# US 2025/0162882 A1 · Silicon Carbide Powder, and Production Method Thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0162882 A1
- Document ID: US20250162882A1
- Status: Published application
- Kind: A1
- Application number: 18/840,717
- Filed: 2023-02-10
- Published: 2025-05-22
- Earliest claimed: 2022-02-24
- Assignees: Tokuyama Corporation
- Applicants: Tokuyama Corporation
- Inventors: Yutaka Fukunaga
- Web page: https://patentgrep.com/patent/US20250162882A1

## CPC

- C01B 32/984: Preparation from elemental silicon
- C01B 32/956: Silicon carbide
- C01B 32/97: Preparation from SiO or SiO2
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2006/12: Surface area
- C01P 2006/40: Electric properties
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

Please delete the Abstract in its entirety and substitute therefor the following new A silicon carbide powder contains free carbon in a content of 0.04 mass % or less, in which a ratio of silicon atoms to carbon atoms (Si/C molar ratio) is 1.00 to 1.02. The silicon carbide powder can be produced by a method including a combustion synthesis step of preheating a mixed powder containing a metal silicon powder and a carbon powder having a Si/C molar ratio of 1.00 or more and 1.02 or less at a temperature of 900° C. to 1300° C. under an inert atmosphere, and igniting a part of the mixed powder to perform combustion synthesis to obtain a crude silicon carbide powder; and a heating step of heating the crude silicon carbide powder at a temperature of 2000° C. to 2500° C. under an inert atmosphere. In addition, the silicon carbide powder can also be obtained, without undergoing the heating step, by preheating the mixed powder at a temperature of 900° C. to 1300° C. under an atmospheric pressure and an inert atmosphere, and igniting a part of the mixed powder to perform combustion synthesis.

## Claims

### Claim 1

A silicon carbide powders comprising:
free carbon in a content of 0.04 mass % or less,
wherein a ratio of silicon atoms to carbon atoms (Si/C molar ratio) is 1.00 to 1.02.

### Claim 2 (depends on 1)

The silicon carbide powder according to claim 1, wherein an amount of metal impurities is 200 ppm or less.

### Claim 3

A method for producing a silicon carbide powder, comprising:
a combustion synthesis step of preheating a mixed powder containing a metal silicon powder and a carbon powder having a Si/C molar ratio of 1.00 or more and 1.02 or less at a temperature of 900° C. to 1300° C. under an inert atmosphere, and then igniting a part of the mixed powder to perform combustion synthesis to obtain a crude silicon carbide powder; and
a heating step of heating the crude silicon carbide powder at a temperature of 2000° C. to 2500° C. under an inert atmosphere.

### Claim 4

A method for producing a silicon carbide powder, comprising:
a combustion synthesis step of preheating a mixed powder containing a metal silicon powder and a carbon powder having a Si/C molar ratio of 1.00 or more and 1.02 or less at a temperature of 900° C. to 1300° C. under an atmospheric pressure and an inert atmosphere, and
then igniting a part of the mixed powder to perform combustion synthesis to obtain a silicon carbide powder.