# US 2025/0167212 A1 · Method for producing nickel metal hydride battery, positive electrode for nickel metal hydride batteries, and nickel metal hydride battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0167212 A1
- Document ID: US20250167212A1
- Status: Published application
- Kind: A1
- Application number: 18/730,434
- Filed: 2023-01-24
- Published: 2025-05-22
- Earliest claimed: 2022-01-25
- Assignees: Kabushiki Kaisha Toyota Jidoshokki; Toyota Jidosha Kabushiki Kaisha
- Applicants: Kabushiki Kaisha Toyota Jidoshokki; Toyota Jidosha Kabushiki Kaisha
- Inventors: Hiroyuki SASAKI; Satoshi KONO; Shuhei MOCHIDA; Keisuke SHIRAI; Norifumi YOSHIDA; Yoshifumi ISHIKAWA; Takeo OKANISHI; Daiki TERASHIMA; Masanobu OUCHI; Hiroyuki KAIYA; Motoyoshi OKUMURA; Hiroyuki NAKANO
- Web page: https://patentgrep.com/patent/US20250167212A1

## CPC

- H01M 4/32: Nickel oxide or hydroxide electrodes
- H01M 4/04: Processes of manufacture in general
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/26: Processes of manufacture
- H01M 4/36: Selection of substances as active materials, active masses, active liquids
- H01M 4/366: {as layered products}
- H01M 4/52: of nickel, cobalt or iron
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 4/625: {Carbon or graphite}
- H01M 4/626: {Metals}
- H01M 10/30: Nickel accumulators (H01M10/34 takes precedence)
- H01M 10/345: {Gastight metal hydride accumulators}
- H01M 2004/027: {Negative electrodes}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method for producing a nickel metal hydride battery includes a positive electrode producing step of layering a raw material composition including a positive electrode active material powder containing nickel hydroxide, a cobalt compound, and flake graphite, on a current collector to produce a positive electrode including a positive electrode active material layer in which a graphitization degree is 0.4 or less as measured by Raman spectroscopy. The method further includes a negative electrode producing step of layering a raw material composition including a negative electrode active material powder on a current collector to produce a negative electrode, an electrode body producing step of arranging a separator between the positive electrode and the negative electrode and impregnating the separator with an electrolytic solution to produce an electrode body, and an overdischarging step of charging, overdischarging, and again charging the electrode body.

## Claims

### Claim 1

A method for producing a nickel metal hydride battery, the method comprising:
a positive electrode producing step of layering a raw material composition, the raw material composition including a positive electrode active material powder containing nickel hydroxide, a cobalt compound, and flake graphite, on a current collector to produce a positive electrode including a positive electrode active material layer in which a content of the cobalt compound is less than or equal to 3 mass % and a graphitization degree is less than or equal to 0.4 as measured by Raman spectroscopy;
a negative electrode producing step of layering a raw material composition including a negative electrode active material powder on a current collector to produce a negative electrode;
an electrode body producing step of arranging a separator between the positive electrode and the negative electrode and impregnating the separator with an electrolytic solution to produce an electrode body; and
an overdischarging step of, after charging the electrode body, overdischarging the electrode body, and again charging the electrode body.

### Claim 2 (depends on 1)

The method according to claim 1, wherein in the raw material composition, an average particle size of the flake graphite is greater than or equal to 0.4 times an average particle size of the positive electrode active material powder.

### Claim 3

A positive electrode for a nickel metal hydride battery, the positive electrode comprising:
a current collector; and
a positive electrode active material layer, wherein
the positive electrode active material layer includes a positive electrode active material, a cobalt compound layer covering the positive electrode active material, and flake graphite,
a content of a cobalt compound in the positive electrode active material layer is less than or equal to 3 mass %,
a coverage of the cobalt compound layer on the positive electrode active material is greater than or equal to 50%, and
the positive electrode active material layer has a graphitization degree that is less than or equal to 0.4 as measured by Raman spectroscopy.

### Claim 4 (depends on 3)

The positive electrode according to claim 3, wherein the cobalt compound layer has an average thickness that is less than or equal to 10 nm.

### Claim 5 (depends on 3)

The positive electrode according to claim 3, wherein an average particle size of the flake graphite is greater than or equal to 0.3 times an average particle size of the positive electrode active material.

### Claim 6 (depends on 3)

The positive electrode according to claim 3, wherein a content of the flake graphite in the positive electrode active material layer is greater than or equal to 3 mass % and less than or equal to 10 mass %.

### Claim 7 (depends on 3)

The positive electrode according to claim 3, wherein the cobalt compound layer is further formed on a surface of the flake graphite.

### Claim 8 (depends on 3)

A nickel metal hydride battery, comprising:
the positive electrode according to claim 3.