim 17 (depends on 13)

The electrode composition according to claim 13, wherein the first conductive carbon black and the second conductive carbon black each have a BET surface area in a range from 1 to 1000 m2·g−1, wherein the BET surface area of the first conductive carbon black differs from the BET surface area of the second conductive carbon black by at least 10%, and wherein the BET surface area is measured according to ASTM D6556-04.

### Claim 18 (depends on 13)

The electrode composition according to claim 13, wherein the first conductive carbon black and the second conductive carbon black each have an oil absorption coefficient in a range from 1 to 800 mL (100 g)−1, wherein the oil absorption coefficient of the first conductive carbon black differs from the oil absorption coefficient of the second conductive carbon black by at least 10%, and wherein the oil absorption coefficient is measured according to ASTM D2414-06 a.

### Claim 19 (depends on 13)

The electrode composition according to claim 13, wherein one of the two conductive carbon blacks of component (B) is obtainable from an incomplete combustion process and the other conductive carbon black is obtainable from a thermal decomposition.

### Claim 20 (depends on 13)

The electrode composition according to claim 13, wherein the first conductive carbon black is present in a fraction of 1% to 99% by weight in the mixture of component (B), based on the total weight of the mixture of component (B).

### Claim 21 (depends on 13)

The electrode composition according to claim 13, wherein the electrode comprises at least one binder selected from the group consisting of polyvinylidene fluoride (PVDF), poly (vinylidene fluoride-hexafluoropropylene) copolymer (PVDF-HFP), polytetrafluoroethylene (PTFE), hydrogenated acrylonitrile-butadiene rubber (HNBR), carboxymethylcellulose (CMC), styrene-butadiene rubber (SBR), polyacrylate (PAA), lithium polyacrylate (LiPAA), polyvinyl alcohol (PVA), and combinations thereof.

### Claim 22 (depends on 13)

The electrode composition according to claim 13, wherein the electrode composition comprises the following components:
(A) 70%-99% by weight of at least one active electrode material;
(B) 0.1%-10% by weight of a mixture of conductive carbon blacks, the mixture comprising at least a first conductive carbon black and a second conductive carbon black, and the first conductive carbon black differing from the second conductive carbon black; and, optionally,
(C) 0%-10% by weight of at least one binder selected from the group consisting of polyvinylidene fluoride (PVDF), poly (vinylidene fluoride-hexafluoropropylene) copolymer (PVDF-HFP), polytetrafluoroethylene (PTFE), hydrogenated acrylonitrile-butadiene rubber (HNBR), carboxymethylcellulose (CMC), styrene-butadiene rubber (SBR), polyacrylate (PAA), lithium polyacrylate (LiPAA), polyvinyl alcohol (PVA), and combinations thereof;
wherein the fractions of the components (A) to (C) add up to 100 percent.

### Claim 23 (depends on 13)

An electrode comprising the electrode composition according to claim 13, wherein the electrode composition is applied to a current collector foil.

### Claim 24 (depends on 23)

A lithium-ion battery comprising the electrode according to claim 23.

### Claim 25 (depends on 24)

The lithium-ion battery according to claim 24, wherein the first conductive carbon black is furnace black and the second conductive carbon black is acetylene black.

### Claim 26 (depends on 24)

The lithium-ion battery according to claim 24, wherein a residual capacity is 80% relative to an initial capacity after about 700 cycles.

### Claim 27

A process for the production of an electrode for a lithium-ion battery, comprising:
adding a first conductive carbon black and a second conductive carbon black to a solution of a binder in a solvent to provide a mixture;
agitating the mixture to provide a homogeneous electrode coating slurry;
applying the slurry to a current collector foil to provide an applied slurry; and
drying the applied slurry;
wherein the first conductive carbon black differs from the second conductive carbon black.

### Claim 28 (depends on 27)

The process according to claim 27, wherein the electrode has a surface weight of 18 mg/cm2 and an electrode density of 3.4 g/cm3.

### Claim 29 (depends on 27)

The process according to claim 27, wherein the agitating is for a duration of about 75 minutes.

### Claim 30 (depends on 27)

The process according to claim 27, further comprising, after the agitating, adjusting a viscosity of the slurry to a target viscosity of from 5 Pa·s−1 to 20 Pa·s−1 by adding or evaporating the solvent.

### Claim 31 (depends on 27)

The process according to claim 27, wherein the first conductive carbon black and the second conductive carbon black differ in at least one property selected from the group consisting of: mean particle diameter; particle size distribution; secondary structure; specific BET surface area; electrical conductivity; oil absorption coefficient; bulk density; tap density; mode of production; impurities; and surface nature.

### Claim 32 (depends on 27)

The process according to claim 27, wherein the binder is selected from the group consisting of polyvinylidene fluoride (PVDF), poly (vinylidene fluoride-hexafluoropropylene) copolymer (PVDF-HFP), polytetrafluoroethylene (PTFE), hydrogenated acrylonitrile-butadiene rubber (HNBR), carboxymethylcellulose (CMC), styrene-butadiene rubber (SBR), polyacrylate (PAA), lithium polyacrylate (LiPAA), polyvinyl alcohol (PVA), and combinations thereof.