# US 2025/0164887 A1 · Process environment for inorganic resist patterning

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0164887 A1
- Document ID: US20250164887A1
- Status: Published application
- Kind: A1
- Application number: 19/032,836
- Filed: 2025-01-21
- Published: 2025-05-22
- Earliest claimed: 2020-03-02
- Assignees: Inpria Corporation
- Applicants: Inpria Corporation
- Inventors: Alan J. Telecky; Jason K. Stowers; Douglas A. Keszler; Stephen T. Meyers; Peter De Schepper; Sonia Castellanos Ortega; Michael Greer; Kirsten Louthan
- Web page: https://patentgrep.com/patent/US20250164887A1

## CPC

- G03F 7/38: Treatment before imagewise removal, e.g. prebaking {(G03F7/265 takes precedence)}
- G03F 7/0042: {with inorganic or organometallic light-sensitive compounds not otherwise provided for, e.g. inorganic resists (G03F7/075 takes precedence)}
- G03F 7/168: {Finishing the coated layer, e.g. drying, baking, soaking}
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

The processing of radiation patternable organometallic coatings is shown to be improved through the appropriate selection of post processing conditions between coating and development of the pattern. In particular, a coated wafer can be subjected to process delays to allow aging of the coating at various process points, in particular following irradiation. Process delays can be combined and interspersed with heating steps. The atmosphere above the coated wafer at various process steps can be adjusted to obtain desired improvements in the development of the pattern. Reactive gases can be beneficial with respect to improvement of coating properties.

## Claims

### Claim 1

A method for developing a radiation exposed organometallic patterning layer with irradiated and non-irradiated portions, the method comprising
exposing the radiation exposed organometallic patterning layer to a first temperature in a range from about 45° C. to about 250° C. and a first atmosphere to form a baked patterned layer; and
exposing the baked patterned layer to a second temperature in a range from about 45° C. to about 250° C. and a second atmosphere, wherein the second temperature is different from the first temperature and/or the second atmosphere is different from the first atmosphere,
wherein the organometallic patterning layer comprises an organometallic oxide/hydroxide network.

### Claim 2 (depends on 1)

The method of claim 1 wherein the first atmosphere comprises a reactive gas.

### Claim 3 (depends on 1)

The method of claim 1 wherein the second atmosphere comprises an inert gas.

### Claim 4 (depends on 3)

The method of claim 3 wherein the second atmosphere comprises nitrogen gas.

### Claim 5 (depends on 1)

The method of claim 1 wherein the first temperature is in a range from 50° C. to about 150° C.

### Claim 6 (depends on 1)

The method of claim 1 wherein the second temperature is in a range from about 95° C. to about 250° C.

### Claim 7 (depends on 3)

The method of claim 3 wherein the first atmosphere comprises air.

### Claim 8 (depends on 3)

The method of claim 3 wherein the first atmosphere comprises water vapor.

### Claim 9 (depends on 3)

The method of claim 3 wherein the first atmosphere comprises oxygen.

### Claim 10 (depends on 3)

The method of claim 3 wherein the first atmosphere comprises carbon dioxide.

### Claim 11 (depends on 3)

The method of claim 3 wherein the first atmosphere comprises oxygen and water vapor.

### Claim 12 (depends on 3)

The method of claim 3 wherein the first atmosphere comprises oxygen and carbon dioxide.

### Claim 13 (depends on 1)

The method of claim 1 wherein the radiation exposed organometallic patterning layer comprises an organo tin oxide hydroxide having Sn—C bonds.

### Claim 14 (depends on 13)

The method of claim 13 wherein the radiation exposed organometallic patterning layer comprises a monoalkyltin oxide hydroxide.

### Claim 15 (depends on 1)

The method of claim 1 wherein the method results in an increase of a contrast in development rate between the irradiated portion and the non-irradiated portion.

### Claim 16

A method for improving the processing of radiation patternable organo tin-based coatings on a wafer having a thickness from about 1 nm to about 500 nm, the method comprising:
following irradiation, storing the wafer with the coating to age prior to pattern development in an oxygen containing atmosphere; and
following storing, contacting the wafer with an inert gas atmosphere.

### Claim 17 (depends on 16)

The method of claim 16 wherein storing the wafer comprises exposing the coating to a first temperature in a range from about 30° C. to about 150° C. and contacting the wafer comprises exposing the coating to a second temperature in a range from about 45° C. to about 250° C., and wherein the second temperature is different from the first temperature.

### Claim 18 (depends on 16)

The method of claim 16 wherein the oxygen containing atmosphere comprises oxygen and water vapor.

### Claim 19

A method for improving the processing of a radiation patternable organo tin-based coating comprising organo tin oxide hydroxide having Sn—C bonds, wherein the coating has a thickness from about 1 nm to about 500 nm, the method comprising:
contacting the wafer with the organo tin oxide hydroxide coating, following irradiation and development to form a developed pattern, to a first atmosphere comprising a reactive gas to alter the tin-bound ligands in the developed pattern, wherein the reactive gas comprises oxygen; and
following contacting the wafer to the first atmosphere, contacting the wafer to an inert gas atmosphere.

### Claim 20 (depends on 19)

The method of claim 19 wherein contacting the wafer to the first atmosphere comprises exposing the wafer to a first temperature and contacting the wafer to the inert gas atmosphere comprises exposing the coating to a second temperature, wherein the first temperature and the second temperature are in a range from about 100° C. to about 500° C., and wherein the second temperature is different from the first temperature.

### Claim 21 (depends on 19)

The method of claim 19 wherein the oxygen containing atmosphere comprises oxygen and water vapor.