- Filed: 2024-07-16
- Published: 2025-05-22
- Earliest claimed: 2023-11-20
- Assignees: Samsung Electronics Co., Ltd.
- Applicants: Samsung Electronics Co., Ltd.
- Inventors: Jiho PARK; Hun KIM; Sora PARK; Hyungkeun YOO; Younghun KWON; Jongchul KIM; Jaeyoung YANG; Chihoon LEE
- Web page: https://patentgrep.com/patent/US20250164872A1

## CPC

- G03F 1/84: Inspecting
- G03F 7/2002: {with visible light or UV light, through an original having an opaque pattern on a transparent support, e.g. film printing, projection printing; by reflection of visible or UV light from an original such as a printed image}
- G06T 7/0004: {Industrial image inspection}
- G06T 7/60: Analysis of geometric attributes
- G06T 2207/20212: Image combination
- G06T 2207/30148: Semiconductor; IC; Wafer
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- G06T: IMAGE DATA PROCESSING OR GENERATION, IN GENERAL

## Abstract

A semiconductor structure inspection method includes obtaining an image of a semiconductor structure, the semiconductor structure including a wafer, a semiconductor layer, and an inspection pattern, determining a material of an insertion layer to be inserted in the semiconductor structure, determining a thickness of the insertion layer, inserting the insertion layer having the determined material and the determined thickness in the semiconductor structure, and measuring the semiconductor structure having the insertion layer inserted therein.

## Claims

### Claim 1

A semiconductor structure inspection method comprising:
obtaining an image of a semiconductor structure, the semiconductor structure comprising a wafer, a semiconductor layer, and an inspection pattern;
determining a material of an insertion layer to be inserted in the semiconductor structure;
determining a thickness of the insertion layer;
inserting the insertion layer having the determined material and the determined thickness in the semiconductor structure; and
measuring the semiconductor structure having the insertion layer inserted therein.

### Claim 2 (depends on 1)

The semiconductor structure inspection method of claim 1, wherein the obtaining of the image of the semiconductor structure comprises measuring the inspection pattern.

### Claim 3 (depends on 1)

The semiconductor structure inspection method of claim 1, wherein the determining of the material of the insertion layer comprises determining the material of the insertion layer based on a refractive index and an absorption coefficient of the insertion layer.

### Claim 4 (depends on 1)

The semiconductor structure inspection method of claim 1, wherein the determining of the thickness of the insertion layer comprises:
obtaining a plurality of patch images at a plurality of wavelengths;
combining the plurality of patch images; and
determining a signal-to-noise ratio (SNR) corresponding to the combined plurality of patch images.

### Claim 5 (depends on 4)

The semiconductor structure inspection method of claim 4, wherein the combining of the plurality of patch images comprises combining the obtained plurality of patch images by assigning weights to the respective light intensities of the plurality of patch images.

### Claim 6 (depends on 4)

The semiconductor structure inspection method of claim 4, wherein the determining of the SNR is performed by:
dividing a difference image into a first region having a first difference in light intensity and a second region having a second difference in light intensity that is less than the first difference in light intensity; and
comparing a value of light intensity of the first region relative to a value of light intensity of the second region,
wherein the difference image is an image corresponding to a difference between a defect image and a normal image,
wherein the defect image is a combined patch image comprising at least one defect, and
wherein the normal image is a combined patch image that does not comprise a defect.

### Claim 7 (depends on 1)

The semiconductor structure inspection method of claim 1, wherein a wavelength band for measuring the semiconductor structure is selected based on a location corresponding to a placement of the inspection pattern, a size of the inspection pattern, and a surrounding material adjacent to the inspection pattern.

### Claim 8

An extreme ultraviolet (EUV) mask inspection method comprising:
forming a photoresist layer on a wafer and a semiconductor layer of a semiconductor structure;
forming a photoresist pattern by exposing the photoresist layer using an EUV mask;
obtaining an image of the photoresist pattern;
determining a material of an insertion layer to be inserted in the semiconductor structure;
determining a thickness of the insertion layer;
inserting the insertion layer in the semiconductor structure; and
determining whether the EUV mask is defective by measuring the photoresist pattern with the insertion layer having the determined material and the determined thickness inserted in the semiconductor structure.

### Claim 9 (depends on 8)

The EUV mask inspection method of claim 8, wherein the obtaining of the image of the photoresist pattern comprises measuring dimensions of the photoresist pattern.

### Claim 10 (depends on 8)

The EUV mask inspection method of claim 8, wherein the determining of the material of the insertion layer is performed by measuring, by a measurement device, the insertion layer while the insertion layer is inserted in the semiconductor structure.

### Claim 11 (depends on 8)

The EUV mask inspection method of claim 8, wherein the determining of the thickness of the insertion layer comprises obtaining a plurality of patch images by performing a simulation for a plurality of wavelengths, with the insertion layer inserted between the wafer and the photoresist pattern.

### Claim 12 (depends on 8)

The EUV mask inspection method of claim 8, wherein the determining of the thickness of the insertion layer comprises:
combining the plurality of patch images; and
determining a signal-to-noise ratio (SNR) of each of combined patch images,
wherein the determining of the SNR is performed by:
dividing a difference image into a first region having a first difference in light intensity and a second region having a second difference in light intensity that is less than the first difference in light intensity; and
comparing, for each of the combined patch images, a maximum light intensity of the first region to a maximum light intensity of the second region, and
wherein the difference image is an image corresponding to a difference between a defect image and a normal image,
wherein the defect image is a combined patch image comprising at least one defect, and
wherein the normal image is a combined patch image that does not comprise a defect.

### Claim 13 (depends on 8)

The EUV mask inspection method of claim 8, wherein the insertion layer comprises at least one of silicon nitride (SiN), silicon oxynitride (SiON), titanium nitride (TiN), tungsten (W), gold (Au), photoresist PR, silicon oxycarbide (SiOC), and silicon carbide (SiC).

### Claim 14 (depends on 8)

The EUV mask inspection method of claim 8, wherein the insertion layer is between the semiconductor layer and the photoresist pattern.

### Claim 15 (depends on 8)

The EUV mask inspection method of claim 8, wherein the thickness of the insertion layer is in a range of about 1 nanometer (nm) to about 200 nm.

### Claim 16 (depends on 8)

The EUV mask inspection method of claim 8, wherein the obtaining of the image of the photoresist pattern is performed by a transmission electron microscope (TEM),
wherein the determining of the material of the insertion layer is performed by a spectroscopic ellipsometer, and
wherein the measuring of the photoresist pattern with the insertion layer inserted in the semiconductor structure is performed by an optical microscope.

### Claim 17

An extreme ultraviolet (EUV) lithography method comprising:
providing a semiconductor layer on a wafer;
providing a photoresist layer on the wafer;
exposing the photoresist layer on the wafer using an EUV mask;
forming a photoresist pattern by developing the exposed photoresist layer; and
determining whether the EUV mask is defective by inspecting the photoresist pattern,
wherein the inspecting of the photoresist pattern comprises:
obtaining an image of the photoresist pattern;
determining a material of an insertion layer to be inserted in a semiconductor structure, the semiconductor structure comprising the semiconductor layer, the wafer, and the photoresist layer;
determining a thickness of the insertion layer;
inserting the insertion layer having the determined material and the determined thickness into the semiconductor structure; and
measuring the photoresist pattern while the insertion layer is inserted in the semiconductor structure.

### Claim 18 (depends on 17)

The EUV lithography method of claim 17, wherein the material of the insertion layer is determined based on a refractive index and an absorption coefficient of the insertion layer, and
wherein the thickness of the insertion layer is determined based on a signal-to-noise ratio (SNR).

### Claim 19 (depends on 17)

The EUV lithography method of claim 17, further comprising, when the EUV mask is determined to be defective, removing the photoresist pattern.

### Claim 20 (depends on 17)

The EUV lithography method of claim 17, further comprising, when the EUV mask is determined not to be defective, etching the semiconductor layer using the photoresist pattern.