# US 2025/0167105 A1 · Semiconductor device and method of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0167105 A1
- Document ID: US20250167105A1
- Status: Published application
- Kind: A1
- Application number: 18/518,415
- Filed: 2023-11-22
- Published: 2025-05-22
- Earliest claimed: 2023-11-22
- Assignees: Nanya Technology Corporation
- Inventors: Chun-Heng WU
- Web page: https://patentgrep.com/patent/US20250167105A1

## CPC

- H10W 20/42: Vias, e.g. via plugs
- H10W 20/033: {in openings in dielectrics}
- H10W 20/056: {by filling conductive material into holes, grooves or trenches}
- H10W 20/082: {the openings being tapered via holes}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A semiconductor device includes a landing pad, a first nitride layer, a first oxide layer, a second nitride layer, a third nitride layer, an electrode layer, and a filling material. The landing pad, the first nitride layer, the first oxide layer, the second nitride layer, and the third nitride layer are sequentially formed. A trench runs through the third nitride layer, the second oxide layer, the second nitride layer, the first oxide layer, and the first nitride layer. The electrode layer is disposed on an inner sidewall of the trench, a top surface of the third nitride layer, and a top surface and a sidewall of the landing pad. The filling material is filled in the trench and contacts the landing pad by the electrode layer.

## Claims

### Claim 1

A semiconductor device, comprising:
a landing pad;
a first nitride layer disposed over the landing pad;
a first oxide layer disposed on the first nitride layer;
a second nitride layer disposed on the first oxide layer;
a second oxide layer disposed on the second nitride layer;
a third nitride layer disposed on the second oxide layer and a trench running through the third nitride layer, the second oxide layer, the second nitride layer, the first oxide layer, and the first nitride layer, wherein the trench further has an expanding portion through the first nitride layer, and a width of a top of the expanding portion of the trench is equal to or greater than a width of a top of the trench;
an electrode layer disposed on an inner sidewall of the trench, a top surface of the third nitride layer, and a top surface and a sidewall of the landing pad; and
a filling material filled in the trench and contacting the landing pad by the electrode layer.

### Claim 2 (depends on 1)

The semiconductor device of claim 1, wherein the filling material contacts the top surface and the sidewall of the landing pad by the electrode layer.

### Claim 3 (depends on 1)

The semiconductor device of claim 1, wherein the expanding portion of the trench is located over the landing pad.

### Claim 4 (depends on 1)

The semiconductor device of claim 1, wherein a width of the expanding portion of the trench tapers downward from a top surface of the first nitride layer to a top surface of the landing pad.

### Claim 5 (depends on 1)

The semiconductor device of claim 1, wherein the width of the top of the expanding portion of the trench is greater than a width of a bottom of the expanding portion of the trench.

### Claim 6 (depends on 1)

The semiconductor device of claim 1, wherein the width of the top of the expanding portion of the trench is greater than the width of the top of the trench.

### Claim 7 (depends on 1)

The semiconductor device of claim 1, wherein a height from a top surface of the first nitride layer to a top surface of the landing pad is in a range between 20 nanometers and 25 nanometers.

### Claim 8 (depends on 1)

The semiconductor device of claim 1, wherein the first oxide layer comprises borophosphosilicate glass.

### Claim 9 (depends on 1)

The semiconductor device of claim 1, wherein the second oxide layer comprises tetraethyl orthosilicate.

### Claim 10

A method of manufacturing a semiconductor device, comprising:
sequentially forming a landing pad, a first nitride layer, a first oxide layer, a second nitride layer, a second oxide layer, and a third nitride layer;
forming a trench running through the third nitride layer, the second oxide layer, the second nitride layer, and the first oxide layer;
depositing a protective liner layer on surfaces of the first nitride layer, the second nitride layer, and the third nitride layer;
punching through the first nitride layer and exposing the landing pad;
etching the first nitride layer and exposing a sidewall of the landing pad;
removing the protective liner layer;
depositing an electrode layer on an inner surface of the trench and a top surface of the third nitride layer; and
depositing a filling material to fill the trench.

### Claim 11 (depends on 10)

The method of claim 10, wherein forming the trench is performed such that the first nitride layer is exposed.

### Claim 12 (depends on 10)

The method of claim 10, wherein depositing the protective liner layer is performed such that the protective liner layer contacts a top surface of the first nitride layer.

### Claim 13 (depends on 10)

The method of claim 10, wherein punching through the first nitride layer and exposing the landing pad are performed such that a portion of the protective liner layer on a top surface of the first nitride layer and a portion of the protective liner layer on a top surface of the third nitride layer are removed.

### Claim 14 (depends on 10)

The method of claim 10, wherein etching the first nitride layer and exposing the sidewall of the landing pad are performed after punching through the first nitride layer and exposing the landing pad.

### Claim 15 (depends on 10)

The method of claim 10, wherein etching the first nitride layer and exposing the sidewall of the landing pad are performed such that an expanding portion of the trench is formed, and wherein the expanding portion of the trench runs through the first nitride layer.

### Claim 16 (depends on 15)

The method of claim 15, wherein etching the first nitride layer and exposing the sidewall of the landing pad are performed such that the expanding portion of the trench is connected between the landing pad and a top surface of the first nitride layer.

### Claim 17 (depends on 15)

The method of claim 15, wherein etching the first nitride layer and exposing the sidewall of the landing pad are performed such that a width of a top of the expanding portion of the trench is greater than a width of a bottom of the expanding portion of the trench.

### Claim 18 (depends on 17)

The method of claim 17, wherein etching the first nitride layer and exposing the sidewall of the landing pad are performed such that the width of the top of the expanding portion of the trench is equal to or greater than a width of a top of the trench.

### Claim 19 (depends on 10)

The method of claim 10, wherein depositing the electrode layer is performed such that the electrode layer contacts a top surface and a sidewall of the landing pad.

### Claim 20 (depends on 10)

The method of claim 10, wherein a thickness of the protective liner layer is equal to or greater than 2 nanometers, and wherein the protective liner layer comprises silicon oxynitride.