# US 2025/0166898 A1 · Capacitor and method of manufacturing thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0166898 A1
- Document ID: US20250166898A1
- Status: Published application
- Kind: A1
- Application number: 18/515,291
- Filed: 2023-11-21
- Published: 2025-05-22
- Earliest claimed: 2023-11-21
- Assignees: Nanya Technology Corporation
- Applicants: Nanya Technology Corporation
- Inventors: Chih-Chun HSIAO; Ji-Feng LIU
- Web page: https://patentgrep.com/patent/US20250166898A1

## CPC

- H01G 4/008: Selection of materials
- H01G 4/1209: {characterised by the ceramic dielectric material (H01G4/1272, H01G4/1281 take precedence)}
- H01G 4/33: Thin- or thick-film capacitors {(thin- or thick-film circuits; capacitors without a potential-jump or surface barrier specially adapted for integrated circuits, details thereof, multistep manufacturing processes therefor)}
- H01G 4/38: Multiple capacitors, i.e. structural combinations of fixed capacitors
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)

## Abstract

A method of manufacturing a capacitor includes forming a bottom electrode layer; forming an insulator on the bottom electrode layer; crystallizing the insulator; and forming a top electrode layer on the crystallized insulator. As such, the leakage problem due to thinner top electrode layer and smaller critical dimension of the capacitor can be reduced. In addition, possibility for the capacitors to collapse is reduced, and the electrical performance of the capacitor won't be affected by the collapse problem.

## Claims

### Claim 1

A method of manufacturing a capacitor, comprising:
forming a bottom electrode layer;
forming an insulator on the bottom electrode layer;
crystallizing the insulator; and
forming a top electrode layer on the crystallized insulator.

### Claim 2 (depends on 1)

The method of manufacturing the capacitor of claim 1, wherein the step of crystallizing the insulator is performed through an anneal treatment.

### Claim 3 (depends on 1)

The method of manufacturing the capacitor of claim 1, wherein the step of crystallizing the insulator is performed before the step of forming the top electrode layer.

### Claim 4 (depends on 1)

The method of manufacturing the capacitor of claim 1, further comprising:
forming an oxide diffusion barrier layer between the insulator and the top electrode layer.

### Claim 5 (depends on 4)

The method of manufacturing the capacitor of claim 4, wherein the oxide diffusion barrier layer comprises titanium oxynitride.

### Claim 6 (depends on 1)

The method of manufacturing the capacitor of claim 1, wherein the bottom electrode layer comprises titanium silicon nitride.

### Claim 7 (depends on 1)

The method of manufacturing the capacitor of claim 1, wherein a temperature of the step of crystallizing the insulator is in a range from 400 degrees to 600 degrees.

### Claim 8 (depends on 1)

The method of manufacturing the capacitor of claim 1, wherein a time period of the step of crystallizing the insulator is in a range from 30 seconds to 100 seconds.

### Claim 9 (depends on 1)

The method of manufacturing the capacitor of claim 1, wherein a time period of the step of crystallizing the insulator is shorter than a time period of the step of forming the top electrode layer.

### Claim 10

A method of manufacturing a capacitor, comprising:
forming a bottom electrode layer;
forming an insulator on the bottom electrode layer;
forming a titanium oxynitride layer on the insulator; and
forming a top electrode layer on the insulator.

### Claim 11 (depends on 10)

The method of manufacturing the capacitor of claim 10, further comprising:
performing an anneal treatment to the insulator.

### Claim 12 (depends on 11)

The method of manufacturing the capacitor of claim 11, wherein the anneal treatment is performed before forming the top electrode layer.

### Claim 13 (depends on 11)

The method of manufacturing the capacitor of claim 11, wherein a temperature of the step of performing the anneal treatment is in a range from 400 degrees to 600 degrees.

### Claim 14 (depends on 11)

The method of manufacturing the capacitor of claim 11, wherein a time period of the step of performing the anneal treatment is in a range from 30 seconds to 100 seconds.

### Claim 15

A capacitor, comprising:
a bottom electrode layer;
an insulator disposed on the bottom electrode layer;
an oxide diffusion barrier layer disposed on the insulator; and
a top electrode layer disposed on the oxide diffusion barrier layer.

### Claim 16 (depends on 15)

The capacitor of claim 15, wherein the top electrode layer comprises titanium nitride, and the oxide diffusion barrier layer comprises titanium oxynitride.

### Claim 17 (depends on 15)

The capacitor of claim 15, wherein the bottom electrode layer comprises titanium silicon nitride.

### Claim 18 (depends on 15)

The capacitor of claim 15, wherein a material of the bottom electrode layer is different form a material of the top electrode layer.

### Claim 19 (depends on 15)

The capacitor of claim 15, wherein the bottom electrode layer has higher mechanical strength than the top electrode layer.

### Claim 20 (depends on 15)

The capacitor of claim 15, wherein an oxygen concentration of the oxide diffusion barrier layer is higher than the top electrode layer.