# US 2025/0166989 A1 · Thermal film deposition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0166989 A1
- Document ID: US20250166989A1
- Status: Published application
- Kind: A1
- Application number: 18/840,453
- Filed: 2023-02-21
- Published: 2025-05-22
- Earliest claimed: 2022-02-22
- Assignees: Lam Research Corporation
- Applicants: Lam Research Corporation
- Inventors: Jason Alexander Varnell; Dustin Zachary Austin; Praneeth Ramasagaram; Bart J. van Schravendijk; Jennifer Leigh Petraglia; Douglas Walter Agnew; Awnish Gupta; Pei-Chi Liu; Pulkit Agarwal
- Web page: https://patentgrep.com/patent/US20250166989A1

## CPC

- C23C 16/45523: {Pulsed gas flow or change of composition over time}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- C23C 16/30: Deposition of compounds, mixtures or solid solutions, e.g. borides, carbides, nitrides
- C23C 16/401: {containing silicon}
- C23C 16/45536: {Use of plasma, radiation or electromagnetic fields}
- C23C 16/56: After-treatment
- H10P 14/6334: {using decomposition or reaction of gaseous or vapour phase compounds, i.e. chemical vapour deposition (deposition by physical ablation of a target H10P14/6329)}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/6519: {the substance being oxygen}
- H10P 14/6522: {introduced into a nitride material, e.g. changing SiN to SiON}
- H10P 14/6524: {the substance being nitrogen}
- H10P 14/6529: {by exposure to a gas or vapour}
- H10P 14/6532: {by exposure to a plasma}
- H10P 14/6682: {the compound being a silane, e.g. disilane, methylsilane or chlorosilane}
- H10P 14/6687: {the compound comprising silicon and nitrogen}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 14/6922: {the material containing Si, O and at least one of H, N, C, F or other non-metal elements, e.g. SiOC, SiOC:H or SiONC}
- H10P 14/6927: {the material being a silicon oxynitride, e.g. SiON or SiON:H}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Methods and apparatuses for depositing superconformal dielectric material using thermal chemical vapor deposition-enhanced atomic layer deposition are provided. Methods and apparatuses for depositing material using modified atomic layer deposition integrating pyrolyzing a deposition precursor such as an aminosilane during dose to form a pyrolyzed layer, optional inert gas plasma for densification, and an oxygen-containing or nitrogen-containing plasma to convert the pyrolyzed layer into an oxygen-containing or nitrogen-containing material.

## Claims

### Claim 1

A method for processing substrates, the method comprising:
pyrolyzing a deposition precursor on a surface of a substrate to form a pyrolyzed film; and
exposing the pyrolyzed film to a first plasma to form a deposited film.

### Claim 2 (depends on 1)

The method of claim 1, wherein the pyrolyzing is performed by heating the substrate to a temperature sufficient to cause pyrolysis of the deposition precursor; and exposing the surface of the substrate to the deposition precursor.

### Claim 3 (depends on 1)

The method of claim 1, wherein the pyrolyzing and the exposing of the pyrolyzed film are performed in a process chamber having a chamber pressure of about 10 Torr to about 60 Torr.

### Claim 4 (depends on 1)

The method of claim 1, wherein exposing the pyrolyzed film to the first plasma comprises exposing the pyrolyzed film to an inert gas plasma and then exposing the pyrolyzed film to an oxygen-containing or nitrogen-containing plasma.

### Claim 5

A method for processing substrates, the method comprising:
setting a temperature of a heatable pedestal holding a substrate to a first temperature;
exposing the substrate to a deposition precursor having a pyrolysis temperature that is less than the substrate temperature while the pedestal is heated to the first temperature in a plasma-free environment;
stopping exposure of the deposition precursor; and
after stopping exposure of the deposition precursor, exposing the substrate to a first plasma to form a deposited film.

### Claim 6 (depends on 1)

The method of claim 1, wherein the deposition precursor is di(isopropylamino)silane or bis(tertiarybutylamino)silane.

### Claim 7 (depends on 1)

The method of claim 1, further comprising exposing the pyrolyzed film to a second plasma.

### Claim 8 (depends on 1)

The method of claim 1, wherein the first plasma is generated by igniting an inert gas and the deposited film is densified.

### Claim 9

(canceled)

### Claim 10

A method of processing a substrate, the method comprising:
(a) introducing a deposition precursor to a process chamber housing the substrate;
(b) introducing a plasma to the process chamber, the plasma being generated from igniting a reactant to form a reactant plasma ambient in the process chamber; and
(c) while the reactant plasma ambient is in the process chamber, introducing the deposition precursor to the process chamber to form at least a partial film on the substrate.