# US 2025/0163606 A1 · Production method for single crystal semiconductor film, production method for multilayer film of single crystal semiconductor film, and semiconductor element

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0163606 A1
- Document ID: US20250163606A1
- Status: Published application
- Kind: A1
- Application number: 18/840,392
- Filed: 2023-02-23
- Published: 2025-05-22
- Earliest claimed: 2022-02-24
- Assignees: Mach, Inc.; National University Corporation Tokyo University of Agriculture and Technology; National Institute of Information and Communications Technology; The University of Electro-Communications
- Applicants: Mach Corporation Co., Ltd.; National University Corporation Tokyo University of Agriculture and Technology; National Institute of Information and Communications Technology; The University of Electro-Communications
- Inventors: Goubun AKATSUKA; Yoshiyuki SUDA; Nobumitsu HIROSE; Satoshi TAMANYU; Yosuke AOYAGI; Shota NOZAKI; Takahiro TSUKAMOTO; Kento IKENO; Hiroya ESAKI
- Web page: https://patentgrep.com/patent/US20250163606A1

## CPC

- C30B 23/02: Epitaxial-layer growth
- C23C 14/06: characterised by the coating material ({C23C14/0021} , C23C14/04 take precedence)
- C23C 14/34: Sputtering
- C23C 14/35: by application of a magnetic field, e.g. magnetron sputtering {(C23C14/3457 takes precedence)}
- C30B 23/08: by condensing ionised vapours (by reactive sputtering C30B25/06)
- C30B 29/06: Silicon
- C30B 29/52: Alloys
- C30B 33/00: After-treatment of single crystals or homogeneous polycrystalline material with defined structure (C30B31/00 takes precedence)
- C30B 33/005: {Oxydation}
- H10P 14/22: using physical deposition, e.g. vacuum deposition or sputtering
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/29: {characterised by the substrates}
- H10P 14/2905: {Silicon, silicon germanium or germanium}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3444: {P-type}
- H10P 14/3466: {Crystal orientation}
- H10P 14/412: {Deposition of metallic or metal-silicide materials}
- H10P 14/6308: {of Group IV semiconductors}
- H10P 14/6316: {Formation by nitridation, e.g. nitridation of the substrate}
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Since a high temperature process is required when adding impurities to a semiconductor crystal film by means of ion implantation or by means of thermal diffusion, it has been difficult to form a steep impurity profile. A production method for a single crystal semiconductor film by means of crystal growth using a magnetron sputtering device to which one or more group 14 semiconductor targets are attached, the method being characterized in that at least one of the targets is doped with impurities, the film-forming temperature is 300° C. or higher, the growth rate is 10 nm or less per minute, the sputtering gas is an inert gas, and the one or more targets are sputtered simultaneously.

## Claims

### Claim 1

A production method for a single crystal silicon semiconductor film by means of crystal growth using a magnetron sputtering device to which one or more targets containing a silicon crystal target doped with boron with a surface plane orientation of within (100) ±6 degrees are attached,
wherein
a sputtering gas is an inert gas, and
the one or more targets containing the silicon crystal target doped with baron are sputtered simultaneously.

### Claim 2

(canceled)

### Claim 3 (depends on 1)

The production method for a single crystal silicon semiconductor film according to claim 1,
wherein the inert gas is argon.

### Claim 4

(canceled)

### Claim 5 (depends on 1)

The production method for a single crystal silicon semiconductor film according to claim 1,
wherein the surface plane orientation of the silicon crystal target doped with boron is within (100) ±1 degrees.

### Claim 6 (depends on 1)

The production method for a single crystal semiconductor film according to claim 1,
wherein a growth temperature is 560° C. or higher.

### Claim 7

(canceled)

### Claim 8

A production method for a single crystal silicon semiconductor film by means of crystal growth using a magnetron sputtering device to which one or more targets containing a phosphorus-doped silicon semiconductor targets are attached
wherein
a growth temperature is 320° or higher and lower than 500° C., and
a growth rate is 7 nm or less per minute,
a sputtering gas is an inert gas, and
the one or more targets containing the phosphorus-doped silicon semiconductor target are sputtered simultaneously.

### Claim 9

A production method for a silicon-germanium mixed crystal semiconductor film by means of crystal growth using a magnetron sputtering device to which one or more targets containing a phosphorus-doped silicon and/or germanium semiconductor target are attached,
wherein a growth rate is 3.5 nm or less per minute.

### Claim 10

(canceled)

### Claim 11

(canceled)

### Claim 12 (depends on 1)

A production method for a multilayer film of a semiconductor oxide and a semiconductor film, wherein without taking the single crystal semiconductor film formed by the production method according to claim 1 out of a vacuum chamber, a surface thereof is oxidized.

### Claim 13 (depends on 1)

A production method for a multilayer film of a semiconductor nitride and a semiconductor film, wherein without taking the single crystal semiconductor film formed by the production method according to claim 1 out of a vacuum chamber, a surface thereof is nitrided.

### Claim 14 (depends on 1)

A production method for a multilayer film of metal and a semiconductor film, wherein a metal film is formed without taking the semiconductor film formed by the production method according to claim 1 out of a vacuum chamber.

### Claim 15 (depends on 1)

A semiconductor element produced using the production method according to claim 1.

### Claim 16 (depends on 8)

A production method for a multilayer film of a semiconductor oxide and a semiconductor film, wherein without taking the single crystal semiconductor film formed by the production method according to claim 8 out of a vacuum chamber, a surface thereof is oxidized.

### Claim 17 (depends on 8)

A production method for a multilayer film of a semiconductor nitride and a semiconductor film, wherein without taking the single crystal semiconductor film formed by the production method according to claim 8 out of a vacuum chamber, a surface thereof is nitrided.

### Claim 18 (depends on 8)

A production method for a multilayer film of metal and a semiconductor film, wherein a metal film is formed without taking the semiconductor film formed by the production method according to claim 8 out of a vacuum chamber.

### Claim 19 (depends on 8)

A semiconductor element produced using the production method according to claim 8.

### Claim 20 (depends on 9)

A production method for a multilayer film of a semiconductor oxide and a semiconductor film, wherein without taking the single crystal semiconductor film formed by the production method according to claim 9 out of a vacuum chamber, a surface thereof is oxidized.

### Claim 21 (depends on 9)

A production method for a multilayer film of a semiconductor nitride and a semiconductor film, wherein without taking the single crystal semiconductor film formed by the production method according to claim 9 of a vacuum chamber, a surface thereof is nitrided.

### Claim 22 (depends on 9)

A production method for a multilayer film of metal and a semiconductor film, wherein a metal film is formed without taking the semiconductor film formed by the production method according to claim 9 out of a vacuum chamber.

### Claim 23 (depends on 9)

A semiconductor element produced using the production method according to claim 9.