# US 2025/0167210 A1 · Electrode active material layer, solid-state battery, and production method for electrode active material layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0167210 A1
- Document ID: US20250167210A1
- Status: Published application
- Kind: A1
- Application number: 18/944,415
- Filed: 2024-11-12
- Published: 2025-05-22
- Earliest claimed: 2023-11-17
- Assignees: Toyota Jidosha Kabushiki Kaisha; Panasonic Holdings Corporation
- Applicants: Toyota Jidosha Kabushiki Kaisha; Panasonic Holdings Corporation
- Inventors: Aiko NAGANO; Yasutaka TSUTSUI; Izuru SASAKI
- Web page: https://patentgrep.com/patent/US20250167210A1

## CPC

- H01M 4/139: Processes of manufacture
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/13: Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof
- H01M 4/622: {being polymers}
- H01M 10/0562: Solid materials
- H01M 10/0585: of accumulators having only flat construction elements, i.e. flat positive electrodes, flat negative electrodes and flat separators
- H01M 2300/0068: inorganic
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

An electrode active material layer in the present disclosure contains an electrode active material and a binder, and the ratio of a binder area fraction of a solid electrolyte layer side to a binder area fraction of a current collector side is 55 area % or more. A solid-state battery in the present disclosure includes a current collector, the electrode active material layer in the present disclosure, and a solid electrolyte layer, in this order. A method in the present disclosure for producing the electrode active material layer includes (a) providing an electrode composite material slurry containing the binder and others, (b) forming a preparatory electrode active material layer by coating the current collector with the slurry, (c) drying the preparatory electrode active material layer at a temperature lower than 100° C., and (d) further drying the dried preparatory electrode active material layer at a temperature of 140° C. or higher.

## Claims

### Claim 1

An electrode active material layer for a solid-state battery, the electrode active material layer being interposed between a current collector and a solid electrolyte layer,
the electrode active material layer containing an electrode active material and a binder, wherein
a ratio of a binder area fraction of a side of the solid electrolyte layer to a binder area fraction of a side of the current collector is 55 area % or more.

### Claim 2 (depends on 1)

The electrode active material layer according to claim 1, wherein a ratio of the binder area fraction of the side of the solid electrolyte layer to a binder volume fraction is 30% or more.

### Claim 3 (depends on 1)

The electrode active material layer according to claim 1, wherein the binder is a styrene-butadiene rubber binder.

### Claim 4 (depends on 1)

A solid-state battery comprising:
a current collector;
a solid electrolyte layer; and
the electrode active material layer according to claim 1, the electrode active material layer being interposed between the current collector and the solid electrolyte layer.

### Claim 5 (depends on 1)

A production method for the electrode active material layer according to claim 1, the production method comprising:
(a) providing an electrode composite material slurry that contains the electrode active material, the binder, and a dispersion medium;
(b) forming a preparatory electrode active material layer by coating the current collector with the slurry;
(c) drying the preparatory electrode active material layer at a temperature lower than 100° C.; and
(d) further drying the preparatory electrode active material layer dried at the temperature lower than 100° C., at a temperature of 140° C. or higher.