# US 2025/0164670 A1 · Anti-sparkle substrates and methods of making the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0164670 A1
- Document ID: US20250164670A1
- Status: Published application
- Kind: A1
- Application number: 18/947,687
- Filed: 2024-11-14
- Published: 2025-05-22
- Earliest claimed: 2023-11-21
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Christine Cecala; Ronghua Chen; Melanie Lian Geiger; Yuhui Jin; Qiao Li; Meng Shang
- Web page: https://patentgrep.com/patent/US20250164670A1

## CPC

- G02B 5/0242: {by means of dispersed particles}
- G02B 5/0221: {the surface having an irregular structure (G02B5/0226 takes precedence)}
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS

## Abstract

Anti-sparkle substrates include a first major surface with a textured surface having a surface roughness Ra from 0.03 micrometers to 0.09 micrometers. The anti-sparkle substrate is a glass-based substrate or a ceramic-based substrate. The anti-sparkle substrate can exhibit a haze from 3% to 40% and a sparkle from 1% to 3.8%. Methods include chemically strengthening an existing first major surface, abrading the existing first major surface to form an intermediate first major surface, and etching the intermediate first major surface to form the first major surface of the anti-sparkle substrate.

## Claims

### Claim 1

A method of forming an anti-sparkle substrate:
chemically strengthening an existing first major surface;
abrading the existing first major surface to form an intermediate first major surface; and
etching the intermediate first major surface to form a first major surface of the anti-sparkle substrate,
wherein the anti-sparkle substrate exhibits a haze from 3% to 40% and a sparkle from 1% to 4%.

### Claim 2 (depends on 1)

The method of claim 1, wherein the chemically strengthening comprises exposing the existing first major surface to a molten salt solution maintained a first temperature from 370° C. to 500° C. for a first period of time from 5 minutes to 8 hours, and the chemically strengthening forms an intermediate compressive stress region extending from the existing first major surface with an intermediate maximum compressive stress from 25 MegaPascals to 1500 MegaPascals.

### Claim 3 (depends on 1)

The method of claim 1, wherein the first major surface of the anti-sparkle substrate is substantially unstrengthened.

### Claim 4 (depends on 1)

The method of claim 1, wherein the abrading comprises impinging the existing first major surface with particles comprising a median particle size of 3 micrometers to 15 micrometers.

### Claim 5 (depends on 4)

The method of claim 4, wherein the particles are propelled with a pressure from 200 kiloPascals to 550 kiloPascals.

### Claim 6 (depends on 4)

The method of claim 4, wherein the particles comprise SiC, Al2O3, or combinations thereof.

### Claim 7 (depends on 4)

The method of claim 4, wherein the etching removes a thickness of from 5 micrometers to 100 micrometers from the intermediate first major surface.

### Claim 8 (depends on 7)

The method of claim 7, wherein the etching removes the thickness of from 9 micrometers to 40 micrometers from the intermediate first major surface.

### Claim 9 (depends on 1)

The method of claim 1, wherein the etching comprises contacting the intermediate first major surface with an acidic solution maintained at a temperature from 20° C. to 45° C. for from 2 minutes to 2 hours.

### Claim 10 (depends on 1)

The method of claim 1, wherein the etching comprises contacting the intermediate first major surface with an alkaline solution maintained at a temperature from 95° C. to 165° C. for from 10 minutes to 4 hours.

### Claim 11 (depends on 1)

The method of claim 1, wherein the sparkle is from 2.7% to 4%, and the anti-sparkle substrate exhibits a light diffusion of 8% or more.

### Claim 12 (depends on 1)

The method of claim 1, wherein the sparkle is from 1% to 2%, and the anti-sparkle substrate exhibits a light diffusion of 5% or less.

### Claim 13 (depends on 1)

The method of claim 1, wherein the anti-sparkle substrate exhibits a transmittance of 92% or more, a gloss from 55% to 150%, and a distinctness of image from 75.1% to 100%.

### Claim 14 (depends on 1)

The method of claim 1, wherein a surface roughness Ra of the first major surface is from 0.03 micrometers to 0.09 micrometers.

### Claim 15 (depends on 1)

The method of claim 1, wherein a root mean square height Sq of the first major surface is from 0.05 micrometers to 0.17 micrometers.

### Claim 16

An anti-sparkle substrate comprising:
a first major surface comprising a textured surface, a surface roughness Ra of the first major surface is from 0.03 micrometers to 0.09 micrometers,
wherein the anti-sparkle substrate is a glass-based substrate or a ceramic-based substrate, and the anti-sparkle substrate exhibits a haze from 3% to 40% and a sparkle from 1% to 4%.

### Claim 17 (depends on 16)

The anti-sparkle substrate of claim 16, wherein the anti-sparkle substrate comprises a compressive stress region extending from the first major surface comprising a maximum compressive stress from 25 MegaPascals to 1200 MegaPascals.

### Claim 18 (depends on 16)

The anti-sparkle substrate of claim 16, wherein the first major surface of the anti-sparkle substrate is substantially unstrengthened.

### Claim 19 (depends on 16)

The anti-sparkle substrate of claim 16, wherein the sparkle is from 2.7% to 4%, and the anti-sparkle substrate exhibits a light diffusion of 8% or more.

### Claim 20 (depends on 16)

The anti-sparkle substrate of claim 16, wherein the sparkle is from 1% to 2%, and the anti-sparkle substrate exhibits a light diffusion of 5% or less.