# US 2025/0167047 A1 · Method of Forming Contact Metal

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0167047 A1
- Document ID: US20250167047A1
- Status: Published application
- Kind: A1
- Application number: 19/027,412
- Filed: 2025-01-17
- Published: 2025-05-22
- Earliest claimed: 2016-03-08
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Co., Ltd.
- Inventors: Chun-Hsien Huang; Wei-Jung Lin; Hsien-Lung Yang; Yu-Kai Chen; Hong-Mao Lee
- Web page: https://patentgrep.com/patent/US20250167047A1

## CPC

- H10W 20/0698: {Local interconnections}
- H10D 30/0212: {using self-aligned silicidation}
- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 30/6211: {having fin-shaped semiconductor bodies integral with the bulk semiconductor substrates}
- H10D 30/6219: {characterised by the source or drain electrodes}
- H10D 84/017: {Manufacturing their source or drain regions, e.g. silicided source or drain regions}
- H10D 84/0186: {Manufacturing their interconnections or electrodes, e.g. source or drain electrodes}
- H10D 84/0193: {the components including FinFETs}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10W 20/033: {in openings in dielectrics}
- H10W 20/066: {by forming silicides of refractory metals}
- H10W 20/083: {the openings being via holes penetrating underlying conductors}
- H10W 20/084: {for dual-damascene structures}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A semiconductor device is disclosed. The device includes a source/drain feature formed over a substrate. A dielectric layer formed over the source/drain feature. A contact trench formed through the dielectric layer to expose the source/drain feature. A titanium nitride (TiN) layer deposited in the contact trench and a cobalt layer deposited over the TiN layer in the contact trench.

## Claims

### Claim 1

A method comprising:
forming a source/drain contact opening that exposes an epitaxial source/drain;
forming a titanium silicide layer on the exposed epitaxial source/drain; and
forming a source/drain contact in the source/drain contact opening, wherein the forming the source/drain contact in the source/drain contact opening includes:
forming a titanium nitride layer that lines sidewalls and a bottom of the source/drain contact opening, and
forming a cobalt plug on the titanium nitride layer, wherein the titanium nitride layer wraps the cobalt plug and the titanium nitride layer is disposed between the cobalt plug and the titanium silicide layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the forming the titanium silicide layer includes:
depositing a titanium layer on the exposed epitaxial source/drain; and
performing an annealing process, wherein the titanium layer reacts with the epitaxial source/drain to form the titanium silicide layer.

### Claim 3 (depends on 2)

The method of claim 2, further comprising depositing the titanium layer on the exposed epitaxial source/drain by chemical vapor deposition or physical vapor deposition.

### Claim 4 (depends on 1)

The method of claim 1, wherein the forming the titanium nitride layer includes depositing the titanium nitride layer by atomic layer deposition (ALD).

### Claim 5 (depends on 4)

The method of claim 4, wherein the titanium nitride layer includes oxygen, and the method further includes tuning parameters of the ALD to provide the titanium nitride layer with a ratio of oxygen to titanium (O/Ti) that is less than 0.5.

### Claim 6 (depends on 4)

The method of claim 4, wherein the method further includes tuning parameters of the ALD to provide the titanium nitride layer with a thickness that is less than 30 angstroms.

### Claim 7 (depends on 4)

The method of claim 4, wherein the method further includes tuning parameters of the ALD to provide the titanium nitride layer with a density of about 4.75 g/cm3.

### Claim 8 (depends on 4)

The method of claim 4, wherein the forming the titanium nitride layer includes using a tetrakis(dimethylamino) titanium (TDMAT) precursor, a process temperature from 200° C. to 450° C., and a deposition pressure from 0.5 torr to 10 torr.

### Claim 9 (depends on 1)

The method of claim 1, wherein the forming the cobalt plug includes:
forming a cobalt seed layer by atomic layer deposition (ALD); and
forming a bulk cobalt layer by physical vapor deposition (PVD) over the cobalt seed layer.

### Claim 10

A method comprising:
forming a silicon-comprising source/drain;
forming a source/drain contact over the silicon-comprising source/drain, wherein the source/drain contact includes:
a cobalt-comprising bulk layer, and
a titanium-and-nitrogen comprising layer that forms a first sidewall of the source/drain contact, a second sidewall of the source/drain contact, and a bottom of the source/drain contact, wherein the cobalt-comprising bulk layer is disposed on the titanium-and-nitrogen comprising layer; and
forming a metal-and-silicon comprising layer between the bottom of the source/drain contact and the silicon-comprising source/drain, wherein a metal of the metal-and-silicon comprising layer is different than cobalt.

### Claim 11 (depends on 10)

The method of claim 10, wherein the metal is titanium and the metal-and-silicon comprising layer is a titanium-and-silicon comprising layer.

### Claim 12 (depends on 10)

The method of claim 10, further comprising depositing the titanium-and-nitrogen comprising layer by atomic layer deposition (ALD), wherein the titanium-and-nitrogen comprising layer further includes oxygen and the method includes tuning ALD parameters to provide the titanium-and-nitrogen comprising layer with a ratio of oxygen to titanium that is less than 0.5.

### Claim 13 (depends on 12)

The method of claim 12, wherein the ALD is a first ALD and the method further includes forming the cobalt-comprising bulk layer by depositing a first cobalt layer by a second ALD and depositing a second cobalt layer by physical vapor deposition (PVD).

### Claim 14 (depends on 10)

The method of claim 10, further comprising forming a source/drain contact opening in a dielectric layer, wherein the source/drain contact and the metal-and-silicon comprising layer are formed in the source/drain contact opening.

### Claim 15

A method comprising:
forming an epitaxial source/drain structure on a portion of a substrate, wherein the epitaxial source/drain structures is disposed between a first gate and a second gate; and
forming a source/drain contact structure on the epitaxial source/drain structure, wherein the source/drain contact structure includes:
a silicide layer abutting the epitaxial source/drain structure, wherein the silicide layer includes a first metal and silicon,
a contact bulk layer that includes cobalt, and
a single contact adhesion layer disposed on sidewalls and a bottom of the contact bulk layer, wherein the single contact adhesion layer includes a second metal and nitrogen, wherein the second metal is the same as the first metal.

### Claim 16 (depends on 15)

The method of claim 15, wherein the forming the source/drain contact structure on the epitaxial source/drain structure includes:
depositing a metal layer on the epitaxial source/drain structure;
depositing a metal nitride layer on the metal layer, wherein the metal layer includes the first metal and the metal nitride layer includes the second metal;
performing an annealing process that causes the metal layer to react with the epitaxial source/drain structure to form the silicide layer;
depositing a cobalt plug material over the metal nitride layer; and
performing a chemical mechanical polishing that removes a portion of the cobalt plug material and a portion of the metal nitride layer, wherein a remaining portion of the cobalt plug material forms the contact bulk layer and a remaining portion of the metal nitride layer forms the single contact adhesion layer.

### Claim 17 (depends on 16)

The method of claim 16, wherein the depositing the metal nitride layer includes using a tetrakis(dimethylamino) titanium precursor.

### Claim 18 (depends on 16)

The method of claim 16, wherein the depositing the metal nitride layer includes using a titanium tetrachloride precursor.

### Claim 19 (depends on 15)

The method of claim 15, wherein the first metal and the second metal are titanium.

### Claim 20 (depends on 15)

The method of claim 15, wherein the first gate and the epitaxial source/drain structure form a portion of a fin-like field effect transistor (FinFET).