# US 2025/0166889 A1 · Method for co-sintering transformer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0166889 A1
- Document ID: US20250166889A1
- Status: Published application
- Kind: A1
- Application number: 18/511,925
- Filed: 2023-11-16
- Published: 2025-05-22
- Earliest claimed: 2023-11-16
- Assignees: Tai-Tech Advanced Electronics Co., Ltd.
- Applicants: Tai-Tech Advanced Electronics Co., Ltd.
- Inventors: Ming-Yen Hsieh; Pao-Lin Shen; Hsiang-Chung Yang; Jian-Hong Lai; Kuan-Yi Lu
- Web page: https://patentgrep.com/patent/US20250166889A1

## CPC

- H01F 27/2847: {Sheets; Strips (H01F27/2866 takes precedence)}
- H01F 41/02: for manufacturing cores, coils, or magnets (H01F41/14 takes precedence; for dynamo-electric machines H02K15/00)
- H01F 1/22: pressed, sintered, or bound together
- H01F 27/255: made from particles (H01F27/26 takes precedence)
- H01F 27/306: {Fastening or mounting coils or windings on core, casing or other support}
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES

## Abstract

The method for co-sintering transformer includes the following steps: a preparation step providing a copper conductor strip and an iron core; a coating step applying a layer of nickel coating, or a layer of precious metal coating, or both on the copper conductor strip from the preparation step; an assembly step putting the copper conductor strip from the coating step and the iron core from the preparation step together to form a transformer; a pressing step pressing the assembled copper conductor strip and the iron core from the assembly step, together with iron power, in a mold into an integrally formed transformer; and a sintering step sintering the pressed transformer from the pressing step in an atmospheric environment. The present method is able to conduct sintering directly under the atmospheric environment without reducing oxygen content. Iron powder also exhibits improved characteristics after sintering in the atmospheric environment.

## Claims

### Claim 1

A method for co-sintering transformer, comprising:
preparation step: providing a copper conductor strip and an iron core;
coating step: applying a layer of nickel coating or a layer of precious metal coating, or first a layer of nickel coating and then a layer of precious metal coating on the copper conductor strip from the preparation step;
assembly step: putting the copper conductor strip from the coating step and the iron core from the preparation step together into a transformer;
pressing step: placing the assembled copper conductor strip and the iron core from the assembly step into a mold, filling iron power into the mold, and producing an integrally formed transformer by pressing; and
sintering step: sintering the pressed transformer from the pressing step in an atmospheric environment.

### Claim 2 (depends on 1)

The method for co-sintering transformer according to claim 1, wherein the atmospheric environment for the sintering step is an environment with an oxygen content of 21%.

### Claim 3 (depends on 1)

The method for co-sintering transformer according to claim 1, wherein the sintering step is conducted at a temperature 600˜900° C.

### Claim 4 (depends on 1)

The method for co-sintering transformer according to claim 1, wherein the sintering step is conducted for a duration 0.5˜3 hours.

### Claim 5 (depends on 1)

The method for co-sintering transformer according to claim 1, wherein the thickness of the nickel coating is 0.1˜20 μm.

### Claim 6 (depends on 1)

The method for co-sintering transformer according to claim 1, wherein the precious metal coating is made of gold with a thickness of 0.1˜1 μm.

### Claim 7 (depends on 1)

The method for co-sintering transformer according to claim 1, wherein the precious metal coating is made of silver with a thickness of 0.1˜10 μm.

### Claim 8 (depends on 1)

The method for co-sintering transformer according to claim 1, wherein the precious metal coating is made of platinum with a thickness of 0.1˜1 μm.