# US 2025/0167228 A1 · Positive electrode active materials, preparation methods thereof, positive electrodes, and rechargeable lithium batteries

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0167228 A1
- Document ID: US20250167228A1
- Status: Published application
- Kind: A1
- Application number: 18/952,931
- Filed: 2024-11-19
- Published: 2025-05-22
- Earliest claimed: 2023-11-20
- Assignees: Samsung SDI Co., Ltd.
- Applicants: Samsung SDI Co., Ltd.
- Inventors: Seungyeon CHOI; Soohyeon KIM; Dongwook SHIN; Soonkie HONG; Aram CHOI; Jeuk HA; Minah CHA; Minhan KIM
- Web page: https://patentgrep.com/patent/US20250167228A1

## CPC

- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- C01G 53/04: Oxides
- C01G 53/42: containing alkali metals, e.g. LiNiO2
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/366: {as layered products}
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2002/52: containing elements as dopants
- C01P 2004/03: obtained by SEM
- C01P 2004/50: Agglomerated particles
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2006/16: Pore diameter
- C01P 2006/40: Electric properties
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A positive electrode active material includes a layered lithium nickel-based composite oxide, wherein, based on 100 mol % of a total mole of metals of the layered lithium nickel-based composite oxide excluding lithium, a nickel content is greater than or equal to about 60 mol %, an aluminum content is about 0.8 mol % to about 1.5 mol %, a zirconium content is about 0.1 mol % to about 0.3 mol %, and a ratio of the aluminum content relative to the zirconium content (Al/Zr) is greater than or equal to about 5, and the positive electrode active material is in a form of a single particle with an average particle diameter (D50) of about 1 μm to about 4 μm.

## Claims

### Claim 1

A positive electrode active material, comprising:
a layered lithium nickel-based composite oxide,
wherein,
a nickel content is greater than or equal to about 60 mol % based on 100 mol % of a total mole of metals of the layered lithium nickel-based composite oxide excluding lithium,
an aluminum content is about 0.8 mol % to about 1.5 mol % based on the 100 mol % of the total mole of the metals of the layered lithium nickel-based composite oxide excluding lithium, and
a zirconium content is about 0.1 mol % to about 0.3 mol % based on the 100 mol % of the total mole of the metals of the layered lithium nickel-based composite oxide excluding lithium,
wherein,
a ratio of the aluminum content relative to the zirconium content (Al/Zr) is greater than or equal to about 5, and
wherein,
the positive electrode active material is in a form of a single particle with an average particle diameter (D50) of about 1 μm to about 4 μm.

### Claim 2 (depends on 1)

The positive electrode active material as claimed in claim 1, wherein: the positive electrode active material is in a form of one single particle separated from another single particle or two to nine single particles attached with each other.

### Claim 3 (depends on 1)

The positive electrode active material as claimed in claim 1, wherein:
the layered lithium nickel-based composite oxide is represented by Chemical Formula 1:
Lia1Nix1M1y1Alz1Zrw1O2-b1Xb1 [Chemical Formula 1]
in Chemical Formula 1, 0.9≤a1≤1.2, 0.6≤x1≤0.991, 0≤y1≤0.391, 0.008≤z1≤0.015, 0.001≤w1≤0.003, 0.9≤x1+y1+z1+w1≤1.1, and 0≤b1≤0.1, M1 being one or more elements selected from among B, Ba, Ca, Ce, Co, Cr, Cu, Fe, Mg, Mn, Mo, Nb, Si, Sn, Sr, Ti, V, W, and Zn, and X being one or more elements selected from among F, P, and S.

### Claim 4 (depends on 1)

A positive electrode, comprising:
a positive electrode current collector, and
a positive electrode active material layer located on the positive electrode current collector and comprising the positive electrode active material as claimed in claim 1.

### Claim 5 (depends on 1, 4)

The positive electrode as claimed in claim 4, wherein the positive electrode active material layer comprises:
a first positive electrode active material comprising the positive electrode active material as claimed in claim 1, and
a second positive electrode active material in a form of secondary particles, wherein each of the secondary particles comprises an agglomeration of a plurality of primary particles,
wherein the second positive electrode active material comprises a layered lithium nickel-based composite oxide,
wherein,
a nickel content is greater than or equal to about 60 mol % based on 100 mol % of a total mole of metals of the layered lithium nickel-based composite oxide excluding lithium,
an aluminum content is about 0.8 mol % to about 1.5 mol % based on the 100 mol % of the total mole of the metals of the layered lithium nickel-based composite oxide excluding lithium, and
a zirconium content is about 0.1 mol % to about 0.3 mol % based on the 100 mol % of the total mole of the metals of the layered lithium nickel-based composite oxide excluding lithium,
wherein,
a ratio of the aluminum content relative to the zirconium content (Al/Zr) is greater than or equal to about 5, and
wherein,
the secondary particles have a hollow structure with pores inside, and an average particle diameter (D50) of the primary particles constituting the secondary particles is about 1 μm to about 4 μm.

### Claim 6 (depends on 5)

The positive electrode as claimed in claim 5, wherein:
the layered lithium nickel-based composite oxide of the second positive electrode active material is represented by Chemical Formula 1:
Lia1Nix1M1y1Alz1Zrw1O2-b1Xb1 [Chemical Formula 1]
in Chemical Formula 1, 0.9≤a1≤1.2, 0.6≤x1≤0.991, 0≤y1≤0.391, 0.008≤z1≤0.015, 0.001≤w1≤0.003, 0.9≤x1+y1+z1+w1≤1.1, and 0≤b1≤0.1, M1 being one or more elements selected from among B, Ba, Ca, Ce, Co, Cr, Cu, Fe, Mg, Mn, Mo, Nb, Si, Sn, Sr, Ti, V, W, and Zn, and X being one or more elements selected from among F, P, and S.

### Claim 7 (depends on 5)

The positive electrode as claimed in claim 5, wherein:
an average particle diameter (D50) of the secondary particles of the second positive electrode active material is about 10 μm to about 20 μm.

### Claim 8 (depends on 7)

The positive electrode as claimed in claim 7, wherein:
a size of the pores inside the secondary particles of the second positive electrode active material is about 1 μm to about 9 μm.

### Claim 9 (depends on 5)

The positive electrode as claimed in claim 5, wherein:
based on 100 wt % of a total weight of the first positive electrode active material and the second positive electrode active material, the first positive electrode active material is included at about 5 wt % to about 60 wt %, and the second positive electrode active material is included at about 40 wt % to about 95 wt %.

### Claim 10

A method of preparing a positive electrode active material comprising
performing a co-precipitation reaction of a nickel precursor and an M1 precursor to prepare a nickel-based composite hydroxide being in a form of particles and having micropores inside the particles,
mixing the nickel-based composite hydroxide, a lithium raw material, an aluminum raw material, and a zirconium raw material and performing a heat treatment to prepare hollow secondary particles comprising layered lithium nickel-based composite oxide and having pores inside as secondary particles made by agglomerating a plurality of primary particles,
pulverizing the secondary particles, and
obtaining a positive electrode active material,
wherein M1 is one or more elements selected from among B, Ba, Ca, Ce, Co, Cr, Cu, Fe, Mg, Mn, Mo, Nb, Si, Sn, Sr, Ti, V, W, and Zn, and
based on 100 mol % of a total mole of metals of the nickel-based composite hydroxide, aluminum in the aluminum raw material, and zirconium in the zirconium raw material, an aluminum content of the aluminum raw material is about 0.8 mol % to about 1.5 mol %, a zirconium content of the zirconium raw material is about 0.1 mol % to about 0.3 mol %, and a ratio of the aluminum content relative to the zirconium content (Al/Zr) is greater than or equal to about 5.

### Claim 11 (depends on 10)

The method as claimed in claim 10, wherein:
the co-precipitation reaction comprises a first reacting at a pH ranging from about 11 to about 12, and a second reacting at a pH lower than that of the first reacting.

### Claim 12 (depends on 10)

The method as claimed in claim 10, wherein:
the nickel-based composite hydroxide is represented by Chemical Formula 11:
Nix11M1y11(OH)2 [Chemical Formula 11]
in Chemical Formula 11, 0.6≤x11≤1, 0≤y11≤0.4, and 0.9≤x11+y11≤1.1, and M1 being one or more elements selected from among B, Ba, Ca, Ce, Co, Cr, Cu, Fe, Mg, Mn, Mo, Nb, Si, Sn, Sr, Ti, V, W, and Zn; and
wherein the nickel-based composite hydroxide is amorphous, and
the nickel-based composite hydroxide is in a form of a particle, and the particle comprises an inner portion comprising a plurality of micropores and an outer portion that surrounds the inner portion and has a dense structure.

### Claim 13 (depends on 10)

The method as claimed in claim 10, wherein:
a lithium content of the lithium raw material is about 0.9 parts by mole to about 1.2 parts by mole based on the total metals of 1 part by mole of metals of the nickel-based composite hydroxide, aluminum of the aluminum raw material, and zirconium of the zirconium raw material,
the aluminum raw material is aluminum oxide, and
the zirconium raw material is zirconium oxide.

### Claim 14 (depends on 10)

The method as claimed in claim 10, wherein:
the heat treatment is performed at about 700° C. to about 900° C. in an oxidizing gas atmosphere; and
in the mixing of the nickel-based composite hydroxide, the lithium raw material, the aluminum raw material, and the zirconium raw material and the performing of the heat treatment, an alkaline grain growth accelerator is not added.

### Claim 15 (depends on 10)

The method as claimed in claim 10, wherein:
the layered lithium nickel-based composite oxide is represented by Chemical Formula 1:
Lia1Nix1M1y1Alz1Zrw1O2-b1Xb1 [Chemical Formula 1]
in Chemical Formula 1, 0.9≤a1≤1.2, 0.6≤x1≤0.991, 0≤y1≤0.391, 0.008≤z1≤0.015, 0.001≤w1≤0.003, 0.9≤x1+y1+z1+w1≤1.1, and 0≤b1≤0.1, M1 being one or more elements selected from among B, Ba, Ca, Ce, Co, Cr, Cu, Fe, Mg, Mn, Mo, Nb, Si, Sn, Sr, Ti, V, W, and Zn, and X being one or more elements selected from among F, P, and S; and
wherein an average particle diameter (D50) of the secondary particles is about 10 μm to about 20 μm, and
an average particle diameter (D50) of the primary particles constituting the secondary particles is about 1 μm to about 4 μm, and
a size of the pores inside the secondary particles is about 1 μm to about 9 μm.

### Claim 16 (depends on 10)

The method as claimed in claim 10, wherein:
the pulverizing of the secondary particles is performed utilizing a jet mill or air flow classifying mill equipment, and is performed for about 10 to about 120 minutes; and
wherein the method comprises:
performing a reheat treatment after the pulverizing of the secondary particles, wherein the reheat treatment is performed in an oxidizing gas atmosphere at about 500° C. to about 900° C.

### Claim 17 (depends on 10)

The method as claimed in claim 10, wherein the method comprises:
mixing the pulverized secondary particles with a coating raw material, and
performing a reheat treatment after the pulverized secondary particles mixed with the coating raw material, wherein the reheat treatment is performed in an oxidizing gas atmosphere at about 500° C. to about 900° C.,
wherein the coating raw material is a raw material of one or more elements selected from among Al, B, Co, Mg, V, Zn, and Zr.

### Claim 18 (depends on 10)

The method as claimed in claim 10, wherein:
the obtained positive electrode active material comprises single particles having an average particle diameter (D50) of about 1 μm to about 4 μm.

### Claim 19 (depends on 10)

The method as claimed in claim 10, wherein the obtained positive electrode active material comprises:
a first positive electrode active material in a form of a single particle having an average particle diameter (D50) of about 1 μm to about 4 μm, and
a second positive electrode active material in a form of secondary particles each made by agglomerating a plurality of primary particles,
wherein an average particle diameter (D50) of the secondary particles of the second positive electrode active material is about 10 μm to about 20 μm, and an average particle diameter (D50) of the primary particles constituting the secondary particles is about 1 μm to about 4 μm.

### Claim 20 (depends on 4)

A rechargeable lithium battery, comprising:
the positive electrode as claimed in claim 4,
a negative electrode, and
an electrolyte.