# US 2025/0167238 A1 · Bipolar electrode with aligned active layers, lithium ion batteries having such electrodes, and a method of making such electrodes

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0167238 A1
- Document ID: US20250167238A1
- Status: Published application
- Kind: A1
- Application number: 18/515,976
- Filed: 2023-11-21
- Published: 2025-05-22
- Earliest claimed: 2023-11-21
- Assignees: GM Global Technology Operations LLC
- Applicants: GM Global Technology Operations LLC
- Inventors: Seung-Woo Chu; Mark Daniel Gottlieb
- Web page: https://patentgrep.com/patent/US20250167238A1

## CPC

- H01M 4/625: {Carbon or graphite}
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/0435: {Rolling or calendering}
- H01M 4/136: Electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/1393: of electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/1397: of electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 4/587: for inserting or intercalating light metals
- H01M 4/622: {being polymers}
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/029: {Bipolar electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A bipolar electrode for use in a lithium-ion battery includes a current collector, an anode having high aspect ratio conductive carbon particles and an anode binder, and a cathode having cathode active particles in a cathode binder. The high aspect ratio conductive carbon particles in the anode are aligned so that a long axis of the high aspect ratio conductive carbon particles is substantially perpendicular to the current collector. The cathode active particles are paramagnetic, diamagnetic, or magnetic and have been magnetically aligned, the cathode further comprises high aspect ratio conductive particles aligned so that a long axis of the high aspect ratio conductive particles is substantially perpendicular to the current collector, or both. The bipolar electrode can be made by subjecting the current collector coated with slurries including the components for the anode and the cathode to a magnetic field while drying.

## Claims

### Claim 1

A bipolar electrode for use in a lithium ion battery, wherein the bipolar electrode comprises:
a current collector;
an anode on a first side of the current collector, the anode comprising high aspect ratio conductive carbon particles and an anode binder wherein the high aspect ratio conductive carbon particles are aligned so that a long axis of the high aspect ratio conductive carbon particles is substantially perpendicular to the current collector; and
a cathode on an opposite side of the current collector from the anode, the cathode comprising cathode active particles in a cathode binder;
wherein (a) the cathode active particles are paramagnetic, diamagnetic, or magnetic and have been magnetically aligned, (b) the cathode further comprises high aspect ratio conductive particles aligned so that a long axis of the high aspect ratio conductive particles is substantially perpendicular to the current collector, or (c) both.

### Claim 2 (depends on 1)

The bipolar electrode of claim 1 wherein the current collector comprises a stainless steel having a thickness of 3 to 50 microns and length and width of 10 to 100 centimeters.

### Claim 3 (depends on 1)

The bipolar electrode of claim 1 wherein the high aspect ratio conductive carbon particles comprise plate shaped particles.

### Claim 4 (depends on 1)

The bipolar electrode of claim 1 wherein the anode comprise 90 to 97 weight percent of the high aspect ratio conductive carbon particles and 3 to 10 weight percent of the anode binder based on total weight of the anode.

### Claim 5 (depends on 3)

The bipolar electrode of claim 3 wherein plate shaped particles are graphite flakes.

### Claim 6 (depends on 1)

The bipolar electrode of claim 1 wherein the anode binder is a carboxymethylcellulose or a styrene butadiene rubber.

### Claim 7 (depends on 1)

The bipolar electrode of claim 1 wherein the cathode active particles comprise lithium transition metal phosphates.

### Claim 8 (depends on 6)

The bipolar electrode of claim 6 wherein the cathode active particles comprise lithium iron phosphates.

### Claim 9 (depends on 1)

The bipolar electrode of claim 1 wherein the cathode includes the high aspect ratio conductive particles.

### Claim 10 (depends on 1)

The bipolar electrode of claim 1 having a thickness of 100 to 300 microns.

### Claim 11

A method of making a bipolar electrode comprising:
preparing a cathode slurry comprising cathode active particles, and a cathode binder in a solvent, provided that (a) the cathode active particles are paramagnetic, magnetic or diamagnetic, (b) the cathode slurry further comprises high aspect ratio conductive particles that are paramagnetic, magnetic or diamagnetic, or (c) both;
coating the cathode slurry onto a first surface of a current collector;
preparing an anode slurry comprising high aspect ratio conductive carbon particles and an anode binder in a solvent form an anode slurry;
coating the anode slurry onto an opposite surface of the current collector from the cathode slurry; and
while drying the coatings of the anode slurry and the cathode slurry subjecting the coated current collector to a magnetic field to cause alignment of any paramagnetic cathode active particles, any high aspect ratio conductive particles, and the high aspect ratio conductive carbon particles.

### Claim 12 (depends on 11)

The method of claim 11 wherein the drying of the anode slurry occurs before the coating of the cathode slurry or the drying of the cathode slurry occurs before the coating of the anode slurry.

### Claim 13 (depends on 11)

The method of claim 11 wherein after drying of the cathode slurry, the cathode and current collector are calendered, the coating and drying of the anode occurs after the calendering of the cathode and current collector, and after drying the anode, the cathode, current collector and anode are calendered.

### Claim 14 (depends on 11)

The method of claim 11 wherein coating the cathode slurry the first surface of the current collector and coating the anode slurry to the opposite surface of the cathode slurry, and then the coatings of the anode slurry and the cathode slurry are simultaneously dried while being subjected to the magnetic field.

### Claim 15 (depends on 11)

The method of claim 11 wherein the magnetic field is from 1 to 12 Tesla and is applied for 1 to 10 minutes.

### Claim 16 (depends on 11)

The method of claim 11 wherein the magnetic field is varied in intensity and/or direction while it is being applied to the electrode during the drying.

### Claim 17

An electrochemical cell comprising one or more bipolar electrodes located between a first anode on a first anode current collector and a first cathode on a first cathode current collector, wherein the bipolar electrode has a cathode and an anode on opposing surfaces of a third current collector, wherein the one or more bipolar electrodes, the first anode and the first cathode are positioned such that each anode is facing and is separated from an adjacent cathode by a separator, wherein the electrochemical cell further comprises an electrolyte,
wherein the anode of the one or more bipolar electrodes comprises high aspect ratio conductive carbon particles and anode binder wherein the high aspect ratio conductive carbon particles are aligned so that a long axis of the high aspect ratio conductive carbon particles is substantially perpendicular to the third current collector, and
the cathode of the one or more bipolar electrodes comprises cathode active particles in a cathode binder wherein the cathode active particles are paramagnetic and have been magnetically aligned, the cathode further comprises high aspect ratio conductive particles aligned so that a long axis of the high aspect ratio conductive particles is substantially perpendicular to the third current collector, or both.

### Claim 18 (depends on 17)

The electrochemical cell of claim 17 wherein the cathode active particles comprise lithium transition metal phosphates.

### Claim 19 (depends on 17)

The electrochemical cell of claim 17 wherein the first anode comprises high aspect ratio conductive carbon particles aligned so that a long axis of the high aspect ratio conductive carbon particles is substantially perpendicular to the first anode current collector, the first cathode comprises high aspect ratio comprises high aspect ratio conductive particles aligned so that a long axis of the high aspect ratio conductive particles is substantially perpendicular to the first cathode current collector, or both.

### Claim 20 (depends on 17)

The electrochemical cell of claim 17 comprising at least two of the bipolar electrodes.