# US 2025/0167224 A1 · Electrode composite material slurry for solid-state battery and production method for electrode composite material slurry

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0167224 A1
- Document ID: US20250167224A1
- Status: Published application
- Kind: A1
- Application number: 18/953,387
- Filed: 2024-11-20
- Published: 2025-05-22
- Earliest claimed: 2023-11-20
- Assignees: Toyota Jidosha Kabushiki Kaisha; Panasonic Holdings Corporation
- Applicants: Toyota Jidosha Kabushiki Kaisha; Panasonic Holdings Corporation
- Inventors: Yasutaka TSUTSUI; Masahiro IWASAKI
- Web page: https://patentgrep.com/patent/US20250167224A1

## CPC

- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/139: Processes of manufacture
- H01M 4/583: Carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 4/622: {being polymers}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0562: Solid materials
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- H01M 2300/0068: inorganic
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

An electrode composite material slurry contains an electrode active material, a solid electrolyte, and a dispersion medium, and the particle diameter of the electrode composite material slurry measured by a fineness gauge method is 60 μm or less. A production method for the electrode composite material slurry includes (i) preparing the electrode composite material slurry by applying a dispersion energy of 1.0×106 J/L or more to a preliminary electrode composite material slurry and stirring the preliminary electrode composite material slurry and/or (ii) preparing the electrode composite material slurry by stirring the preliminary electrode composite material slurry until the particle diameter that is measured by the fineness gauge method becomes 0.75 times or less the particle diameter that is measured by the fineness gauge method when a dispersion energy of 5.0×105 J/L is applied to the preliminary electrode composite material slurry and stirring is performed.

## Claims

### Claim 1

An electrode composite material slurry for a solid-state battery, wherein:
the electrode composite material slurry contains an electrode active material, a solid electrolyte, and a dispersion medium; and
a particle diameter of the electrode composite material slurry that is measured by a fineness gauge method is 60 μm or less.

### Claim 2 (depends on 1)

The electrode composite material slurry according to claim 1, wherein the electrode composite material slurry contains a rubber binder.

### Claim 3 (depends on 1)

The electrode composite material slurry according to claim 1, wherein the electrode composite material slurry contains a negative electrode active material.

### Claim 4 (depends on 1)

A production method for the electrode composite material slurry according to claim 1, the production method comprising:
providing a preliminary electrode composite material slurry that contains an electrode active material, a solid electrolyte, and a dispersion medium; and
(i) preparing the electrode composite material slurry by applying a dispersion energy of 1.0×106 J/L or more to the preliminary electrode composite material slurry and stirring the preliminary electrode composite material slurry and/or (ii) preparing the electrode composite material slurry by stirring the preliminary electrode composite material slurry until the particle diameter that is measured by the fineness gauge method becomes 0.75 times or less the particle diameter that is measured by the fineness gauge method when a dispersion energy of 5.0×105 J/L is applied to the preliminary electrode composite material slurry and the preliminary electrode composite material slurry is stirred.

### Claim 5

An electrode active material layer for a solid battery, comprising:
a maximum particle diameter of an electrode active material and a solid electrolyte measured from an SEM image of a cross section of the electrode active material layer is 60 μm or less.