# US 2025/0167232 A1 · Lithium manganese iron phosphate material, preparation method thereof, and lithium battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0167232 A1
- Document ID: US20250167232A1
- Status: Published application
- Kind: A1
- Application number: 18/946,990
- Filed: 2024-11-14
- Published: 2025-05-22
- Earliest claimed: 2023-11-21
- Assignees: Eve Power Co., Ltd.
- Applicants: Eve Power Co., Ltd.
- Inventors: Tingting WU; Fanfen LIU; Shengyao WEN; Jianhang GAO; Meng CHEN
- Web page: https://patentgrep.com/patent/US20250167232A1

## CPC

- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- C01B 25/45: containing plural metal, or metal and ammonium
- H01M 4/136: Electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/366: {as layered products}
- H01M 4/625: {Carbon or graphite}
- H01M 4/628: {Inhibitors, e.g. gassing inhibitors, corrosion inhibitors}
- H01M 10/052: Li-accumulators
- H01M 10/4235: {Safety or regulating additives or arrangements in electrodes, separators or electrolyte (H01M10/4242 takes precedence)}
- C01P 2002/54: one element only
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2002/82: by IR- or Raman-data
- C01P 2004/03: obtained by SEM
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2004/80: Particles consisting of a mixture of two or more inorganic phases
- C01P 2006/40: Electric properties
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Disclosed are a lithium manganese iron phosphate material, a preparation method thereof, and a lithium battery. The lithium manganese iron phosphate material includes a core and a coating layer on the core. A material of the core includes Li, M, and PO4 in a non-stoichiometric ratio, M is FeyMnxDz, in which D is a metal. The coating layer includes a carbon material. The lithium manganese iron phosphate material has good structural stability, actual capacity per gram, and cycle life.

## Claims

### Claim 1

A lithium manganese iron phosphate material comprising a core and a coating layer on the core;
wherein a material of the core comprises Li, M and PO4 in a non-stoichiometric ratio, in which Mis FeyMnxDz, D is a metal except Fe or Mn, x, y and z represent a molar amount of Fe, Mn and the metal in the lithium manganese iron phosphate material, respectively, and a sum of molar amounts of Fe, Mn and the metal is A; and the coating layer comprises a carbon material;
in the lithium manganese iron phosphate material, a ratio of a molar amount of Li to A is 1.01 to 1.10, a ratio of the molar amount of Li to a molar amount of PO4 is 0.95 to 1.10, and a ratio of A to the molar amount of PO4 is 0.90 to 1.15.

### Claim 2 (depends on 1)

The lithium manganese iron phosphate material according to claim 1, wherein, in the lithium manganese iron phosphate material, at least one of the following is satisfied:
the ratio of the molar amount of Li to A is 1.03 to 1.07,
the ratio of the molar amount of Li to the molar amount of PO4 is 1.00 to 1.05, or
the ratio of A to the molar amount of PO4 is 0.95 to 1.10.

### Claim 3 (depends on 1)

The lithium manganese iron phosphate material according to claim 1, wherein a particle size D50 of the core is less than 10 μm.

### Claim 4 (depends on 1)

The lithium manganese iron phosphate material according to claim 1, wherein at least one of the following is satisfied:
a mass of the carbon material constitutes 0.5% to 3% of a total mass of the lithium manganese iron phosphate material; or
a thickness of the coating layer is 3 nm to 5 nm.

### Claim 5 (depends on 4)

The lithium manganese iron phosphate material according to claim 4, wherein a ratio of a D band to a G band of the carbon material is ID/IG, and 0.50<ID/IG<0.95.

### Claim 6 (depends on 1)

The lithium manganese iron phosphate material according to claim 1, wherein, at least one of the following is satisfied:
in M, D is selected from one or more of Mg, Ti, V, Ni, Co, Al, Nb, Nd, Y, Mo, Sr, La, Zr, B, and Ca; or
in M, 0.1<x<0.9, 0.1<y<0.5, and 0<z<0.5.

### Claim 7

A method for preparing a lithium manganese iron phosphate material, comprising the following steps:
providing a first slurry comprising a lithium source, a manganese source, an iron source, a phosphorus source, a carbon source, and a D source;
grinding the first slurry to obtain a second slurry;
subjecting the second slurry to spray drying to obtain a pre-sintered material; and
sintering the pre-sintered material under an atmosphere of a protective gas, and
obtaining the lithium manganese iron phosphate material;
wherein the obtained lithium manganese iron phosphate material comprises a core and a coating layer on the core; a material of the core comprises Li, M and PO4 in a non-stoichiometric ratio, in which Mis FeyMnxDz, in which D is a metal except Fe or Mn, x, y and z represent a molar amount of Fe, Mn and the metal in the lithium manganese iron phosphate material, respectively, and a sum of molar amounts of Fe, Mn and the metal is A; the coating layer comprises a carbon material; and in the lithium manganese iron phosphate material, a ratio of a molar amount of Li to A is 1.01 to 1.10, a ratio of the molar amount of Li to a molar amount of PO4 is 0.95 to 1.10, and a ratio of A to the molar amount of PO4 is 0.90 to 1.15.

### Claim 8 (depends on 7)

The method according to claim 7, wherein at least one of the following is satisfied:
the sintering step is conducted at a temperature of 600° C. to 800° C. for 4 h to 8 h;
the method for preparing the lithium manganese iron phosphate material further comprises, after the sintering step and before the step of obtaining the lithium manganese iron phosphate material, pulverizing the sintered material, and then screening the pulverized material through a mesh sieve of 150 mesh to 200 mesh to obtain the lithium manganese iron phosphate material; or
the protective gas is selected from one or more of nitrogen gas, argon gas, helium gas, neon gas, krypton gas, and xenon gas.

### Claim 9 (depends on 7)

The method according to claim 7, wherein, in the lithium manganese iron phosphate material, at least one of the following is satisfied:
the ratio of the molar amount of Li to A is 1.03 to 1.07,
the ratio of the molar amount of Li to the molar amount of PO4 is 1.00 to 1.05, or
the ratio of A to the molar amount of PO4 is 0.95 to 1.10.

### Claim 10 (depends on 7)

The method according to claim 7, wherein a particle size D50 of the core is less than 10 μm.

### Claim 11 (depends on 7)

The method according to claim 7, wherein at least one of the following is satisfied:
a mass of the carbon material constitutes 0.5% to 3% of a total mass of the lithium manganese iron phosphate material; or
a thickness of the coating layer is 3 nm to 5 nm.

### Claim 12 (depends on 7)

The method according to claim 7, wherein at least one of the following is satisfied:
a ratio of a D band to a G band of the carbon material is ID/IG, satisfying 0.50<ID/IG<0.95;
in M, D is selected from one or more of Mg, Ti, V, Ni, Co, Al, Nb, Nd, Y, Mo, Sr, La, Zr, B, and Ca; or
in M, 0.1<x<0.9, 0.1<y<0.5, 0<z<0.5.

### Claim 13

A lithium battery comprising one or more battery cell units, wherein each of the battery cell units comprises a positive electrode sheet, a separator, and a negative electrode sheet, which are stacked in sequence, the positive electrode sheet comprises a positive current collector and a positive active material layer disposed on one or more surfaces of the positive current collector, and the positive active material layer comprises a lithium manganese iron phosphate material;
the lithium manganese iron phosphate material comprises a core and a coating layer on the core; a material of the core comprises Li, M and PO4 in a non-stoichiometric ratio, in which M is FeyMnxDz, D is a metal except Fe or Mn, in which x, y and z represent a molar amount of Fe, Mn and the metal in the lithium manganese iron phosphate material, respectively, and a sum of molar amounts of Fe, Mn and the metal is A; and the coating layer comprises a carbon material;
in the lithium manganese iron phosphate material, a ratio of a molar amount of Li to A is 1.01 to 1.10, a ratio of the molar amount of Li to a molar amount of PO4 is 0.95 to 1.10, and a ratio of A to the molar amount of PO4 is 0.90 to 1.15.

### Claim 14 (depends on 13)

The lithium battery according to claim 13, wherein, in the lithium manganese iron phosphate material, at least one of the following is satisfied:
the ratio of the molar amount of Li to A is 1.03 to 1.07,
the ratio of the molar amount of Li to the molar amount of PO4 is 1.00 to 1.05, or
the ratio of A to the molar amount of PO4 is 0.95 to 1.10.

### Claim 15 (depends on 13)

The lithium battery according to claim 13, wherein at least one of the following is satisfied:
a particle size D50 of the core is less than 10 μm;
a mass of the carbon material constitutes 0.5% to 3% of a total mass of the lithium manganese iron phosphate material;
a thickness of the coating layer is 3 nm to 5 nm;
a ratio of a D band to a G band of the carbon material is ID/IG, satisfying 0.50<ID/IG<0.95;
in M, D is selected from one or more of Mg, Ti, V, Ni, Co, Al, Nb, Nd, Y, Mo, Sr, La, Zr, B, and Ca; or