# US 2025/0167221 A1 · Electrode for secondary battery, manufacturing method thereof, and lithium secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0167221 A1
- Document ID: US20250167221A1
- Status: Published application
- Kind: A1
- Application number: 18/841,397
- Filed: 2023-03-22
- Published: 2025-05-22
- Earliest claimed: 2022-05-16
- Assignees: SK On Co., Ltd.
- Applicants: SK On Co., Ltd.
- Inventors: Byoung-Ho KO
- Web page: https://patentgrep.com/patent/US20250167221A1

## CPC

- H01M 4/366: {as layered products}
- H01M 4/02: Electrodes composed of, or comprising, active material
- H01M 4/04: Processes of manufacture in general
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/13: Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof
- H01M 4/139: Processes of manufacture
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 4/623: {fluorinated polymers}
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

An electrode for a secondary battery according to one embodiment of the present invention comprises: a current collector; a first electrode mixture layer disposed on the current collector and including a first active material and a first binder; and a second electrode mixture layer disposed on the first electrode mixture layer and including a second active material and a second binder, wherein the weight ratio of the first binder in the first electrode mixture layer is equal to or greater than the weight ratio of the second binder in the second electrode mixture layer, and the electrode adhesive force with the current collector is 0.37 N/18 mm or greater. According to one embodiment of the present invention, provided are an electrode for a secondary battery having excellent electrode adhesion, resistance characteristics, etc., and a method for manufacturing same.

## Claims

### Claim 1

An electrode for a secondary battery, comprising:
a current collector;
a first electrode mixture layer located on the current collector, and including a first active material and a first binder; and
a second electrode mixture layer located on the first electrode mixture layer, and including a second active material and a second binder,
wherein a weight ratio of the first binder to the first electrode mixture layer is greater than or equal to a weight ratio of the second binder to the second electrode mixture layer, and
electrode adhesion with the current collector is 0.37 N/18 mm or more.

### Claim 2 (depends on 1)

The electrode for a secondary battery of claim 1, wherein a molecular weight of the second binder is greater than a molecular weight of the first binder.

### Claim 3 (depends on 1)

The electrode for a secondary battery of claim 1, wherein a weight average molecular weight (Mw) of the first binder is 900,000 or less, and
a weight average molecular weight (Mw) of the second binder is 950,000 or more.

### Claim 4 (depends on 1)

The electrode for a secondary battery of claim 1, wherein a bulk resistance value is 5.5 Ω·cm or less.

### Claim 5 (depends on 1)

The electrode for a secondary battery of claim 1, wherein an interfacial resistance value is 0.035 Ω·cm2 or more.

### Claim 6

A method for manufacturing an electrode for a secondary battery, comprising:
forming a first electrode mixture layer on a current collector with a first slurry including a first active material and a first binder; and
forming a second electrode mixture layer on the first electrode mixture layer with a second slurry including a second active material and a second binder,
wherein a weight ratio of the first binder to the first electrode mixture layer is greater than or equal to a weight ratio of the second binder to the second electrode mixture layer, and
a molecular weight of the second binder is greater than a molecular weight of the first binder.

### Claim 7 (depends on 6)

The method for manufacturing an electrode for a secondary battery of claim 6, wherein the first binder is included in an amount of 0.8 to 1.5 parts by weight based on 100 parts by weight of the first electrode mixture layer, and
the second binder is included in an amount of 0.05 to 0.8 parts by weight based on 100 parts by weight of the second electrode mixture layer.

### Claim 8 (depends on 6)

The method for manufacturing an electrode for a secondary battery of claim 6, wherein a weight average molecular weight (Mw) of the first binder is 900,000 or less,
a weight average molecular weight (Mw) of the second binder is 950,000 or more.

### Claim 9 (depends on 6)

The method for manufacturing an electrode for a secondary battery of claim 6, wherein the first binder and the second binder are respectively polyvinylidene fluoride (PVDF) having different molecular weights.

### Claim 10 (depends on 6)

The method for manufacturing an electrode for a secondary battery of claim 6, wherein a difference in solids contents between the first slurry and the second slurry is 3.5% or less.

### Claim 11 (depends on 6)

The method for manufacturing an electrode for a secondary battery of claim 6, wherein a difference in viscosity between the first slurry and the second slurry is 3,500 cP or less.

### Claim 12 (depends on 1)

A lithium secondary battery, comprising:
the electrode for a secondary battery of claim 1.